US4460546A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Trigger to controllably initiate crystallization
Assignee: OLDEST AMERICAN Corp 1001 FRANKLIN AVENUE GARDEN CITY NEW YORK A CORP OF DE
•
Filing: 1980-08-11
•
Granted: 1984-07-17
•
Expires: 2000-08-11
Abstract
Abstract A trigger usable in initiating crystallization of a supercooled salt solution comprises a thin metallic strip containing multiple pin-hole size openings, and which is bendable with snap displacement. The strip may typically be non-ferrous.
Inventors
- 👤 Imants P. Kapralis
- 👤 Harry Krukle
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-24 03:07
CPC Classifications
A; A61; A61F; A61F7/00; A61F7/02; A61F7/03; B; B01; B01D; B01D9/00; B01D9/005; F; F28; F28D; F28D20/00; F28D20/02; F28D20/028; A61F2007/0292; A61F2007/0293; Y; Y02; Y02E; Y02E60/00; Y02E60/14
Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
194 words
For use in initiating crystallization of a supercooled salt solution, the combination that includes a flexible container containing said solution, and a trigger located in the container in contact with the solution, the trigger comprising (a) a thin, non-ferrous, metallic strip having a perimeter, (b) said strip having a multiplicity of openings formed therein, each opening characterized as having opposed edges which face one another in near touching relation, said openings being of pin-hole size and everywhere spaced inwardly from the strip periphery, (c) the strip further characterized as having two configurations between which it is bendable with snap-displacement causing (said edges to initiate) progressive exothermic crystallization of said salt in the solution, (d) the strip being in the general form of a dished disc having a central portion and an outer portion surrounding said central portion, the outer portion having a curved periphery, (e) said openings everywhere spaced inwardly from the disc periphery and located in at least one of said disc portions whereby said periphery is free of opening edges which could otherwise penetrate the container, the container consisting of plastic material, (f) the strip having molecular structure which is impact oriented.
Claim 2
Dependent Claim
194 words
For use in initiating crystallization of a supercooled salt solution, the combination that includes a flexible container containing said solution, and a trigger located in the container in contact with the solution, the trigger comprising (a) a thin, non-ferrous, metallic strip having a perimeter, (b) said strip having a multiplicity of openings formed therein, each opening characterized as having opposed edges which face one another in near touching relation, said openings being of pin-hole size and everywhere spaced inwardly from the strip periphery, (c) the strip further characterized as having two configurations between which it is bendable with snap-displacement causing (said edges to initiate) progressive exothermic crystallization of said salt in the solution, (d) the strip being in the general form of a dished disc having a central portion and an outer portion surrounding said central portion, the outer portion having a curved periphery, (e) said openings everywhere spaced inwardly from the disc periphery and located in at least one of said disc portions whereby said periphery is free of opening edges which could otherwise penetrate the container, the container consisting of plastic material, (f) the strip having molecular structure which is impact oriented.
Claim 3
Dependent Claim
11 words
The trigger of claim 1 wherein said openings are generally circular.
Claim 4
Dependent Claim
22 words
The trigger of claim 1 wherein said strip is metallic and has dished configuration in one of said configurations characterized as stable.
Claim 5
Dependent Claim
14 words
The trigger of claim 1 wherein said opening are located in said outer portions.
Claim 6
Dependent Claim
12 words
The trigger of claim 1 wherein said strip consists of beryllium copper.
Claim 7
Dependent Claim
12 words
The trigger of claim 1 wherein said strip consists of phospor bronze.
Claim 8
Dependent Claim
15 words
The trigger of claim 1 wherein the strip is in the form of a disc.
Claim 9
Dependent Claim
198 words
For use in initiating crystallization of a supercooled salt solution, the combination that includes a flexible container containing said solution, and a trigger located in the container in contact with the solution, the trigger comprising (a) a thin non-ferrous metallic strip having a perimeter, (b) said strip having at least one pin-hole size opening formed therein and spaced inwardly from the strip periphery, (c) the strip metal selected from the group consisting of phosphor bronze and beryllium copper, (d) the strip further characterized as having two configurations between which it is bendable with snap-displacement causing progressive exothermic crystallization of said salt in the solution, (e) the strip being in the general form of a dished disc having a central portion and an outer portion surrounding said central portion, the outer portion having a curved periphery, (f) said opening or openings located in said outer portion and said central portion being substantially free of said opening or openings, said opening or openings everywhere spaced inwardly from the disc periphery whereby said periphery is free of opening edges which could otherwise penetrate the container, the container consisting of plastic material, (g) the strip having molecular structure which is impact oriented.
Claim 10
Dependent Claim
198 words
For use in initiating crystallization of a supercooled salt solution, the combination that includes a flexible container containing said solution, and a trigger located in the container in contact with the solution, the trigger comprising (a) a thin non-ferrous metallic strip having a perimeter, (b) said strip having at least one pin-hole size opening formed therein and spaced inwardly from the strip periphery, (c) the strip metal selected from the group consisting of phosphor bronze and beryllium copper, (d) the strip further characterized as having two configurations between which it is bendable with snap-displacement causing progressive exothermic crystallization of said salt in the solution, (e) the strip being in the general form of a dished disc having a central portion and an outer portion surrounding said central portion, the outer portion having a curved periphery, (f) said opening or openings located in said outer portion and said central portion being substantially free of said opening or openings, said opening or openings everywhere spaced inwardly from the disc periphery whereby said periphery is free of opening edges which could otherwise penetrate the container, the container consisting of plastic material, (g) the strip having molecular structure which is impact oriented.
Claim 11
Dependent Claim
169 words
For use in initiating crystallization of a supercooled salt solution, the combination that includes a flexible container containing said solution, and a trigger located in the container in contact with the solution, the trigger comprising (a) a thin metallic strip having a perimeter, (b) said strip having a multiplicity of pin-hole size openings therethrough and everywhere spaced inwardly from the strip periphery, (c) the strip further characterized as having two configurations between which it is bendable with snap-displacement causing progressive exothermic crystallization of said salt in the solution, (d) the strip being in the general form of a dished disc having a central portion and an outer portion surrounding said centra portion, the outer portion having a curved periphery, (e) said openings everywhere spaced inwardly from the disc periphery and located in a zone extending about said central portion, whereby said periphery is free of opening edges which could otherwise penetrate the container, the container consisting of plastic material, (f) the strip having molecular structure which is impact oriented.
Claim 12
Dependent Claim
169 words
For use in initiating crystallization of a supercooled salt solution, the combination that includes a flexible container containing said solution, and a trigger located in the container in contact with the solution, the trigger comprising (a) a thin metallic strip having a perimeter, (b) said strip having a multiplicity of pin-hole size openings therethrough and everywhere spaced inwardly from the strip periphery, (c) the strip further characterized as having two configurations between which it is bendable with snap-displacement causing progressive exothermic crystallization of said salt in the solution, (d) the strip being in the general form of a dished disc having a central portion and an outer portion surrounding said centra portion, the outer portion having a curved periphery, (e) said openings everywhere spaced inwardly from the disc periphery and located in a zone extending about said central portion, whereby said periphery is free of opening edges which could otherwise penetrate the container, the container consisting of plastic material, (f) the strip having molecular structure which is impact oriented.
References Cited (Backward Citations)
US811750A
Cited
US1502744A
Cited
US1656366A
Cited
US1679432A
Cited
US1894775A
Cited
US2157169A
Cited
US2220777A
Cited
US2827438A
Cited
US3093308A
Cited
US3175558A
Cited
US3223081A
Cited
US3468025A
Cited
US3536058A
Cited
US3475239A
Cited
US3550578A
Cited
US3854156A
Cited
US3951127A
Cited
US4077390A
Cited
US4379448A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-07-17 | 1988-01-16 | 1988-07-17 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-07-17 | 1992-01-16 | 1992-07-17 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-07-17 | 1996-01-16 | 1996-07-17 | $7700.00 | Window Closed / Lapsed |