Method of reducing pollution in microwave devulcanization process

Assignee: Goodyear Tire and Rubber Co
•
Filing: 1982-09-28
•
Granted: 1984-07-10
•
Expires: 2002-09-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract This invention provides a method of controlling the pollution in a microwave devulcanization process consisting of passing particles of sulfur-vulcanized elastomer containing polar groups through a microwave energy devulcanization device to generate heat in the devulcanization of said particles whereby said particles exits said device at a temperature in excess of 260° C., feeding said particles from the devulcanization device to feed input of an extruder, extruding said particles to exit the extruder at a temperature of about 90° to 125° C. as an extrudate. The extrudate can be used per se as a compounding stock or sent to a mill to be sheeted and stored until needed.

Inventors

  • 👤 Keith A. Tyler
  • 👤 Gene L. Cerny

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 19:24
CPC Classifications
H; H05; H05B; H05B6/00; H05B6/64; H05B6/78; H05B6/788

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 83 words
A method of controlling the pollution in a microwave devulcanization process consisting of passing particles of sulfur-vulcanized elastomer containing polar groups through a microwave energy devulcanization device which generates heat in the devulcanization of said particles whereby said particles exits said device at a temperature in excess of 260° C., feeding said particles from the devulcanization device to a feed input of an extruder, extruding said particles to exit the extruder at a temperature of about 90° to 125° C. as an extrudate.
Claim 2
Independent Claim 83 words
A method of controlling the pollution in a microwave devulcanization process consisting of passing particles of sulfur-vulcanized elastomer containing polar groups through a microwave energy devulcanization device which generates heat in the devulcanization of said particles whereby said particles exits said device at a temperature in excess of 260° C., feeding said particles from the devulcanization device to a feed input of an extruder, extruding said particles to exit the extruder at a temperature of about 90° to 125° C. as an extrudate.
Claim 3
Dependent Claim 26 words
The method of claim 1 wherein the extruder has a screw with the ratio of length of screw to its diameter being about 3.5-4.5 to 1.

References Cited (Backward Citations)

US3993723A Cited
US4107354A Cited
US4104205A Cited
US4129768A Cited
US4123584A Cited
US4130616A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-07-10 1988-01-09 1988-07-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-07-10 1992-01-09 1992-07-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-07-10 1996-01-09 1996-07-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag