Abstract

Abstract A piezoelectric resonator which resonates in thickness shear mode. The piezoelectric resonator includes a strip shaped resonance chip made of an X-cut plate of lithium tantalate crystal and having a rectangular cross-section. Electrodes are formed at the center portion with respect to the longitudinal direction of the resonance chip on each of two X-plane surfaces. The width of the electrodes is equal to the width of the resonance chip. The longitudinal direction of the resonance chip inclines with respect to the Y-axis by an angle of 50°±2' in the clockwise direction in the X-plane so as to make the longitudinal direction of the resonance chip coincide with the displacement direction of primary oscillation of the crystal. Optimal ratios of the dimensions of the resonance chip and terminal connectors at the ends of the resonance chip are given to reduce spurious response. The temperature characteristic is optimized by selecting rotation angles about the Y-and Z-axes in relation to the amount of trapped energy.

Inventors

  • 👤 Yoshiro Fujiwara
  • 👤 Sumio Yamada
  • 👤 Hiroshi Hoshino
  • 👤 Noboru Wakatsuki

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 10:14
CPC Classifications
H; H03; H03H; H03H9/00; H03H9/02; H03H9/02007; H03H9/02015; H03H9/02031; H03H9/02157; H03H9/15; H03H9/17; H03H9/177

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 148 words
A piezoelectric resonator which resonates due to thickness shear, comprising: a strip-shaped resonance chip, made from an X-cut plate of lithium tantalate crystal having two surfaces, a thickness and a direction of primary oscillation, said resonance chip having a rectangular prism shape with a thickness corresponding to the thickness of the X-cut plate and a width measured perpendicular to the axis of said resonance chip; and electrodes, formed on the sides of said resonance chip corresponding to the surfaces of the X-cut plate, said electrodes being centered along the axis of the resonance chip and having a width equal to the width of said resonance chip, the axis of said resonance chip inclining with respect to the Y-axis by an angle of 50°±2° in the clockwise direction, and the axis of said resonance chip coincides with the displacement direction of the primary oscillation mode of the X-cut plate.
Claim 2
Dependent Claim 148 words
A piezoelectric resonator which resonates due to thickness shear, comprising: a strip-shaped resonance chip, made from an X-cut plate of lithium tantalate crystal having two surfaces, a thickness and a direction of primary oscillation, said resonance chip having a rectangular prism shape with a thickness corresponding to the thickness of the X-cut plate and a width measured perpendicular to the axis of said resonance chip; and electrodes, formed on the sides of said resonance chip corresponding to the surfaces of the X-cut plate, said electrodes being centered along the axis of the resonance chip and having a width equal to the width of said resonance chip, the axis of said resonance chip inclining with respect to the Y-axis by an angle of 50°±2° in the clockwise direction, and the axis of said resonance chip coincides with the displacement direction of the primary oscillation mode of the X-cut plate.
Claim 3
Dependent Claim 54 words
A piezoelectric resonator as set forth in claim 1, wherein the X-cut plate is rotated about the Y-axis and Z-axis of the lithium tantalate crystal with angles of rotation less than or equal to 10°, and wherein said electrodes have a length which is less than 3.95 times the thickness of said resonance chip.
Claim 4
Dependent Claim 39 words
A piezoelectric resonator as set forth in claim 2, wherein the angles of rotation about the Y-axis and Z-axis are selected where the trapped energy of the oscillation in said resonance chip has a primary temperature coefficient of zero.
Claim 5
Dependent Claim 38 words
A piezoelectric resonator as set forth in claim 1, wherein the trapped energy ζ is defined by ζ=1/8·θ+(0.65±0.1) when the angle of rotation about the Z-axis is zero and the angle of rotation about the Y-axis is θ.
Claim 6
Dependent Claim 32 words
A piezoelectric resonator as set forth in claim 2, wherein the angle of rotation about the Y-axis is zero while the angle of rotation about the Z-axis is between -6° and 6°.
Claim 7
Dependent Claim 56 words
A piezoelectric resonator as set forth in claim 1, wherein the length of said resonance chip divided by the thickness of said resonance chip is more than 14 and the width of said resonance chip divided by the thickness of said resonance chip is selected from among the ranges 1.35 to 3.0 and 3.8 to 5.0.
Claim 8
Dependent Claim 80 words
A piezoelectric resonator as set forth in claim 1, further comprising terminal conductors, operatively connected to said electrodes and connectable to outside wiring, each of said terminal conductors formed on one of the X-plane surfaces at each end of said resonance chip, the thickness of said terminal conductor divided by the thickness of said resonance chip being between 0.29 and 0.42 and the width of said terminal conductor divided by the length of said resonance chip being less that 0.06.
Claim 9
Dependent Claim 178 words
A piezoelectric resonator which resonates due to thickness shear, comprising: a strip-shaped resonance chip, made from an X-cut plate of lithium tantalate crystal having two surfaces, a thickness and a direction of primary oscillation, said resonance chip having a rectangular prism shape with a thickness corresponding to the thickness of the X-cut plate and a width measured perpendicular to the axis of said resonance chip; and electrodes formed on the sides of said resonance chip corresponding to the surfaces of the X-cut plate, said electrode being centered along the axis of said resonance chip and having a width equal to the width of said resonance chip, the axis of said resonance chip inclining with respect to the Y-axis and the axis of said resonance chip coincides with the displacement direction of the primary oscillation mode of the crystal, said X-cut plate being rotated about at least one of the Y-axis and Z-axis within an angle of 10° in one direction, and said electrodes have a length which is less than 3.95 times the thickness of said resonance chip.
Claim 10
Dependent Claim 178 words
A piezoelectric resonator which resonates due to thickness shear, comprising: a strip-shaped resonance chip, made from an X-cut plate of lithium tantalate crystal having two surfaces, a thickness and a direction of primary oscillation, said resonance chip having a rectangular prism shape with a thickness corresponding to the thickness of the X-cut plate and a width measured perpendicular to the axis of said resonance chip; and electrodes formed on the sides of said resonance chip corresponding to the surfaces of the X-cut plate, said electrode being centered along the axis of said resonance chip and having a width equal to the width of said resonance chip, the axis of said resonance chip inclining with respect to the Y-axis and the axis of said resonance chip coincides with the displacement direction of the primary oscillation mode of the crystal, said X-cut plate being rotated about at least one of the Y-axis and Z-axis within an angle of 10° in one direction, and said electrodes have a length which is less than 3.95 times the thickness of said resonance chip.
Claim 11
Dependent Claim 39 words
A piezoelectric resonator as set forth in claim 8, wherein the angles of rotation about the Y-axis and Z-axis are selected where the trapped energy of the oscillation in said resonance chip has a primary temperature coefficient of zero.
Claim 12
Dependent Claim 38 words
A piezoelectric resonator as set forth in claim 8, wherein the trapped energy ζ is defined by ζ=1/8·θ+(0.65 ±0.1) when angle of rotation about the Z-axis is zero and the angle of rotation about the Y-axis is θ.
Claim 13
Dependent Claim 32 words
A piezoelectric resonator as set forth in claim 8, wherein the angle of rotation about the Y-axis is zero while the angle of rotation about the Z-axis is between -6° and 6°.

References Cited (Backward Citations)

US3525885A Cited
JPS5468194A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-06-12 1987-12-12 1988-06-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-06-12 1991-12-12 1992-06-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-06-12 1995-12-12 1996-06-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag