Abstract
Abstract The decorative objects on which a light-interference surface layer showing an esthetic design is formed is produced by the steps of forming a metal thin film on glazed and baked surface of a base body and treating the base body at high temperature in oxygen atmosphere, and which are highly useful as decorative articles, dinner sets, building materials, and industrial art objects.
Inventors
- 👤 Toru Mashida
- 👤 Sumeo Matsushita
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-30 14:51
CPC Classifications
C; C04; C04B; C04B41/00; C04B41/009; B; B44; B44C; B44C1/00; B44C1/005; B44C1/26; B44F; B44F1/00; C04B41/45; C04B41/50; C04B41/51; C04B41/80; C04B41/81; C04B41/85; C04B41/88; C23; C23C; C23C26/00; C23C8/00; C23C8/06; C23C8/08; C23C8/10; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/24355; Y10T428/24471; Y10T428/24802; Y10T428/24851; Y10T428/24868; Y10T428/24876
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
88 words
A method of producing decorative objects comprising the steps of forming a metal thin film on glazed and baked surface of a base body and treating the base body at high temperature in oxygen atmosphere, wherein the high temperature treatment causes oxidation of the thin film applied directly to the glazed and baked surface and the glazed and baked surface comes to a semi-fluid state to provide a surface with a form of fine ruggedness or unevenness, whereby a light-interference surface layer showing an esthetic pattern is formed.
Claim 2
Independent Claim
88 words
A method of producing decorative objects comprising the steps of forming a metal thin film on glazed and baked surface of a base body and treating the base body at high temperature in oxygen atmosphere, wherein the high temperature treatment causes oxidation of the thin film applied directly to the glazed and baked surface and the glazed and baked surface comes to a semi-fluid state to provide a surface with a form of fine ruggedness or unevenness, whereby a light-interference surface layer showing an esthetic pattern is formed.
Claim 3
Dependent Claim
26 words
The method of producing decorative objects as claimed in claim 1, wherein the base body is glazed appropriately using variety of color glazes having different characteristics.
Claim 4
Dependent Claim
79 words
The method of producing decorative objects as claimed in claim 1 which comprises the steps of forming fine ruggedness or unevenness on the surface of a glazed base body or a glazed and baked base body by sprinkling heat-resisting fine powder and baking, then forming a metal film thereon, and treating the metal thin film applied directly to said base body at high temperature in an oxygen atmosphere, whereby a light-interference surface layer showing an esthetic pattern is formed.
Claim 5
Dependent Claim
36 words
The method of producing decorative objects as claimed in claim 1, wherein the formation of the metal thin film is carried out by any of vacuum deposition, sputtering, ion plating, chemical vapour deposition and plating methods.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-05-08 | 1987-11-07 | 1988-05-08 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-05-08 | 1991-11-07 | 1992-05-08 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-05-08 | 1995-11-07 | 1996-05-08 | $7700.00 | Window Closed / Lapsed |