US4445262A Expired / Lapsed US ⏱️ 0.0 years remaining

Procedure for rebuilding the movable plate in the pouring valve of a ladle

Assignee: USS ENGINEERS AND CONSULTANTS Inc A DE CORP
•
Filing: 1982-12-21
•
Granted: 1984-05-01
•
Expires: 2002-12-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Procedure for rebuilding a movable plate in the pouring valve of a ladle, involving the complete reconstruction of the original nozzle, which has been removed, and of a flat portion, also removed, around the pouring hole, in a circular or rectangular area whose width is equal to at least the external diameter of the nozzle. The nozzle is reconstructed with a prefabricated piece of refractory material, or with fresh refractory material packed "in situ", and may be of the same shape as the original nozzle, or of a different shape; the flat portion is reconstructed using a prefabricated refractory piece, or with fresh refractory material packed "in situ".

Inventors

  • 👤 Romano Cappelli

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 16:49
CPC Classifications
B; B22; B22D; B22D41/00; B22D41/14; B22D41/22; B22D41/28; B22D41/30; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49718; Y10T29/49719; Y10T29/49721; Y10T29/4973

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 243 words
Procedure for rebuilding a movable plate in the pouring valve of a ladle, according to which the portions around the pouring hole are removed and rebuilt using suitable prefabricated parts of refractory material, or packed directly "in situ" to replace the parts removed; characterized by the fact that it consists of the removal of an upper element of the flat part of the plate (1) over an area (φ, L) which is greater in width than the diameter that fits within the thickness (4) of the refractory putty placed between the nozzle (5) and its casing (6), and less than the minimum width (a) of the plate (1); removal of the nozzle (5); replacement of the nozzle thus removed (5) with a nozzle (5'), which is either prefabricated or packed "in situ", with a height less than that of the nozzle that was removed (5); replacement of the upper element that was removed with a stepped upper element (9, 9") which has an upper width (φ e , L') slightly smaller than the width (φ, L) of the upper element that was removed to allow for the interposition of a layer (10) of refractory putty, and with a lower annular part with an external diameter (φ 1 ) corresponding to the external diameter (φ 1 ) of the nozzle (5') and with a total height (h 2 ) greater than the height (h 1 ) of the flat part of the plate (1).
Claim 2
Dependent Claim 243 words
Procedure for rebuilding a movable plate in the pouring valve of a ladle, according to which the portions around the pouring hole are removed and rebuilt using suitable prefabricated parts of refractory material, or packed directly "in situ" to replace the parts removed; characterized by the fact that it consists of the removal of an upper element of the flat part of the plate (1) over an area (φ, L) which is greater in width than the diameter that fits within the thickness (4) of the refractory putty placed between the nozzle (5) and its casing (6), and less than the minimum width (a) of the plate (1); removal of the nozzle (5); replacement of the nozzle thus removed (5) with a nozzle (5'), which is either prefabricated or packed "in situ", with a height less than that of the nozzle that was removed (5); replacement of the upper element that was removed with a stepped upper element (9, 9") which has an upper width (φ e , L') slightly smaller than the width (φ, L) of the upper element that was removed to allow for the interposition of a layer (10) of refractory putty, and with a lower annular part with an external diameter (φ 1 ) corresponding to the external diameter (φ 1 ) of the nozzle (5') and with a total height (h 2 ) greater than the height (h 1 ) of the flat part of the plate (1).
Claim 3
Dependent Claim 174 words
Procedure for rebuilding the movable plate in the pouring valve of a ladle, according to which the portions around the pouring hole are reconstructed with parts which replace the parts removed and are prefabricated from suitable refractory material or are packed directly "in situ", characterized in that it consists of the removal of an upper element of the flat part of the plate (1) over an area (φ, L), which is greater in width than the diameter that fits within the thickness (4) of the refractory putty placed between the nozzle (5) and its casing (6) and is less than the minimum width (a) of the plate (1); removal of the nozzle (5); replacement of the removed nozzle and upper element by a single piece (12) prefabricated or packed "in situ", consisting of a nozzle (5') and an upper part (9') with a width (φ e , L') slightly smaller than the width (φ, L) of the upper element that was removed to allow for the interposition of a layer (10) of refractory putty.
Claim 4
Dependent Claim 174 words
Procedure for rebuilding the movable plate in the pouring valve of a ladle, according to which the portions around the pouring hole are reconstructed with parts which replace the parts removed and are prefabricated from suitable refractory material or are packed directly "in situ", characterized in that it consists of the removal of an upper element of the flat part of the plate (1) over an area (φ, L), which is greater in width than the diameter that fits within the thickness (4) of the refractory putty placed between the nozzle (5) and its casing (6) and is less than the minimum width (a) of the plate (1); removal of the nozzle (5); replacement of the removed nozzle and upper element by a single piece (12) prefabricated or packed "in situ", consisting of a nozzle (5') and an upper part (9') with a width (φ e , L') slightly smaller than the width (φ, L) of the upper element that was removed to allow for the interposition of a layer (10) of refractory putty.
Claim 5
Dependent Claim 184 words
Procedure for rebuilding the movable plate in the pouring valve of a ladle, according to which the portions around the pouring hole are reconstructed with parts which replace the parts removed and are prefabricated from suitable refractory material or packed directly "in situ", characterized in that it consists of the removal of an upper element of the flat portion of the plate (1) over an area (φ, L) which is greater in width than the diameter that fits within the thickness (4) of the refractory putty placed between the nozzle (5) and its casing (6) and is less than the diameter which fits within the minimum width (a) of the plate (1); removal of the nozzle (5); replacement of the nozzle which has been removed (5) by a similar nozzle, either prefabricated or packed directly "in situ"; replacement of the upper element which was removed by an upper element (9') which has a width (φ e , L') slightly smaller than the width (φ, L) of the upper element which was removed to allow for the interposition of a layer (10) of refractory putty.
Claim 6
Dependent Claim 184 words
Procedure for rebuilding the movable plate in the pouring valve of a ladle, according to which the portions around the pouring hole are reconstructed with parts which replace the parts removed and are prefabricated from suitable refractory material or packed directly "in situ", characterized in that it consists of the removal of an upper element of the flat portion of the plate (1) over an area (φ, L) which is greater in width than the diameter that fits within the thickness (4) of the refractory putty placed between the nozzle (5) and its casing (6) and is less than the diameter which fits within the minimum width (a) of the plate (1); removal of the nozzle (5); replacement of the nozzle which has been removed (5) by a similar nozzle, either prefabricated or packed directly "in situ"; replacement of the upper element which was removed by an upper element (9') which has a width (φ e , L') slightly smaller than the width (φ, L) of the upper element which was removed to allow for the interposition of a layer (10) of refractory putty.
Claim 7
Dependent Claim 56 words
Procedure according to any of the preceding claims, characterized in that the upper element (9, 9', 9") installed in the flat portion of the plate (1) to replace the upper element that was removed initially projects above the upper surface of said flat portion and is subsequently smoothed off to the level of said upper surface.

References Cited (Backward Citations)

US4092771A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-05-01 1987-10-31 1988-05-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-05-01 1991-10-31 1992-05-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-05-01 1995-10-31 1996-05-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag