US4444951A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Polyblends of thermoplastic polynorbornene nitrile polymers, styrenemaleic anhydride polymers and acrylonitrile-butradiene-styrene polymers
Assignee: Bayer Antwerpen NV
•
Filing: 1983-04-11
•
Granted: 1984-04-24
•
Expires: 2003-04-11
Abstract
Abstract Molding compositions are prepared from blends of (A) thermoplastic polynorbornene nitrile polymers; (B) styrene/maleic anhydride polymers; (C) at least one of the polymers selected from the group consisting of ABS polymers, MBS polymers, and styrene/acrylonitrile polymers. Component B, the styrene/maleic anhydride polymer may optionally contain a termonomer such as methylmethacrylate or acrylonitrile and a rubber component.
Inventors
- 👤 Robert A. Mendelson
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 20:34
CPC Classifications
C; C08; C08L; C08L35/00; C08L35/06; C08L25/00; C08L25/02; C08L25/04; C08L25/08; C08L25/12; C08L51/00; C08L51/04; C08L55/00; C08L55/02; C08L45/00
Claims Analysis
Total Claims: 19
Claim 1
Independent Claim
338 words
A polyblend comprising: A. from 3 to 90% by weight of a thermoplastic polynorbornene nitrile polymer wherein the polynorbornene nitrile polymer is prepared by the ring opening polymerization of a 5-substituted norbornene-2 wherein one of the 5-substituents is a nitrile group and the other 5-substituent is chosen from the group consisting of hydrogen and C 1 to C 6 alkyls; B. from 5 to 70% by weight of a polymer of a vinylaromatic monomer and an unsaturated dicarboxylic acid anhydride monomer and optionally a termonomer, selected from the group consisting of C 1 to C 3 acrylates and methacrylates and unsaturated nitriles, wherein the relative amounts by weight of the monomers in the polymer are 50 to 85% of the vinylaromatic monomer, 15 to 35% of the dicarboxylic acid anhydride and 0 to 20% of the termonomer; and wherein the monomers are polymerized in the presence of 0 to 35% by weight of a rubber having a glass transition temperature below 0° C.; C. from 5 to 70% by weight of at least one polymer selected from the group consisting of (1) a grafted polymer composition comprising a matrix copolymer and a rubber substrate grafted with a superstrate copolymer wherein the copolymer consists of from 20 to 40 parts by weight of a monomer selected from the group consisting of methyl methacrylate and acrylonitrile and 80 to 60 parts by weight of a vinyl aromatic monomer, wherein the substrate rubber has a glass transition temperature below 0° C., wherein the monomers are polymerized in the presence of and grafted onto the substrate rubber, wherein the weight percent of the rubber is in the range from 5 to 50% by weight based on the weight of the grafted polymer composition; and (2) a polymer consists of of a vinylaromatic monomer and an unsaturated nitrile in a weight ratio of 80:20 to 60:40 respectively; and wherein the weight percent for Components (A), (B), and (C) is based on the total amount of Components (A), (B), and (C) in the polyblend.
Claim 2
Dependent Claim
338 words
A polyblend comprising: A. from 3 to 90% by weight of a thermoplastic polynorbornene nitrile polymer wherein the polynorbornene nitrile polymer is prepared by the ring opening polymerization of a 5-substituted norbornene-2 wherein one of the 5-substituents is a nitrile group and the other 5-substituent is chosen from the group consisting of hydrogen and C 1 to C 6 alkyls; B. from 5 to 70% by weight of a polymer of a vinylaromatic monomer and an unsaturated dicarboxylic acid anhydride monomer and optionally a termonomer, selected from the group consisting of C 1 to C 3 acrylates and methacrylates and unsaturated nitriles, wherein the relative amounts by weight of the monomers in the polymer are 50 to 85% of the vinylaromatic monomer, 15 to 35% of the dicarboxylic acid anhydride and 0 to 20% of the termonomer; and wherein the monomers are polymerized in the presence of 0 to 35% by weight of a rubber having a glass transition temperature below 0° C.; C. from 5 to 70% by weight of at least one polymer selected from the group consisting of (1) a grafted polymer composition comprising a matrix copolymer and a rubber substrate grafted with a superstrate copolymer wherein the copolymer consists of from 20 to 40 parts by weight of a monomer selected from the group consisting of methyl methacrylate and acrylonitrile and 80 to 60 parts by weight of a vinyl aromatic monomer, wherein the substrate rubber has a glass transition temperature below 0° C., wherein the monomers are polymerized in the presence of and grafted onto the substrate rubber, wherein the weight percent of the rubber is in the range from 5 to 50% by weight based on the weight of the grafted polymer composition; and (2) a polymer consists of of a vinylaromatic monomer and an unsaturated nitrile in a weight ratio of 80:20 to 60:40 respectively; and wherein the weight percent for Components (A), (B), and (C) is based on the total amount of Components (A), (B), and (C) in the polyblend.
Claim 3
Dependent Claim
14 words
A polyblend as in claim 1 wherein Component B is a styrene/maleic anhydride polymer.
Claim 4
Dependent Claim
28 words
A polyblend as in claim 1 wherein the grafted polymer of Component C is the polymerized monomers are acrylonitrile with styrene and the rubber substrate is butadiene rubber.
Claim 5
Dependent Claim
298 words
A polyblend comprising: A. from 3 to 90% by weight of a thermoplastic polynorbornene nitrile polymer wherein the polynorbornene nitrile polymer is prepared by the ring opening polymerization of a 5-substituted norbornene-2 wherein one of the 5-substituents is a nitrile group and the other 5-substituent is chosen from the group consisting of hydrogen and C 1 to C 6 alkyls; B. from 5 to 70% by weight of a styrene/maleic anhydride polymer comprising 50 to 85% by weight of styrene, 15 to 35% by weight of maleic anhydride and 0 to 20% of a methyl methacrylate termonomer; C. from 5 to 70% by weight of at least one polymer selected from the group consisting of (1) a grafted polymer composition comprising a matrix copolymer and a rubber substrate grafted with a superstrate copolymer wherein the copolymer consists of from 20 to 40 parts by weight of a monomer selected from the group consisting of methyl methacrylate and acrylonitrile and 80 to 60 parts by weight of a vinyl aromatic monomer, wherein the substrate rubber has a glass transition temperature below 0° C., wherein the monomers are polymerized in the presence of and grafted onto the substrate rubber, wherein the weight percent of the rubber is in the range from 5 to 50% by weight based on the weight of the grafted polymer composition; and (2) a styrene and acrylonitrile polymer consists of 60 to 80% by weight of styrene and 20 to 40% by weight of acrylonitrile and wherein the weight ratio of the styrene/maleic anhydride polymer (B) to the grafted polymer composition (C) is in the range of 80:20 to 20:80; and wherein the weight percent for Components (A), (B) and (C) is based on the total amount of Components (A), (B) and (C) in the polyblend.
Claim 6
Dependent Claim
298 words
A polyblend comprising: A. from 3 to 90% by weight of a thermoplastic polynorbornene nitrile polymer wherein the polynorbornene nitrile polymer is prepared by the ring opening polymerization of a 5-substituted norbornene-2 wherein one of the 5-substituents is a nitrile group and the other 5-substituent is chosen from the group consisting of hydrogen and C 1 to C 6 alkyls; B. from 5 to 70% by weight of a styrene/maleic anhydride polymer comprising 50 to 85% by weight of styrene, 15 to 35% by weight of maleic anhydride and 0 to 20% of a methyl methacrylate termonomer; C. from 5 to 70% by weight of at least one polymer selected from the group consisting of (1) a grafted polymer composition comprising a matrix copolymer and a rubber substrate grafted with a superstrate copolymer wherein the copolymer consists of from 20 to 40 parts by weight of a monomer selected from the group consisting of methyl methacrylate and acrylonitrile and 80 to 60 parts by weight of a vinyl aromatic monomer, wherein the substrate rubber has a glass transition temperature below 0° C., wherein the monomers are polymerized in the presence of and grafted onto the substrate rubber, wherein the weight percent of the rubber is in the range from 5 to 50% by weight based on the weight of the grafted polymer composition; and (2) a styrene and acrylonitrile polymer consists of 60 to 80% by weight of styrene and 20 to 40% by weight of acrylonitrile and wherein the weight ratio of the styrene/maleic anhydride polymer (B) to the grafted polymer composition (C) is in the range of 80:20 to 20:80; and wherein the weight percent for Components (A), (B) and (C) is based on the total amount of Components (A), (B) and (C) in the polyblend.
Claim 7
Dependent Claim
49 words
A polyblend as in claim 4 wherein the polynorbornene nitrile polymer is in the range from 15 to 55% by weight and the weight ratio of the styrene/maleic anhydride polymer of Component B to the grafted polymer composition of Component C is in the range from 80:20 to 20:80.
Claim 8
Dependent Claim
50 words
A polyblend as in claim 4 wherein the styrene monomer of Component B is substituted by the 5 to 15% by weight of a methyl methacrylate termonomer and wherein the grafted polymer of Component C is the polymerized monomers are acrylonitrile with styrene and the rubber substrate is butadiene rubber.
Claim 9
Dependent Claim
56 words
A polyblend according to claim 1 comprising: A. 3 to 90% by weight of the thermoplastic polynorbornene nitrile polymer; B. 5 to 70% by weight of the styrene/maleic anhydride/methylmethacrylate polymer; and C. 5 to 70% by weight of the grafted polymer is the polymerized monomers of acrylonitrile with styrene and the rubber substrate is butadiene rubber.
Claim 10
Dependent Claim
78 words
A polyblend according to claim 1 wherein the polymer of the vinyl aromatic monomer, the unsaturated discarboxylic acid anhydride and optionally a termonomer selected from the group consisting of C 1 to C 3 alkyl acrylates or methacrylate, acrylonitrile or methacrylonitrile of Component B is prepared by polymerizing the monomers in the presence of the rubber component having a glass transition temperature below 0° C., to provide from 5 to 25% by weight of rubber in the polymer.
Claim 11
Dependent Claim
20 words
A polyblend of claim 1 wherein said thermoplastic polynorbornene nitrile polymer is prepared by the ring-opening polymerization of a 5-cyano-norbornene-2.
Claim 12
Dependent Claim
24 words
A polyblend of claim 9 wherein the 5- position of said norbornene is also substituted by a C 1 to C 6 alkyl group.
Claim 13
Dependent Claim
15 words
A polyblend of claim 9 wherein said polynorbornene nitrile polymer has the general structure: ##STR2##
Claim 14
Dependent Claim
49 words
A polyblend according to claim 9 wherein the thermoplastic polynorbornene nitrile polymer of Component A is prepared by polymerizing the norbornene nitrile monomers and then blending with a rubber component having a glass transition temperature below 0° C., to provide from 5 to 25% of rubber in the product.
Claim 15
Dependent Claim
20 words
A polyblend according to claim 9 wherein the thermoplastic polynorbornene nitrile polymer of Component A is blended with butadiene/acrylonitrile rubber.
Claim 16
Dependent Claim
240 words
A polyblend comprising: A. from 3 to 90% by weight of a thermoplastic polynorbornene nitrile polymer wherein the polynorbornene nitrile polymer is prepared by the ring opening polymerization of a 5-substituted norbornene-2 wherein one of the other 5-substituents is a nitrile group and the other 5-substituent is chosen from the group consisting of hydrogen and C 1 to C 6 alkyls; B. from 5 to 70% by weight of a styrene/maleic anhydride polymer comprising 50 to 85% by weight of styrene, 15 to 35% by weight of maleic anhydride 0 to 20% of a methyl methacrylate termonomer; C. from 5 to 70% by weight of a grafted polymer composition comprising a matrix copolymer and a polybutadiene rubber substrate grafted with a superstrate copolymer wherein the copolymer consists of from 20 to 40 parts by weight of acrylonitrile and 80 to 60 parts by weight of a styrene monomer, wherein the monomers are polymerized in the pesence of and grafted onto the substrate rubber, wherein the weight percent of the rubber is in the range from 5 to 50% by weight based on the weight of the grafted polymer composition; and wherein the weight ratio of the styrene/maleic anhydride polymer (B) to the grafted polymer composition (C) is in the range of 80:20 to 20:80; and wherein the weight percent for Components (A), (B) and (C) is based on the total amount of Components (A), (B) and (C) in the polyblend.
Claim 17
Dependent Claim
240 words
A polyblend comprising: A. from 3 to 90% by weight of a thermoplastic polynorbornene nitrile polymer wherein the polynorbornene nitrile polymer is prepared by the ring opening polymerization of a 5-substituted norbornene-2 wherein one of the other 5-substituents is a nitrile group and the other 5-substituent is chosen from the group consisting of hydrogen and C 1 to C 6 alkyls; B. from 5 to 70% by weight of a styrene/maleic anhydride polymer comprising 50 to 85% by weight of styrene, 15 to 35% by weight of maleic anhydride 0 to 20% of a methyl methacrylate termonomer; C. from 5 to 70% by weight of a grafted polymer composition comprising a matrix copolymer and a polybutadiene rubber substrate grafted with a superstrate copolymer wherein the copolymer consists of from 20 to 40 parts by weight of acrylonitrile and 80 to 60 parts by weight of a styrene monomer, wherein the monomers are polymerized in the pesence of and grafted onto the substrate rubber, wherein the weight percent of the rubber is in the range from 5 to 50% by weight based on the weight of the grafted polymer composition; and wherein the weight ratio of the styrene/maleic anhydride polymer (B) to the grafted polymer composition (C) is in the range of 80:20 to 20:80; and wherein the weight percent for Components (A), (B) and (C) is based on the total amount of Components (A), (B) and (C) in the polyblend.
Claim 18
Dependent Claim
347 words
Molded and extruded articles prepared from a polyblend comprising: A. from 3 to 90% by weight of a thermoplastic polynorbornene nitrile polymer wherein the polynorbornene nitrile polymer is prepared by the ring opening polymerization of a 5-substituted norbornene-2 wherein one of the 5-substituents is a nitrile group and the other 5-substituent is chosen from the group consisting of hydrogen and C 1 to C 6 alkyls; B. from 5 to 70% by weight of a polymer of a vinylaromatic monomer and an unsaturated dicarboxylic acid anhydride and optionally a termonomer, selected from the group consisting of C 1 to C 3 acrylates and methacrylates and unsaturated nitriles, wherein the relative amounts by weight of the monomers in the polymer are 50 to 85% by weight of a vinyl aromatic monomer, 15 to 35% of the dicarboxylic acid anhydride and 0 to 20% of the termonomer; and wherein the monomers are polymerized in the presence of 0 to 35% by weight of a rubber having a glass transition temperature below 0° C.; and C. from 0 to 70% by weight of at least one polymer selected from the group consisting of (1) a grafted polymer composition comprising a matrix copolymer and a rubber substrate grafted with a superstrate copolymer wherein the copolymer consists of from 20 to 40 parts by weight of a monomer selected from the group consisting of methyl methacrylate and acrylonitrile and 80 to 60 parts by weight of a vinyl aromatic monomer, wherein the substrate rubber has a glass transition temperature below 0° C., wherein the monomers are polymerized in the presence of and grafted onto the substrate rubber, wherein the weight percent of the rubber is in the range from 5 to 50% by weight based on the weight of the grafted polymer composition; and (2) a polymer consists of a vinyl aromatic monomer and an unsaturated nitrile in a weight ratio of 80:20 to 60:40 respectively; and wherein the weight percent for Componets (A), (B) and (C) is based on the total amount of Components (A), (B) and (C) in the polyblend.
Claim 19
Dependent Claim
347 words
Molded and extruded articles prepared from a polyblend comprising: A. from 3 to 90% by weight of a thermoplastic polynorbornene nitrile polymer wherein the polynorbornene nitrile polymer is prepared by the ring opening polymerization of a 5-substituted norbornene-2 wherein one of the 5-substituents is a nitrile group and the other 5-substituent is chosen from the group consisting of hydrogen and C 1 to C 6 alkyls; B. from 5 to 70% by weight of a polymer of a vinylaromatic monomer and an unsaturated dicarboxylic acid anhydride and optionally a termonomer, selected from the group consisting of C 1 to C 3 acrylates and methacrylates and unsaturated nitriles, wherein the relative amounts by weight of the monomers in the polymer are 50 to 85% by weight of a vinyl aromatic monomer, 15 to 35% of the dicarboxylic acid anhydride and 0 to 20% of the termonomer; and wherein the monomers are polymerized in the presence of 0 to 35% by weight of a rubber having a glass transition temperature below 0° C.; and C. from 0 to 70% by weight of at least one polymer selected from the group consisting of (1) a grafted polymer composition comprising a matrix copolymer and a rubber substrate grafted with a superstrate copolymer wherein the copolymer consists of from 20 to 40 parts by weight of a monomer selected from the group consisting of methyl methacrylate and acrylonitrile and 80 to 60 parts by weight of a vinyl aromatic monomer, wherein the substrate rubber has a glass transition temperature below 0° C., wherein the monomers are polymerized in the presence of and grafted onto the substrate rubber, wherein the weight percent of the rubber is in the range from 5 to 50% by weight based on the weight of the grafted polymer composition; and (2) a polymer consists of a vinyl aromatic monomer and an unsaturated nitrile in a weight ratio of 80:20 to 60:40 respectively; and wherein the weight percent for Componets (A), (B) and (C) is based on the total amount of Components (A), (B) and (C) in the polyblend.
References Cited (Backward Citations)
US4021510A
Cited
US4104325A
Cited
US4059561A
Cited
US4167543A
Cited
US4197376A
Cited
US4305869A
Cited
US4298716A
Cited
US4310637A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-04-24 | 1987-10-24 | 1988-04-24 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-04-24 | 1991-10-24 | 1992-04-24 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-04-24 | 1995-10-24 | 1996-04-24 | $7700.00 | Window Closed / Lapsed |