Abstract A synthetic resin bottle produced by blow-molding a parison of a synthetic resin. In the blow-molding process of the parison, the portion of the parison supporting the handle is prevented from being expanded, thereby to sufficiently increase the supporting strength of the handle. Since the bottle product has its drum recessed in the vicinity of the handle, the grip of the handle can be facilitated.
Inventors
- 👤 Tadao Saito
- 👤 Masao Akutsu
- 👤 Hiroaki Sugiura
- 👤 Shuzo Endo
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 19:50
CPC Classifications
B; B29; B29C; B29C49/00; B29C49/42; B29C49/48; B29C49/071; B65; B65D; B65D1/00; B65D1/02; B65D1/0223; B65D23/00; B65D23/10; B29C2049/4879; B29C2049/4882; B29C2049/48825; B29C2949/00; B29C2949/07; B29C2949/0715; B29C2949/072; B29C2949/0721; B29C2949/0723; B29C2949/0724; B29C2949/073; B29C2949/0733; B29C2949/074; B29C2949/0747; B29C2949/076; B29C2949/0761; B29C2949/0763; B29C2949/0768; B29C2949/077; B29C2949/0772; B29C2949/0773; B29C2949/0778; B29C2949/0779; B29C2949/078; B29C2949/079; B29C2949/0791; B29C2949/20; B29C2949/22; B29C2949/24; B29C2949/26; B29C2949/28; B29C49/02; B29C49/06; B29K; B29K2105/00; B29K2105/25; B29K2105/253; B29L; B29L2031/00; B29L2031/46; B29L2031/463; B65D2501/00; B65D2501/0009; B65D2501/0018; B65D2501/0036
Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
173 words
A method of forming a nonsymmetrical container having walls of equal thickness, comprising the steps of: forming a parison having a top portion, a central portion, a lower portion, and a handle extending laterally of said top portion and said central portion, said parison defining an axially off-center annular cavity in its central section whereby said central section is formed with a first thin wall portion adjacent said handle and a circumferentially opposing second wall portion thicker than said first wall portion; heating at least said central and lower portion of said parison; placing said parison in at least one mold defining the shape of said nonsymmetrical container such that said thin wall portion lies in direct contact with said mold; and inserting a blow pipe into said parison and blowing air under high pressure into said parison, said thin wall portion being prevented from undesirable expansion by said contact with said mold while said central and lower portions other than said thin wall portion expand and are biaxially oriented upon said blowing.
Claim 2
Independent Claim
173 words
A method of forming a nonsymmetrical container having walls of equal thickness, comprising the steps of: forming a parison having a top portion, a central portion, a lower portion, and a handle extending laterally of said top portion and said central portion, said parison defining an axially off-center annular cavity in its central section whereby said central section is formed with a first thin wall portion adjacent said handle and a circumferentially opposing second wall portion thicker than said first wall portion; heating at least said central and lower portion of said parison; placing said parison in at least one mold defining the shape of said nonsymmetrical container such that said thin wall portion lies in direct contact with said mold; and inserting a blow pipe into said parison and blowing air under high pressure into said parison, said thin wall portion being prevented from undesirable expansion by said contact with said mold while said central and lower portions other than said thin wall portion expand and are biaxially oriented upon said blowing.
Claim 3
Dependent Claim
22 words
A method according to claim 1 wherein only the central and lower portion of said parison is placed in a blow mold.
Claim 4
Dependent Claim
18 words
A method according to claim 1 wherein said blow pipe defines a plurality of openings about its surface.
Claim 5
Dependent Claim
14 words
A method according to claim 1 wherein said blow pipe biaxially stretches said parison.
Claim 6
Dependent Claim
19 words
A method according to claim 1 wherein said parison is composed of a synthetic resin and is injection molded.
Claim 7
Dependent Claim
22 words
A method according to claim 1 wherein said handle has a portion which encircles said top portion acting as a strengthening rib.
Claim 8
Dependent Claim
39 words
A method according to claim 1 wherein the cavity wall of said blow mold defines at least one annular groove such that a parison molded in such cavity will bear in its final form at least one strengthening rib.
Claim 9
Independent Claim
160 words
A method of forming a nonsymmetrical container having walls of equal thickness, comprising the steps of: forming a parison having a neck portion and a base portion and a handle extending laterally of said neck portion and said base portion, said parison defining a nonsymmetrical cavity which lies longitudinally within said neck portion and said base portion, whereby a wall portion of said base portion adjacent said handle is thinner than at least the circumferentially opposite wall of said parison; heating at least said base portion of said parison; placing said parison in at least one mold defining the shape of said nonsymmetrical container such that said thin wall portion lies in direct contact with said mold; and inserting a blow pipe into said parison and blowing air under high pressure into said parison to expand and biaxially orient said base portion other than said thin wall portion which is prevented from undesirable expansion by said contact with said mold.
Claim 10
Independent Claim
160 words
A method of forming a nonsymmetrical container having walls of equal thickness, comprising the steps of: forming a parison having a neck portion and a base portion and a handle extending laterally of said neck portion and said base portion, said parison defining a nonsymmetrical cavity which lies longitudinally within said neck portion and said base portion, whereby a wall portion of said base portion adjacent said handle is thinner than at least the circumferentially opposite wall of said parison; heating at least said base portion of said parison; placing said parison in at least one mold defining the shape of said nonsymmetrical container such that said thin wall portion lies in direct contact with said mold; and inserting a blow pipe into said parison and blowing air under high pressure into said parison to expand and biaxially orient said base portion other than said thin wall portion which is prevented from undesirable expansion by said contact with said mold.
References Cited (Backward Citations)
US688924A
Cited
FR1192475A
Cited
US2831593A
Cited
US2831594A
Cited
GB818618A
Cited
US3050773A
Cited
US3294883A
Cited
US3029471A
Cited
GB1003019A
Cited
FR1310519A
Cited
CH386268A
Cited
US3278666A
Cited
GB1053729A
Cited
US3589542A
Cited
US3900120A
Cited
US4024975A
Cited
US4042657A
Cited
US4046275A
Cited
US4280859A
Cited
US4280805A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-03-27 | 1987-09-26 | 1988-03-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-03-27 | 1991-09-26 | 1992-03-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-03-27 | 1995-09-26 | 1996-03-27 | $7700.00 | Window Closed / Lapsed |