Abstract

Abstract Method for vacuum-tight butt joining by brazing a stainless steel part to a ceramic part, in particular stainless steel end caps to a ceramic housing of a vacuum switch, in which the stainless steel part is annealed prior to the brazing step and the portion of the stainless steel part directly adjoining the ceramic part at the brazing joint location is of a thickness not exceeding 0.8 mm and a height between about 4 and 12 mm.

Inventors

  • 👤 Joseph H. F. G. Lipperts

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 05:15
CPC Classifications
H; H01; H01H; H01H33/00; H01H33/60; H01H33/66; H01H33/662; H01H33/66207; B; B23; B23K; B23K1/00; B23K1/19; C; C04; C04B; C04B37/00; C04B37/02; C04B37/023; C04B37/026; H01H11/00; C04B2235/00; C04B2235/65; C04B2235/656; C04B2235/6567; C04B2237/00; C04B2237/02; C04B2237/12; C04B2237/30; C04B2237/32; C04B2237/34; C04B2237/343; C04B2237/40; C04B2237/405; C04B2237/406; C04B2237/50; C04B2237/52; C04B2237/525; C04B2237/70; C04B2237/704; C04B2237/706; C04B2237/76; C04B2237/765; H01H2033/66215

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 101 words
A method for producing a vacuum-tight butt brazing joint between a metallized ceramic part and a stainless steel part, said method comprising the steps of (a) shaping the end portion of the stainless steel part to be joined with the metallized ceramic part such that it has a height of from about 4 mm to about 12 mm and a maximum thickness along this height of 0.8 mm, (b) annealing at least said shaped end portion of said stainless steel part, and (c) brazing said annealed and shaped end portion of said stainless steel part directly to said metallized ceramic part.
Claim 2
Independent Claim 101 words
A method for producing a vacuum-tight butt brazing joint between a metallized ceramic part and a stainless steel part, said method comprising the steps of (a) shaping the end portion of the stainless steel part to be joined with the metallized ceramic part such that it has a height of from about 4 mm to about 12 mm and a maximum thickness along this height of 0.8 mm, (b) annealing at least said shaped end portion of said stainless steel part, and (c) brazing said annealed and shaped end portion of said stainless steel part directly to said metallized ceramic part.
Claim 3
Dependent Claim 39 words
The method as defined in claim 1 wherein said stainless steel part is composed of austenitic stainless steel, and wherein the annealing in step (b) is conducted in an evacuated, oil-free environment and at a temperature of 1050° C.
Claim 4
Dependent Claim 45 words
The method as defined in claim 2 wherein the time period during which the annealing in step (b) is conducted based on the thickness of the end portion of said stainless steel part in a ratio of about 1 hour per 1 mm of thickness.
Claim 5
Dependent Claim 22 words
The method as defined in claim 1 wherein the brazing in step (c) is conducted at a temperature of about 800° C.
Claim 6
Dependent Claim 31 words
The method as defined in claim 1 wherein the ratio between the thickness of the end portion of said stainless steel part and its height is between about 1 and 10.
Claim 7
Dependent Claim 21 words
The method as defined in claim 1 wherein the ceramic material includes at least 95% of Al 2 O 3 .
Claim 8
Independent Claim 182 words
A method of producing a vacuum switch including a metallized ceramic housing and two stainless steel caps, said two stainless steel caps being joined to said metallized ceramic housing by separate vacuum-tight butt brazing joints, said method being produced by the steps of (a) providing a metallized tubular ceramic housing which has opposite annular end surfaces, (b) providing two stainless steel caps, each including a head part and a tubular part extending away from the head part, the tubular part defining a free annular end surface opposite the head part, (c) shaping the tubular part of each of said two stainless steel caps such that the portion thereof which extends from the associated free annular end surface to a location therealong about 4 mm to about 12 mm towards the associated head part has a thickness of 0.8 mm, (d) annealing at least said portion of each of said two stainless steel caps, and (e) brazing the respective free annular end surfaces of said two stainless steel caps directly to the respective opposite annular end surfaces of said metallized tubular ceramic housing.
Claim 9
Independent Claim 182 words
A method of producing a vacuum switch including a metallized ceramic housing and two stainless steel caps, said two stainless steel caps being joined to said metallized ceramic housing by separate vacuum-tight butt brazing joints, said method being produced by the steps of (a) providing a metallized tubular ceramic housing which has opposite annular end surfaces, (b) providing two stainless steel caps, each including a head part and a tubular part extending away from the head part, the tubular part defining a free annular end surface opposite the head part, (c) shaping the tubular part of each of said two stainless steel caps such that the portion thereof which extends from the associated free annular end surface to a location therealong about 4 mm to about 12 mm towards the associated head part has a thickness of 0.8 mm, (d) annealing at least said portion of each of said two stainless steel caps, and (e) brazing the respective free annular end surfaces of said two stainless steel caps directly to the respective opposite annular end surfaces of said metallized tubular ceramic housing.

References Cited (Backward Citations)

US3371406A Cited
US4148973A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-03-13 1987-09-12 1988-03-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-03-13 1991-09-12 1992-03-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-03-13 1995-09-12 1996-03-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag