← Back to Patent Explorer
US4432826A Expired / Lapsed US ⏱️ 0.0 years remaining

Coextrusion method and apparatus

Assignee: Health-Ex Corp
•
Filing: 1982-07-26
•
Granted: 1984-02-21
•
Expires: 2002-07-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A coextruded film having an integral tear path is provided such that the tear path has a thickness that is smaller than the overall thickness of the coextruded film, said product being formed by a method and on an apparatus that introduces an elongated void in at least one of the extrudates before being combined with other extrudates into the coextruded film, said elongated void accounting for the reduced thickness of the tear path.

Inventors

  • 👤 Walter P. Scarberry
  • 👤 Charles K. Vollman

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 02:30
CPC Classifications
B; B29; B29C; B29C37/00; B29C37/0053; B29C37/0057; B29C48/00; B29C48/001; B29C48/0013; B29C48/0014; B29C48/0015; B29C48/03; B29C48/07; B29C48/08; B29C48/09; B29C48/10; B29C48/16; B29C48/18; B29C48/21; B29C48/25; B29C48/30; B29C48/305; B29C48/32; B29C48/335; B29C48/337; B29C48/338; B65; B65D; B65D75/00; B65D75/52; B65D75/58; B65D75/5827; Y; Y10; Y10T; Y10T156/00; Y10T156/10; Y10T156/1052; Y10T156/1056; Y10T156/1062; Y10T156/1064; Y10T156/12

Claims Analysis

Total Claims: 29
Claim 1
Independent Claim 153 words
A method for providing a coextruded film having a tear path with a thickness less than the coextruded film thickness, comprising: coextruding a plurality of molten extrudates into a zone wherein the multiple extrudates are combined into a multiple ply coextrusion of at least two non-tacky polymer films; interrupting the extrusion path of at least one of the molten extrudates, said interrupting step preventing extrudate flow at a narrow location in order to form an elongated void in said at least one molten extrudate and in the non-tacky polymer film formed from said molten extrudate, said interrupting being carried out before the multiple extrudates are combined into the multiple ply coextrusion; and combining said plurality of molten extrudates into a multiple ply coextruded film having at least one tear path at the location of each elongated void, said tear path having an overall thickness less than the thickness of the coextruded non-tacky film.
Claim 2
Independent Claim 153 words
A method for providing a coextruded film having a tear path with a thickness less than the coextruded film thickness, comprising: coextruding a plurality of molten extrudates into a zone wherein the multiple extrudates are combined into a multiple ply coextrusion of at least two non-tacky polymer films; interrupting the extrusion path of at least one of the molten extrudates, said interrupting step preventing extrudate flow at a narrow location in order to form an elongated void in said at least one molten extrudate and in the non-tacky polymer film formed from said molten extrudate, said interrupting being carried out before the multiple extrudates are combined into the multiple ply coextrusion; and combining said plurality of molten extrudates into a multiple ply coextruded film having at least one tear path at the location of each elongated void, said tear path having an overall thickness less than the thickness of the coextruded non-tacky film.
Claim 3
Dependent Claim 167 words
In a method for providing a coextruded film having a tear path with a thickness less than the coextruded film thickness, including coextruding a plurality of molten extrudates into a zone wherein the multiple extrudates are combined into a multiple ply coextrusion of at least two non-tacky polymer films, and combining said plurality of molten extrudates into a multiple ply coextruded film of said non-tacky polymer films, said multiple ply coextruded film having at least one tear path that has an overall thickness less than the thickness of the coextruded film, the improvement comprising: interrupting the extrusion path of at least one of the molten extrudates before the multiple extrudates are combined into the multiple ply coextrusion of non-tacky polymer films, said interrupting step preventing extrudate flow at a preselected location in order to form an elongated void in said molten extrudate and in the non-tacky polymer film formed from said molten extrudate, which elongated void forms said tear path in the non-tacky coextruded multiple ply film.
Claim 4
Dependent Claim 167 words
In a method for providing a coextruded film having a tear path with a thickness less than the coextruded film thickness, including coextruding a plurality of molten extrudates into a zone wherein the multiple extrudates are combined into a multiple ply coextrusion of at least two non-tacky polymer films, and combining said plurality of molten extrudates into a multiple ply coextruded film of said non-tacky polymer films, said multiple ply coextruded film having at least one tear path that has an overall thickness less than the thickness of the coextruded film, the improvement comprising: interrupting the extrusion path of at least one of the molten extrudates before the multiple extrudates are combined into the multiple ply coextrusion of non-tacky polymer films, said interrupting step preventing extrudate flow at a preselected location in order to form an elongated void in said molten extrudate and in the non-tacky polymer film formed from said molten extrudate, which elongated void forms said tear path in the non-tacky coextruded multiple ply film.
Claim 5
Dependent Claim 23 words
The method of claim 1 or 2, wherein said interrupting step takes place prior to cooling said molten extrudates into said coextruded film.
Claim 6
Dependent Claim 21 words
The method of claim 1 or 2, wherein said interrupting step is carried out shortly after completion of said extruding step.
Claim 7
Dependent Claim 20 words
The method of claim 1 or 2, wherein said interrupting step is carried out generally simultaneously with said extruding step.
Claim 8
Dependent Claim 29 words
The method of claim 1 or 2, wherein said interrupting step forms an elongated void completely through the molten extrudate by interposing a stationary tine in said extrusion path.
Claim 9
Dependent Claim 30 words
The method of claim 1 or 2, wherein said interrupting step forms an elongated void completely through the molten extrudate by interposing a tine generally parallel to said extrusion path.
Claim 10
Dependent Claim 25 words
The method of claim 1 or 2, wherein said interrupting step interposes a reciprocating member in said extrusion path to form a discontinuous elongated void.
Claim 11
Dependent Claim 17 words
The method of claim 1 or 2, wherein said extruding step forms extrudates of differing visible appearance.
Claim 12
Dependent Claim 17 words
The method of claim 1 or 2, wherein said extruding step forms extrudates of differing polymer materials.
Claim 13
Dependent Claim 15 words
The method of claim 1 or 2, wherein said extruding step is a sheet extrusion.
Claim 14
Dependent Claim 15 words
The method of claim 1 or 2, wherein said extruding step is a blown extrusion.
Claim 15
Independent Claim 137 words
An apparatus for forming a coextruded film having a tear path therein, including means for coextruding at least two distinct extrudate flows of non-tacky polymer films, said extruding means having at least two extrudate outlet orifices; means for combining each of said extrudate flows and for forming a coextruded flow; means for transforming said coextruded flow into a coextruded film having multiple plies of non-tacky polymer films; and means for providing a tear path in said coextruded film, said tear path having a thickness less than the overall thickness of the coextruded film; in combination with the improvement comprising: means for interrupting at least one of said extrudate flows of non-tacky polymer film to form an elongated void in the non-tacky coextruded polymer film, said interrupting means being upstream of said combining means and said transforming means.
Claim 16
Independent Claim 137 words
An apparatus for forming a coextruded film having a tear path therein, including means for coextruding at least two distinct extrudate flows of non-tacky polymer films, said extruding means having at least two extrudate outlet orifices; means for combining each of said extrudate flows and for forming a coextruded flow; means for transforming said coextruded flow into a coextruded film having multiple plies of non-tacky polymer films; and means for providing a tear path in said coextruded film, said tear path having a thickness less than the overall thickness of the coextruded film; in combination with the improvement comprising: means for interrupting at least one of said extrudate flows of non-tacky polymer film to form an elongated void in the non-tacky coextruded polymer film, said interrupting means being upstream of said combining means and said transforming means.
Claim 17
Dependent Claim 23 words
The apparatus of claim 13, wherein said transforming means includes cooling means for reducing the temperature of said extrudate flows and coextruded flow.
Claim 18
Dependent Claim 18 words
The apparatus of claim 13, wherein said interrupting means blocks said extrudate flow at a narrow location therealong.
Claim 19
Dependent Claim 12 words
The apparatus of claim 13, wherein said interrupting means includes a tine.
Claim 20
Dependent Claim 13 words
The apparatus of claim 13, wherein said interrupting means includes a stationary tine.
Claim 21
Dependent Claim 18 words
The apparatus of claim 13, wherein said interrupting means includes a tine rigidly mounted to said coextruding means.
Claim 22
Dependent Claim 23 words
The apparatus of claim 13, wherein said interrupting means includes a tine rigidly mounted to at least one of said extrudate outlet orifices.
Claim 23
Dependent Claim 26 words
The apparatus of claim 13, wherein said interrupting means includes reciprocating means having a member that alternates between an extended interrupting position and a retracted position.
Claim 24
Dependent Claim 26 words
The apparatus of claim 13, wherein said interrupting means includes a member having a length at least as great as the height of the outlet orifice.
Claim 25
Dependent Claim 17 words
The apparatus of claim 13, wherein said interrupting means includes a member positioned within the outlet orifice.
Claim 26
Dependent Claim 20 words
The apparatus of claim 13, wherein said interrupting means includes an elongated member positioned generally parallel to the extrudate flow.
Claim 27
Dependent Claim 15 words
The apparatus of claim 13, wherein said coextruding means coextrudes a film in sheet form.
Claim 28
Dependent Claim 15 words
The apparatus of claim 13, wherein said coextruding means coextrudes a film in cylindrical form.
Claim 29
Dependent Claim 18 words
The apparatus of claim 13, wherein said interrupting means forms an elongated void completely through the extrudate flow.

References Cited (Backward Citations)

CA719189A Cited
US3186628A Cited
US3369267A Cited
US3368740A Cited
US3535409A Cited
US3533550A Cited
US3523859A Cited
US3640381A Cited
US3790744A Cited
US3909582A Cited
US3939972A Cited
US4379806A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-02-20 1987-08-22 1988-02-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-02-20 1991-08-22 1992-02-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-02-20 1995-08-22 1996-02-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags