High temperature circuit board

Assignee: ELITE CIRCUITS Inc A CORP OF CALIFORNIA
•
Filing: 1981-09-04
•
Granted: 1984-01-03
•
Expires: 2001-09-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A high temperature circuit board made by flame spraying a high temperature resistant metal film, such as aluminum, zinc or silver solder braze alloy, onto a high temperature resistant insulative substrate in which in one embodiment a reverse circuit image resist is layed on the board surface and the metal is flame sprayed onto the board surface and the reverse image resist screen is then removed leaving the circuit without etching. In the other embodiment aluminum is flame sprayed onto the substrate and then a silver solder braze alloy or copper or nickel is flame sprayed onto the aluminum film, and then resist and etching stops are applied to remove unwanted metal to the substrate and the resist is stripped providing the high temperature printed circuit board.

Inventors

  • 👤 Vito D. Elarde

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 20:56
CPC Classifications
H; H05; H05K; H05K3/00; H05K3/22; H05K3/24; H05K1/00; H05K1/02; H05K1/09; H05K3/10; H05K3/14; H05K2201/00; H05K2201/03; H05K2201/0332; H05K2201/0335; H05K2201/0338; H05K2203/00; H05K2203/13; H05K2203/1333; H05K2203/1344; H05K3/02; H05K3/06; H05K3/143; H05K3/38; H05K3/388

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 158 words
A high temperature performance circuit board comprising: an insulating board of high temperature resistant material, said high temperature resistant material selected from the group consisting of polyimide, modified polyimide and epoxy glass bonded laminate, and a metal circuit of conductive metal flame sprayed on said board, said metal circuit comprising a first layer of aluminum, and a second metal layer selected from the group consisting of nickel, copper, silver solder brazed alloy comprising about 20% to 45% silver and 30% to 52.5% copper and 22.5% to 35% zinc, an alloy of about 5% to 15% silver and 80% to 89% copper and 5% to 6% phosphorous, an alloy of about 5% to 9% silver and 53% to 58% copper and 37% to 38% zinc, an alloy of about 7% silver and 85% copper and 8% tin, an alloy of about 60% copper and 40% zinc, and an alloy of about 50% copper and 40% zinc and 10% nickel.
Claim 2
Dependent Claim 158 words
A high temperature performance circuit board comprising: an insulating board of high temperature resistant material, said high temperature resistant material selected from the group consisting of polyimide, modified polyimide and epoxy glass bonded laminate, and a metal circuit of conductive metal flame sprayed on said board, said metal circuit comprising a first layer of aluminum, and a second metal layer selected from the group consisting of nickel, copper, silver solder brazed alloy comprising about 20% to 45% silver and 30% to 52.5% copper and 22.5% to 35% zinc, an alloy of about 5% to 15% silver and 80% to 89% copper and 5% to 6% phosphorous, an alloy of about 5% to 9% silver and 53% to 58% copper and 37% to 38% zinc, an alloy of about 7% silver and 85% copper and 8% tin, an alloy of about 60% copper and 40% zinc, and an alloy of about 50% copper and 40% zinc and 10% nickel.
Claim 3
Dependent Claim 139 words
A circuit board comprising: an insulating board of heat resistant material, and a metal circuit flame sprayed on said board, said metal circuit comprising a first thin layer of a bond enhancing material and a second layer consisting of a metal selected from the group consisting of nickel, copper, silver solder brazed alloy comprising about 20% to 45% silver and 30% to 52.5% copper and 22.5% to 35% zinc, an alloy of about 5% to 15% silver and 80% to 89% copper and 5% to 6% phosphorous, an alloy of about 5% to 9% silver and 53% to 58% copper and 37% to 38% zinc, an alloy of about 7% silver and 85% copper and 8% tin, an alloy of about 60% copper and 40% zinc, and an alloy of about 50% copper and 40% zinc and 10% nickel.
Claim 4
Dependent Claim 139 words
A circuit board comprising: an insulating board of heat resistant material, and a metal circuit flame sprayed on said board, said metal circuit comprising a first thin layer of a bond enhancing material and a second layer consisting of a metal selected from the group consisting of nickel, copper, silver solder brazed alloy comprising about 20% to 45% silver and 30% to 52.5% copper and 22.5% to 35% zinc, an alloy of about 5% to 15% silver and 80% to 89% copper and 5% to 6% phosphorous, an alloy of about 5% to 9% silver and 53% to 58% copper and 37% to 38% zinc, an alloy of about 7% silver and 85% copper and 8% tin, an alloy of about 60% copper and 40% zinc, and an alloy of about 50% copper and 40% zinc and 10% nickel.

References Cited (Backward Citations)

US2861911A Cited
US2876530A Cited
US3023390A Cited
US3680209A Cited
US3891901A Cited
US3666617A Cited
US3811934A Cited
US3781596A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-01-02 1987-07-04 1988-01-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-01-02 1991-07-04 1992-01-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-01-02 1995-07-04 1996-01-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag