Method for making a self-lubricating liner

Assignee: Verbatim Corp
•
Filing: 1982-07-01
•
Granted: 1983-12-06
•
Expires: 2002-07-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An improved floppy disk having a liner material into the fibers of which has been compounded identically the same lubricant as that compounded into the surface of the magnetic recording disk.

Inventors

  • 👤 Lawrence G. Martinelli

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 21:40
CPC Classifications
G; G11; G11B; G11B23/00; G11B23/50; G11B23/505; G11B23/02; G11B23/03; G11B23/033; G11B23/0332; Y; Y10; Y10S; Y10S428/00; Y10S428/90

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 132 words
An improved method for manufacturing a lubricated liner for a floppy disk assembly of the type wherein the assembly includes a disk provided with a magnetic coating including a lubricant compounded therein, the improvement comprising the steps of: infusing a lubricant, identical to the lubricant compounded into the magnetic coating of the disk, into a precursor material; extruding fibers from the lubricant-infused precursor material; and binding the extruded fibers together to form a fibrous liner for abutting against the coating surface of the disk; wherein said lubricant infused into said precursor material is of a quantity sufficient to produce the result that, for the finished floppy disk assembly, migration of lubricant from said disk to said fibrous liner is substantially less than if said lubricant were not infused into said precursor material.
Claim 2
Dependent Claim 132 words
An improved method for manufacturing a lubricated liner for a floppy disk assembly of the type wherein the assembly includes a disk provided with a magnetic coating including a lubricant compounded therein, the improvement comprising the steps of: infusing a lubricant, identical to the lubricant compounded into the magnetic coating of the disk, into a precursor material; extruding fibers from the lubricant-infused precursor material; and binding the extruded fibers together to form a fibrous liner for abutting against the coating surface of the disk; wherein said lubricant infused into said precursor material is of a quantity sufficient to produce the result that, for the finished floppy disk assembly, migration of lubricant from said disk to said fibrous liner is substantially less than if said lubricant were not infused into said precursor material.
Claim 3
Dependent Claim 137 words
An improved method for manufacturing a lubricated liner for a floppy disk assembly of the type wherein the assembly includes a disk provided with a magnetic coating including a lubricant compounded therein, the improvement comprising the steps of: thoroughly mixing a lubricant, identical to the lubricant compounded into the magnetic coating of the disk, into a solution of binder material; and applying the binder material-lubricant mixture to a mass of loose fibers to bind said fibers into a fibrous liner for abutting against the coated surface of the disk; wherein said lubricant mixed into said binder material is of a quantity sufficient to produce the result that, for the finished floppy disk assembly, migration of lubricant from said disk to said fibrous liner is substantially less than if said lubricant were not mixed into said binder material.
Claim 4
Dependent Claim 137 words
An improved method for manufacturing a lubricated liner for a floppy disk assembly of the type wherein the assembly includes a disk provided with a magnetic coating including a lubricant compounded therein, the improvement comprising the steps of: thoroughly mixing a lubricant, identical to the lubricant compounded into the magnetic coating of the disk, into a solution of binder material; and applying the binder material-lubricant mixture to a mass of loose fibers to bind said fibers into a fibrous liner for abutting against the coated surface of the disk; wherein said lubricant mixed into said binder material is of a quantity sufficient to produce the result that, for the finished floppy disk assembly, migration of lubricant from said disk to said fibrous liner is substantially less than if said lubricant were not mixed into said binder material.

References Cited (Backward Citations)

US3455864A Cited
US3779918A Cited
US3781205A Cited
US3985661A Cited
US4056478A Cited
US4065798A Cited
US4106067A Cited
JPS53110980A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-12-05 1987-06-06 1987-12-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-12-05 1991-06-06 1991-12-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-12-05 1995-06-06 1995-12-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag