Abstract

Abstract A glass faceplate having a central area of required useful diameter surrounded by a narrow ring of opaque glass and an outer glass mounting flange. Light entering the flange or ring is prevented from reaching the central area as stray light or glare in the system and spurious reflections at the interface of the ring and central area are minimized by a refractive index match of the two innermost glasses.

Inventors

  • 👤 Walter P. Siegmund

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 18:59
CPC Classifications
H; H01; H01J; H01J29/00; H01J29/86; H01J29/89; C; C03; C03B; C03B23/00; C03B23/04; C03B23/047; H01J2229/00; H01J2229/89; H01J2229/8913

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 79 words
The method of making faceplates for image intensifiers comprising the steps of: grinding and polishing the side of a glass rod; assembling against said rod a closely related succession of relatively thin pieces of light-absorbing glass; fitting a tube of supporting glass over said assembly of pieces and rod; heating and stretching the resulting faceplate preform into a boule; annealing and transaxially slicing flat plates from said boule; and machining said flat plates to configurations desired of said faceplates.
Claim 2
Independent Claim 79 words
The method of making faceplates for image intensifiers comprising the steps of: grinding and polishing the side of a glass rod; assembling against said rod a closely related succession of relatively thin pieces of light-absorbing glass; fitting a tube of supporting glass over said assembly of pieces and rod; heating and stretching the resulting faceplate preform into a boule; annealing and transaxially slicing flat plates from said boule; and machining said flat plates to configurations desired of said faceplates.
Claim 3
Dependent Claim 33 words
The method according to claim 1 wherein said glass rod is formed to a diametral dimension greater than 18 mm and said preform is drawn to a boule diameter of approximately 18 mm.
Claim 4
Dependent Claim 38 words
The method according to claim 2 wherein the thickness of pieces of said light-absorbing glasses of said preform are such as to approximate 1 mm when said preform is drawn to said boule diameter of approximately 18 mm.
Claim 5
Dependent Claim 29 words
The method according to claim 1 including the step of applying a photocathode coating to one side of said drawn and sliced glass rod component of said machined plates.

References Cited (Backward Citations)

US2311704A Cited
US2455667A Cited
US3554721A Cited
GB1229528A Cited
US3877912A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-11-07 1987-05-09 1987-11-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-11-07 1991-05-09 1991-11-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-11-07 1995-05-09 1995-11-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag