Abstract

Abstract A method for manufacturing high information density storage disks, suitable for optical reading, out of transparent synthetics having a high glass temperature and high dimensional stability. The present injection molding method avoids potential double diffraction disruptive effects created by frictional or shearing forces. The synthetic material which is to be pressed is injected into one of the mold halves at a temperature that significantly exceeds the pressing temperature of the compression form and is injected so as to form a lump of the material. The pressing step wherein the compression form is closed down to a squeezing gap width is initiated prior to the termination of the injection operation. Likewise the cooling operation is initiated prior to the termination of the pressing step and both the cooling and pressing operations chronologically proceed at approximately an exponential rate.

Inventors

  • 👤 Dieter Bartholdsten
  • 👤 Hermann Koop
  • 👤 Erhard Schrode
  • 👤 Adelbert Zielasek

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 06:12
CPC Classifications
B; B29; B29C; B29C45/00; B29C45/17; B29C45/46; B29C45/56; B29C45/561; B29C43/00; B29C43/02; B29C43/021; B29C2043/023; B29C2043/025; B29C43/32; B29C43/34; B29C2043/3488; B29C43/58; B29C2043/5833; B29C2045/5615; B29C2045/562; B29C2045/565; B29L; B29L2017/00; B29L2017/001; B29L2017/003; Y; Y10; Y10S; Y10S425/00; Y10S425/81

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 298 words
In a method for manufacturing disk-shaped information carriers with a high storage density which can be optically read out, of the type manufactured out of transparent synthetics employing a molding press equipped with at least one pressing matrix, the press havng a compression form comprised of separable mold halves which can be moved towards one another and both of which have means for heating and cooling during the pressing cycle, wherein the improvement comprises: said mold halves each being provided with an annular ridge, the ridges lying opposite one another so as to form a squeezing gap when the mold is closed and serving as an outer boundary for the hollow space of the mold at which material can flow through the gap; preheating the transparent synthetic material to a temperature significantly greater than the initial pressing temperature of the compression form; injecting an excess of the preheated material than is required for the finished product into the compression form via a central aperture in one of the mold halves so as to form a lump of material; pressing the lump of material by closing the compression form to obtain a squeezing gap width with a magnitude equal to several tenths of the thickness of the finished storage disk, said squeezing gap maintaining a pressure in the pressed material while permitting excess material to squeeze therethrough, said pressing step being initiated prior to the termination of the injecting step; cooling the compression form, said cooling step being initiated prior to the termination of the pressing step; and the pressing and cooling steps chronologically proceeding in an internal sequence which approximates an exponential function so that along with the use of the squeezing gap condensation bubbles and double diffraction effects due to frictional and shearing forces are substantially avoided.
Claim 2
Dependent Claim 298 words
In a method for manufacturing disk-shaped information carriers with a high storage density which can be optically read out, of the type manufactured out of transparent synthetics employing a molding press equipped with at least one pressing matrix, the press havng a compression form comprised of separable mold halves which can be moved towards one another and both of which have means for heating and cooling during the pressing cycle, wherein the improvement comprises: said mold halves each being provided with an annular ridge, the ridges lying opposite one another so as to form a squeezing gap when the mold is closed and serving as an outer boundary for the hollow space of the mold at which material can flow through the gap; preheating the transparent synthetic material to a temperature significantly greater than the initial pressing temperature of the compression form; injecting an excess of the preheated material than is required for the finished product into the compression form via a central aperture in one of the mold halves so as to form a lump of material; pressing the lump of material by closing the compression form to obtain a squeezing gap width with a magnitude equal to several tenths of the thickness of the finished storage disk, said squeezing gap maintaining a pressure in the pressed material while permitting excess material to squeeze therethrough, said pressing step being initiated prior to the termination of the injecting step; cooling the compression form, said cooling step being initiated prior to the termination of the pressing step; and the pressing and cooling steps chronologically proceeding in an internal sequence which approximates an exponential function so that along with the use of the squeezing gap condensation bubbles and double diffraction effects due to frictional and shearing forces are substantially avoided.
Claim 3
Dependent Claim 49 words
In a method for manufacturing disk-shaped information carriers as described in claim 1, wherein an injection unit which plasticizes the synthetic material and injects it into the compression form is integrated into the molding press in order to obtain a material transport path which is as short as possible.
Claim 4
Dependent Claim 32 words
In a method for manufacturing disk-shaped information carriers as described in claim 1, wherein the hollow space of the mold, which is bounded by the annular ridges, is free of profile skips.
Claim 5
Dependent Claim 39 words
In a method for manufacturing disk-shaped information carriers as described in claim 1, wherein the amount of material injected into the compression form has a mass which is 5-8% in excess of the amount of the finished storage disk.
Claim 6
Dependent Claim 34 words
In a method for manufacturing disk-shaped information carriers as described in claim 1, wherein the diameter of the hollow space of the mold is larger than a rated diameter for the finished storage disk.
Claim 7
Dependent Claim 31 words
In a method for manufacturing disk-shaped information carriers as described in claim 5, wherein the hollow space of the mold is 5% larger than the rated diameter for the finished disk.
Claim 8
Dependent Claim 54 words
In a method for manufacturing disk-shaped information carriers as described in claim 1 and further comprising: unmolding the cooled material which has been molded into a storage disk; reducing the diameter of the unmolded storage disk utilizing a cutting means which largely avoids shearing forces to obtain a storage disk with the rated diameter.
Claim 9
Dependent Claim 24 words
In a method for manufacturing disk-shaped information carriers as described in claim 7 wherein a laser cutting device is provided as the cutting means.
Claim 10
Dependent Claim 68 words
In a method for manufacturing disk-shaped information carriers as described in claim 1, wherein the initiation and rate of cooling of the compression form are selected in such a manner that the mass viscosity of the synthetic material is increased sufficiently to compensate for the decreased flow resistance in the area of the squeezing gap and thus allow for the proper buildup of pressure in the synthetic material.
Claim 11
Dependent Claim 37 words
In a method for manufacturing disk-shaped information carriers as described in claim 1 wherein the clear height of the opened compression form has a magnitude equivalent to a multiple of the thickness of the finished storage disk.
Claim 12
Dependent Claim 41 words
In a method for manufacturing disk-shaped information carriers as described in claim 1 wherein predried polycarbonate granulate, utilized as the synthetic material, is preheated to 300° C. and injected into the compression form which has been heated to approximately 220° C.
Claim 13
Dependent Claim 91 words
In a method for manufacturing disk-shaped information carriers as described in claim 11 wherein the injection step occurs over a time period of between 0.8 seconds and 3 seconds, the pressing step occurs over a time period of approximately 2 seconds, the cooling step occurs over a time period of about 25 seconds, the closing pressure of the mold is ≦1.2 MN, the pressing step is initiated between 20-40% prior to the termination of the injection step, and the cooling step begins 20-40% prior to the termination of the pressing step.

References Cited (Backward Citations)

US3039139A Cited
US3196485A Cited
US3941547A Cited
US4302411A Cited
US4251479A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-10-10 1987-04-11 1987-10-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-10-10 1991-04-11 1991-10-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-10-10 1995-04-11 1995-10-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag