Abstract

Abstract A method for controlling the thickness of an extruded, biaxially elongated film product, in which thickness deviations are controlled automatically and without supervision. In the method, correlation between positions along the widthwise direction of a film sheet and positions of die manipulation bolts of an extrusion die is obtained, and initially, a profile of the film sheet prior to lateral elongation is converged into a tolerable range; thereafter, the thickness of the film sheet after lateral elongation is measured, and if there are thickness deviations outside the tolerable range, a thickness regulation is effected by transmitting a signal corresponding to the thickness deviations to the appropriate die manipulation bolts.

Inventors

  • 👤 Nobuhiko Kogo
  • 👤 Yoshimitsu Tsutsui
  • 👤 Koji Kato
  • 👤 Hisao Kishigami

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 16:51
CPC Classifications
G; G05; G05D; G05D5/00; G05D5/02; G05D5/03; B; B29; B29C; B29C48/00; B29C48/25; B29C48/92; B29C2948/00; B29C2948/92; B29C2948/92009; B29C2948/92114; B29C2948/92133; B29C2948/92152; B29C2948/92323; B29C2948/92428; B29C2948/92504; B29C2948/9258; B29C2948/926; B29C2948/92609; B29C2948/92647; B29C2948/92819; B29C2948/92857; B29C2948/92904; B29C48/03; B29C48/07; B29C48/08

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 98 words
A method for automatically controlling the thickness of extruded biaxially elongated films characterised in that a correlation between positions along the widthwise direction of a film sheet and positions of die manipulation bolts of an extrusion die is obtained, and initially, a profile of the film sheet prior to lateral elongation is converged into a tolerable range; therafter, the thickness of the film sheet after lateral elongation is measured, and if there are thickness deviations outside the tolerable range, a thickness regulation is effected by transmitting a signal corresponding to the thickness deviations to appropriate die manipulation bolts.
Claim 2
Independent Claim 98 words
A method for automatically controlling the thickness of extruded biaxially elongated films characterised in that a correlation between positions along the widthwise direction of a film sheet and positions of die manipulation bolts of an extrusion die is obtained, and initially, a profile of the film sheet prior to lateral elongation is converged into a tolerable range; therafter, the thickness of the film sheet after lateral elongation is measured, and if there are thickness deviations outside the tolerable range, a thickness regulation is effected by transmitting a signal corresponding to the thickness deviations to appropriate die manipulation bolts.
Claim 3
Independent Claim 166 words
A method for automatically controlling the thickness of extruded biaxially elongated films characterised in that a correlation between positions along the widthwise direction of a film sheet prior to lateral elongation and the film sheet after lateral elongation and positions of die manipulation bolts of an extrusion die is obtained, and initially, a profile of the film sheet prior to lateral elongation is converged into a tolerable range with respect to a preset profile; the thickness over the width of the film sheet after lateral elongation is then measured, and if thickness deviations are present which are outside the tolerable range, then the profile prior to lateral elongation is corrected, and the die manipulation bolts are manipulated so as to converge the profile prior to lateral elongation into a tolerable range with respect to the corrected profile; the measurement of the thickness of the film after lateral elongation is then repeated, whereby the thickness of the film sheet being produced can be continuously regulated, if necessary.
Claim 4
Independent Claim 166 words
A method for automatically controlling the thickness of extruded biaxially elongated films characterised in that a correlation between positions along the widthwise direction of a film sheet prior to lateral elongation and the film sheet after lateral elongation and positions of die manipulation bolts of an extrusion die is obtained, and initially, a profile of the film sheet prior to lateral elongation is converged into a tolerable range with respect to a preset profile; the thickness over the width of the film sheet after lateral elongation is then measured, and if thickness deviations are present which are outside the tolerable range, then the profile prior to lateral elongation is corrected, and the die manipulation bolts are manipulated so as to converge the profile prior to lateral elongation into a tolerable range with respect to the corrected profile; the measurement of the thickness of the film after lateral elongation is then repeated, whereby the thickness of the film sheet being produced can be continuously regulated, if necessary.

References Cited (Backward Citations)

US3122784A Cited
US3122783A Cited
US3212127A Cited
US3347960A Cited
US3782873A Cited
US3694726A Cited
US4124342A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-10-10 1987-04-11 1987-10-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-10-10 1991-04-11 1991-10-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-10-10 1995-04-11 1995-10-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag