US4401733A Expired / Lapsed US ⏱️ 0.0 years remaining

Alkaline galvanic cell

Assignee: Panasonic Holdings Corp
•
Filing: 1981-12-22
•
Granted: 1983-08-30
•
Expires: 2001-12-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An improved alkaline galvanic cell which includes an anode sealing plate of a layered structure serving as an anode terminal and having a copper layer as the innermost layer, a cathode container serving as a cathode terminal, an insulating packing provided around the peripheral edge of the anode sealing plate to be fitted into the cathode container for hermetically sealing the cell, and two layers of sealing agents provided between the anode sealing plate and the insulating packing. One of the layers at the side of the anode sealing plate is of epoxy adduct polyamide amine having amine valence in the range of 50 to 400, while the other of the layers at the side of the insulating packing is arranged to be of chlorosulfonated polyethylene for improvement of resistance against leakage of electrolyte.

Inventors

  • 👤 Iwao Shirai
  • 👤 Keigo Momose
  • 👤 Tadashi Sawai
  • 👤 Masakazu Komatsu
  • 👤 Takao Inoue
  • 👤 Tamotsu Wakahata

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 03:49
CPC Classifications
H; H01; H01M; H01M50/00; H01M50/10; H01M50/183; H01M50/186; H01M50/184; H01M50/19; H01M50/191; H01M50/193; H01M50/195; H01M50/197; Y; Y02; Y02E; Y02E60/00; Y02E60/10

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 128 words
An alkaline galvanic cell which comprises an anode sealing plate in the form of a layered clad plate which has a copper layer as the innermost layer thereof and in which an anode active substance is accommodated, a cathode container in which a cathode active substance is accommodated, an insulating packing provided around the peripheral edge of said anode sealing plate which is fitted into said cathode for hermetically sealing said cell, and first and second layers of sealing agents provided between said innermost copper layer of said anode sealing plate and said insulating packing, said first layer which contacts said innermost copper layer of said anode sealing plate being of epoxy adduct polyamide amine, and said second layer which contacts said insulating packing being of chlorosulfonated polyethylene.
Claim 2
Dependent Claim 128 words
An alkaline galvanic cell which comprises an anode sealing plate in the form of a layered clad plate which has a copper layer as the innermost layer thereof and in which an anode active substance is accommodated, a cathode container in which a cathode active substance is accommodated, an insulating packing provided around the peripheral edge of said anode sealing plate which is fitted into said cathode for hermetically sealing said cell, and first and second layers of sealing agents provided between said innermost copper layer of said anode sealing plate and said insulating packing, said first layer which contacts said innermost copper layer of said anode sealing plate being of epoxy adduct polyamide amine, and said second layer which contacts said insulating packing being of chlorosulfonated polyethylene.
Claim 3
Dependent Claim 36 words
An alkaline galvanic cell as claimed in claim 1, wherein said epoxy adduct polyamide amine for said first layer contains carbon powder in the range of 2 to 20% in the weight ratio with respect thereto.
Claim 4
Dependent Claim 25 words
An alkaline galvanic cell as claimed in claim 1, wherein said epoxy adduct polyamide amine has amine valence in the range of 50 to 400.
Claim 5
Dependent Claim 29 words
An alkaline galvanic cell as claimed in claim 1, wherein said anode sealing plate is of a three-layered clad plate construction having said copper layer as the innermost layer.

References Cited (Backward Citations)

US3713896A Cited
US3922178A Cited
US4248944A Cited
US4256815A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-08-29 1987-02-28 1987-08-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-08-29 1991-02-28 1991-08-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-08-29 1995-02-28 1995-08-30 $7700.00 Window Closed / Lapsed