Abstract
Abstract A method of vacuum depositing a layer on a plastic film in which the film is transported so as to pass along a metal surface moving with the film, which surface removes heat from the film, and vacuum depositing the vapor of an evaporant onto the surface of the plastic film while it is in contact with the metal surface. The film is in an electret state when it is located at the metal surface, whereby an electrostatic attractive force is produced between the film and the metal surface, thereby increasing the efficiency of heat conduction between the film and the metal.
Inventors
- 👤 Koichi Shinohara
- 👤 Takashi Fujita
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-24 08:17
CPC Classifications
C; C23; C23C; C23C14/00; C23C14/06; C23C14/14; C23C14/20; C23C14/22; C23C14/56; C23C14/562
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
160 words
A method of vacuum depositing a layer on a plastic film prior to winding the film comprising the steps of: transporting the film along a metal surface which is movable with the film, said metal surface being grounded and which metal serves to control the temperature of the film in contact therewith by conducting heat away from said film; rendering said film in an electret state with a surface potential higher than 150 V, prior to or at the same time as the film contacts the metal surface, whereby said film is electrostatically attracted to said metal surface, thereby increasing the efficiency of the heat conduction between the film and the metal surface; depositing a material on the portion of said film which is opposite the portion in contact with said metal surface; and neutralizing the surface potential of said film so as to render it into a non-electret state after said deposition step and prior to winding the film.
Claim 2
Independent Claim
160 words
A method of vacuum depositing a layer on a plastic film prior to winding the film comprising the steps of: transporting the film along a metal surface which is movable with the film, said metal surface being grounded and which metal serves to control the temperature of the film in contact therewith by conducting heat away from said film; rendering said film in an electret state with a surface potential higher than 150 V, prior to or at the same time as the film contacts the metal surface, whereby said film is electrostatically attracted to said metal surface, thereby increasing the efficiency of the heat conduction between the film and the metal surface; depositing a material on the portion of said film which is opposite the portion in contact with said metal surface; and neutralizing the surface potential of said film so as to render it into a non-electret state after said deposition step and prior to winding the film.
Claim 3
Dependent Claim
57 words
A method as claimed in claim 1, in which said source material is heated and evaporated by an electron beam bombardment, the energy of said electron being high enough to cause an electron reflected from said source material to be implanted into the film to form a static charge to render the film into an electret state.
Claim 4
Dependent Claim
20 words
A method as claimed in claim 1, in which said metal surface comprises the peripheral surface of a rotary can.
Claim 5
Dependent Claim
29 words
A method as claimed in claim 1, in which said neutralizing is performed by exposing the surface of the film reverse to the deposited layer to a glow discharge.
Claim 6
Dependent Claim
20 words
A method as claimed in claim 1, in which the surface roughness of said metal surface is smaller than 0.1μ.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1986-07-11 | 1987-01-10 | 1987-07-12 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1990-07-11 | 1991-01-10 | 1991-07-12 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1994-07-11 | 1995-01-10 | 1995-07-12 | $7700.00 | Window Closed / Lapsed |