Abstract

Abstract This invention relates to emulsion type adhesive compositions which include a metal neutralized sulfonated elastomeric co or terpolymer, wherein the neutralized sulfonated copolymer has about 5 to about 250 meq. of neutralized sulfonate groups per 100 grams of the neutralized sulfonated copolymer, and less than about 200 parts by weight of a hydrocarbon resin of a petroleum or coal tar distillate, having about 5 to 6 carbon atoms, the hydrocarbon resin being composed of aliphatic dienes and monoolefins per 100 parts by weight of the neutralized sulfonated co or terpolymer.

Inventors

  • 👤 Pawan K. Agarwal
  • 👤 S. Richard Turner
  • 👤 Robert D. Lundberg
  • 👤 Morris L. Evans

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 10:08
CPC Classifications
C; C08; C08F; C08F236/00; C08F236/02; C08F236/04; C08L; C08L95/00; C09; C09J; C09J109/00; C09J109/10

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 260 words
An adhesive composition which comprises an emulsion of: (a) a metal neutralized sulfonated elastomeric co- or terpolymer, said neutralized sulfonated co- or terpolymer having about 5 to about 250 meq. of neutralized sulfonated groups per 100 grams of said metal neutralized sulfonated co- or terpolymer, wherein said metal neutralized sulfonated elastomeric co- or terpolymer comprises at least 80% by weight of at least one conjugated diene having from 4 to 12 carbon atoms or a combination of at least 80% by weight of at least one conjugated diene and styrene, wherein the combination contains less than 50 weight percent styrene of the total 80 weight percent and a minor proportion of a metal or amine neutralized sulfonate monomer characterized by the formula: ##STR6## where X is aromatic, and Y is a cation selected from Groups IA, IIA, IB and IIB of the Periodic Table or an amine of the formula: ##STR7## where R 1 and R 2 can be aliphatic groups of C 1 to C 12 or hydrogen, said co- or terpolymer being water insoluble, substantially gel-free, thermally stable and oxidatively stable having at least 0.5 weight percent chemically combined to less than 5 weight percent chemically combined sulfur, with a reduced viscosity as measured in a solvent at a concentration of 10 gm/liter of greater than 0.2 and less than 5.0; and (b) about 25 to about 700 parts by weight of a hydrocarbon tackifying resin based on a petroleum or coal tar distillate per 100 parts by weight of said metal neutralized sulfonated elastomeric co- or terpolymer.
Claim 2
Dependent Claim 260 words
An adhesive composition which comprises an emulsion of: (a) a metal neutralized sulfonated elastomeric co- or terpolymer, said neutralized sulfonated co- or terpolymer having about 5 to about 250 meq. of neutralized sulfonated groups per 100 grams of said metal neutralized sulfonated co- or terpolymer, wherein said metal neutralized sulfonated elastomeric co- or terpolymer comprises at least 80% by weight of at least one conjugated diene having from 4 to 12 carbon atoms or a combination of at least 80% by weight of at least one conjugated diene and styrene, wherein the combination contains less than 50 weight percent styrene of the total 80 weight percent and a minor proportion of a metal or amine neutralized sulfonate monomer characterized by the formula: ##STR6## where X is aromatic, and Y is a cation selected from Groups IA, IIA, IB and IIB of the Periodic Table or an amine of the formula: ##STR7## where R 1 and R 2 can be aliphatic groups of C 1 to C 12 or hydrogen, said co- or terpolymer being water insoluble, substantially gel-free, thermally stable and oxidatively stable having at least 0.5 weight percent chemically combined to less than 5 weight percent chemically combined sulfur, with a reduced viscosity as measured in a solvent at a concentration of 10 gm/liter of greater than 0.2 and less than 5.0; and (b) about 25 to about 700 parts by weight of a hydrocarbon tackifying resin based on a petroleum or coal tar distillate per 100 parts by weight of said metal neutralized sulfonated elastomeric co- or terpolymer.
Claim 3
Dependent Claim 18 words
An adhesive composition according to claim 1, wherein said sulfonate containing monomer is a metal neutralized sulfonated styrene.
Claim 4
Dependent Claim 27 words
An adhesive composition according to claims 2 or 1, wherein said conjugated diene is selected from the group consisting of 1,3-butadiene, isoprene and chloroprene and mixtures thereof.
Claim 5
Dependent Claim 15 words
An adhesive composition according to claims 2 or 1, wherein said conjugated diene is 1,3-butadiene.
Claim 6
Dependent Claim 15 words
An adhesive composition according to claims 2 or 1, wherein said conjugated diene is isoprene.

References Cited (Backward Citations)

US3801531A Cited
US3867247A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-06-06 1986-12-06 1987-06-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-06-06 1990-12-06 1991-06-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-06-06 1994-12-06 1995-06-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag