Abstract

Abstract Printing cylinder with an outside covering of a thermoplastic elastomeric composition which can be hardened by exposure to light, the covering being snugly applied to the circumference of the cylinder by suction in the annular clearance between cylinder and covering; the cylinder comprising several coaxial parts during the covering process, only the central portion with its covering forming the printing cylinder.

Inventors

  • 👤 Hendricus H. van der Velden

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 20:25
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/16; G03F7/18; B; B29; B29C; B29C37/00; B29C37/0078; B29C37/0082; B29C63/00; B29C63/18; B29C63/20; B41; B41C; B41C1/00; B41C1/18; B41N; B41N1/00; B41N1/16; B41N1/22; B29L; B29L2031/00; B29L2031/32; B29L2031/324; Y; Y10; Y10T; Y10T156/00; Y10T156/10; Y10T156/1002; Y10T156/1028; Y10T156/1033

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 151 words
A method for forming a printing cylinder comprising the steps of completely covering the outer surface of a cylinder with a closely fitting layer of a thermoplastic elastomeric composition adapted to be hardened by exposure to light, maintaining a space between said cylinder and said layer by the provision of a pattern of interconnected cavities or channels on said outer surface of said cylinder, enveloping the outer side of the layer with a flexible film of gas-tight material after application of the layer, applying a vacuum to said space for removing any accumulated gases, and thereafter heating said cylinder and said covered layer for 10 to 120 min. at a temperature of 100° to 150° C., while maintaining the vacuum, thereafter removing the application of vacuum and the film, and further heating said cylinder and said covered layer for 10 to 60 min. at a temperature of 100° to 150° C.
Claim 2
Independent Claim 151 words
A method for forming a printing cylinder comprising the steps of completely covering the outer surface of a cylinder with a closely fitting layer of a thermoplastic elastomeric composition adapted to be hardened by exposure to light, maintaining a space between said cylinder and said layer by the provision of a pattern of interconnected cavities or channels on said outer surface of said cylinder, enveloping the outer side of the layer with a flexible film of gas-tight material after application of the layer, applying a vacuum to said space for removing any accumulated gases, and thereafter heating said cylinder and said covered layer for 10 to 120 min. at a temperature of 100° to 150° C., while maintaining the vacuum, thereafter removing the application of vacuum and the film, and further heating said cylinder and said covered layer for 10 to 60 min. at a temperature of 100° to 150° C.
Claim 3
Dependent Claim 56 words
Method according to claim 1, wherein the vacuum is applied at a maximum absolute pressure of 50 mm of mercury in the space between said cylinder and said layer, the temperature during the heating step being maintained at 140° C. for a period of one hour and subsequently for a second period of half an hour.
Claim 4
Dependent Claim 40 words
Method according to claim 1, wherein the covering step includes joining free ends of the layer together, and the enveloping step includes overlapping free ends of the film and locating the overlapped ends a circumferential distance from the joined ends.

References Cited (Backward Citations)

US2343225A Cited
US2429121A Cited
US2762736A Cited
US3010194A Cited
US3405019A Cited
US3933562A Cited
US3962394A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-05-02 1986-11-01 1987-05-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-05-02 1990-11-01 1991-05-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-05-02 1994-11-01 1995-05-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag