← Back to Patent Explorer
US4381810A Expired / Lapsed US ⏱️ 0.0 years remaining

Tire with dual tread compound

Assignee: Goodyear Tire and Rubber Co
•
Filing: 1981-05-22
•
Granted: 1983-05-03
•
Expires: 2001-05-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A tire which has an outer and an inner layer of compound in the non-skid portion of the tread thereof. The outer layer is composed of a lower rolling resistance compound than the inner layer is composed. The inner layer is composed of a compound which provides better traction than the compound of the outer layer provides.

Inventors

  • 👤 John M. Cady
  • 👤 William E. Egan

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 14:50
CPC Classifications
B; B60; B60C; B60C1/00; B60C1/0016; B60C11/00; B60C11/0041; B60C11/005; B60C11/14; B60C11/18; B60C11/0008; B60C2011/0016; B60C2011/0033; Y; Y02; Y02T; Y02T10/00; Y02T10/80; Y02T10/86; Y10; Y10T; Y10T152/00; Y10T152/10; Y10T152/10495; Y10T152/10819; Y10T152/10846

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 300 words
A tire comprising a tread having a non-skid portion which includes a radially outer and a radially inner layer of elastomeric compound, said outer layer being composed of a lower rolling resistance compound than said inner layer, and said inner layer being composed of a compound which provides better traction than the compound of said outer layer, wherein A. the compound of said outer layer has a hot rebound of at least 75 and the compound of said inner layer has a hot rebound of less than 65 according to ASTMD1054-79, B. the kinetic coefficient of friction between the compound of said inner layer and a wet concrete surface is at least 5 percent greater than the kinetic coefficient of friction between the compound of said outer layer and the same wet concrete surface, C. the compound of said outer layer is composed of, based upon 100 parts by weight rubber, (1) about 50 to about 90 percent butadiene/styrene rubber, about 10 to about 50 percent polybutadiene, about 60 to about 80 phr carbon black, and about 25 to about 45 phr processing oil, (2) about 40 to about 60 percent natural rubber, about 40 to about 60 percent polybutadiene, about 40 to about 60 phr carbon black, and about 10 to about 30 phr processing oil, or (3) about 80 to 100 percent natural rubber, 0 to about 20 percent butadiene/styrene rubber, about 40 to about 60 phr carbon black, and about 2 to about 5 phr processing oil, and D. the compound of said inner layer is composed of, based upon 100 parts by weight rubber, about 60 to about 90 percent butadiene/styrene rubber, about 10 to about 40 percent polybutadiene, about 70 to about 100 phr carbon black, and about 30 to about 55 phr processing oil.
Claim 2
Dependent Claim 300 words
A tire comprising a tread having a non-skid portion which includes a radially outer and a radially inner layer of elastomeric compound, said outer layer being composed of a lower rolling resistance compound than said inner layer, and said inner layer being composed of a compound which provides better traction than the compound of said outer layer, wherein A. the compound of said outer layer has a hot rebound of at least 75 and the compound of said inner layer has a hot rebound of less than 65 according to ASTMD1054-79, B. the kinetic coefficient of friction between the compound of said inner layer and a wet concrete surface is at least 5 percent greater than the kinetic coefficient of friction between the compound of said outer layer and the same wet concrete surface, C. the compound of said outer layer is composed of, based upon 100 parts by weight rubber, (1) about 50 to about 90 percent butadiene/styrene rubber, about 10 to about 50 percent polybutadiene, about 60 to about 80 phr carbon black, and about 25 to about 45 phr processing oil, (2) about 40 to about 60 percent natural rubber, about 40 to about 60 percent polybutadiene, about 40 to about 60 phr carbon black, and about 10 to about 30 phr processing oil, or (3) about 80 to 100 percent natural rubber, 0 to about 20 percent butadiene/styrene rubber, about 40 to about 60 phr carbon black, and about 2 to about 5 phr processing oil, and D. the compound of said inner layer is composed of, based upon 100 parts by weight rubber, about 60 to about 90 percent butadiene/styrene rubber, about 10 to about 40 percent polybutadiene, about 70 to about 100 phr carbon black, and about 30 to about 55 phr processing oil.

References Cited (Backward Citations)

US2445725A Cited
GB1255952A Cited
US3830275A Cited
US4224197A Cited
GB2058687A Cited
US4281703A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-05-02 1986-11-01 1987-05-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-05-02 1990-11-01 1991-05-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-05-02 1994-11-01 1995-05-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag