Abstract

Abstract Improved conductor inks useful in constructing multilayer circuits, particularly on porcelain-coated metal substrates, are provided. The subject inks comprise: copper powder, a barium calcium borosilicate glass frit, a suitable organic vehicle and bismuth oxide, which is present either in admixture with the copper powder or as a component of the glass frit.

Inventors

  • 👤 Ashok N. Prabhu
  • 👤 Kenneth W. Hang

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 14:51
CPC Classifications
H; H05; H05K; H05K1/00; H05K1/02; H05K1/09; H05K1/092; C; C03; C03C; C03C8/00; C03C8/02; C03C8/14; C03C8/18; H01; H01B; H01B1/00; H01B1/14; H01B1/16

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 94 words
A copper conductor ink suitable for forming a conductor film on a circuit board consisting of: (a) from about 70 to about 90 percent by weight of copper powder; (b) from about 1 to about 15 percent by weight of a barium calcium borosilicate glass frit; (c) from about 0.5 to about 3 percent by weight of bismuth oxide, wherein bismuth oxide is present in admixture with the copper powder or as a component of the glass frit; and (d) from about 6 to about 25 percent by weight of a suitable organic vehicle.
Claim 2
Dependent Claim 94 words
A copper conductor ink suitable for forming a conductor film on a circuit board consisting of: (a) from about 70 to about 90 percent by weight of copper powder; (b) from about 1 to about 15 percent by weight of a barium calcium borosilicate glass frit; (c) from about 0.5 to about 3 percent by weight of bismuth oxide, wherein bismuth oxide is present in admixture with the copper powder or as a component of the glass frit; and (d) from about 6 to about 25 percent by weight of a suitable organic vehicle.
Claim 3
Dependent Claim 62 words
A conductor ink in accordance with claim 1, wherein said ink comprises: from about 78 to about 82 percent by weight of copper powder; from about 2 to about 6 percent by weight of said glass frit; from about 1 to about 2 percent by of weight bismuth oxide; and from about 12 to about 15 percent by weight of said vehicle.
Claim 4
Dependent Claim 68 words
A conductor ink in accordance with claim 1, wherein said glass frit has the composition: (a) from about 40 to about 55 percent by weight of barium oxide; (b) from about 10 to about 15 percent by weight of calcium oxide; (c) from about 14 to about 25 percent by weight of boron trioxide; and (d) from about 13 to about 23 percent by weight of silicon dioxide.
Claim 5
Dependent Claim 48 words
A conductor ink in accordance with claim 3, wherein said glass frit has the composition: about 52 percent by weight of barium oxide; about 12 percent by weight of calcium oxide; about 16 percent by weight of boron trioxide; and about 20 percent by weight of silicon dioxide.
Claim 6
Dependent Claim 29 words
A conductor ink in accordance with claim 1, wherein said organic vehicle contains up to about 25 percent by weight, based on the vehicle, of a suitable wetting agent.
Claim 7
Dependent Claim 25 words
A conductor ink in accordance with claim 5, wherein said wetting agent comprises from about 10 to about 20 percent by weight of said vehicle.
Claim 8
Dependent Claim 19 words
A conductor ink in accordance with claim 1, wherein bismuth oxide is present in admixture with the copper powder.
Claim 9
Dependent Claim 20 words
A conductor ink in accordance with claim 1, wherein bismuth oxide is present as a component of the glass frit.
Claim 10
Dependent Claim 26 words
A conductor ink in accordance with claim 1, wherein the weight ratio of bismuth oxide to said glass frit is from about 1:1 to about 1:3.

References Cited (Backward Citations)

US2993815A Cited
US3484284A Cited
US4039721A Cited
US4029605A Cited
US4256796A Cited
US4316942A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-03-14 1986-09-13 1987-03-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-03-14 1990-09-13 1991-03-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-03-14 1994-09-13 1995-03-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag