Abstract

Abstract An orientation layer for liquid crystal display devices is formed from an organic tin compound of the type: Rn SnX4-n wherein R is an organic radical; X is a reactive residual radical and n is an integer ranging from 1 to 3, by applying such organic tin compound onto a free surface of a carrier plate of a liquid crystal display device and generating the desired layer. In a preferred embodiment, the organic radical is an alkyl and the reactive residual radical is chlorine. In a preferred embodiment, the orientation layer is applied via an immersion technique wherein a select organic tin compound is dissolved in a suitable organic solvent, applied to a carrier plate surface and thereafter dried at somewhat elevated temperatures. The so-obtained orientation layer is stable, strongly adherent to its substrate and gives adjacent liquid crystal molecules a specific angle of incidence, whose size depends on the selected tin compound as well as on the liquid crystal material utilized and can range between about 20 DEG and 90 DEG . Smaller angles of incidence can be obtained by rubbing the orientation layer. These orientation layers can also be made electrically conductive by doping and subsequent pyrolysis. In this manner, transparent electrodes and orientation layers for liquid crystal display devices can be produced from substantially identical starting materials and with very similar production conditions.

Inventors

  • 👤 Joerg Bernhardt

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 18:46
CPC Classifications
G; G02; G02F; G02F1/00; G02F1/01; G02F1/13; G02F1/133; G02F1/1333; G02F1/1343; G02F1/13439; G02F1/1337; G02F1/133711; G02F1/133719; C; C09; C09K; C09K2323/00; C09K2323/02; Y; Y10; Y10S; Y10S359/00; Y10S359/90

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 89 words
In a method of producing a liquid crystal display device comprised of two carrier plates which enclose a liquid crystal layer therebetween and each plate is provided with an electrically conductive coating (electrode) on a respective surface thereof facing one another and provided with an orientation layer thereabove, the improvement comprising wherein: said orientation layer is generated from an organic tin compound of the type: R.sub.n SnX.sub.4-n wherein R is an organic radical, X is a reactive residual radical and n is an integer ranging from 1 to 3.
Claim 2
Dependent Claim 89 words
In a method of producing a liquid crystal display device comprised of two carrier plates which enclose a liquid crystal layer therebetween and each plate is provided with an electrically conductive coating (electrode) on a respective surface thereof facing one another and provided with an orientation layer thereabove, the improvement comprising wherein: said orientation layer is generated from an organic tin compound of the type: R.sub.n SnX.sub.4-n wherein R is an organic radical, X is a reactive residual radical and n is an integer ranging from 1 to 3.
Claim 3
Dependent Claim 53 words
In a method as defined in claim 1 wherein said orientation layer is generated by first dissolving said organic tin compound in an organic solvent to obtain a solution, then applying such solution to a select surface of a carrier plate and thereafter heating the resultant plate sufficiently to obtain the orientation layer.
Claim 4
Dependent Claim 43 words
In a method as defined in claim 2, wherein said solution is applied by immersion of the carrier plate into such solution and the resultant plate is heated for about 20 to 40 minutes at temperatures ranging between about 100° to 120° C.
Claim 5
Dependent Claim 47 words
In a method as defined in claim 1, wherein said organic radical of the tin compound is selected from the group consisting of alkyls, alkyl amides, phenols, biphenyls, triphenyls, cyanophenyls, cyanobiphenyls, cyanotriphenyls, cyclohexyls, bicyclohexyls, phenyl cyclohexyls, biphenyl cyclohexyls, cyano biphenyl cyclohexyls, pheny pyrimidenes and cyano phenyl pyrimidenes.
Claim 6
Dependent Claim 24 words
In a method as defined in claim 1 wherein said reactive residual radical is selected from the group consisting of chlorine, bromine and iodine.
Claim 7
Dependent Claim 28 words
In a method as defined in claim 1 wherein said reactive residual radical is an alcoholate of the type OR', wherein R' is an alkyl or an aryl.
Claim 8
Dependent Claim 25 words
In a method as defined in claim 1, wherein said organic tin compound is selected from the group consisting of a mono-n-alkyl-tin-trichloride and a di-n-alkyl-tin-dichloride.
Claim 9
Dependent Claim 25 words
In a method as defined in claim 1, wherein said organic tin compound is selected from the group consisting of a di-n-alkyl-tin-diethoxide and a mono-n-alkyl-tin-triethoxide.
Claim 10
Dependent Claim 88 words
In a method as defined in claim 1, wherein prior to generation of said orientation layer, said electrically conductive coating is formed by first adding an oxidizable additive whose oxide increases the electrical conductivity of tin oxide to said organic tin compound to attain an admixture thereof; then generating a layer of such admixture onto a select surface of a carrier plate and thereafter heating the resultant layer in such a manner that said organic tin compound and said oxidizable additive are both converted into their respective oxides.
Claim 11
Dependent Claim 34 words
In a method as defined in claim 9, wherein said oxidizable additive has cations selected from the group consisting of indium, antimony, cadmium and rare earth metals having a valence of +3 or +5.
Claim 12
Dependent Claim 28 words
In a method as defined in claim 9, wherein an identical organic tin compound is utilized for forming the electrically conductive layer and for generating the orientation layer.
Claim 13
Dependent Claim 105 words
In an operative liquid crystal display device comprised of a pair of opposing carrier plates spaced from one another via a frame means so as to define a liquid crystal chamber therebetween, with the respective surfaces of each plate facing one another being provided with an electrically conductive coating and an orientation layer thereabove, and said chamber being filled with a liquid crystal layer, the improvement comprising wherein said orientation layer is generated from an organic tin compound of the type: R.sub.n SnX.sub.4-n wherein R is an organic radical, X is a reactive residual radical and n is an integer ranging from 1 to 3.
Claim 14
Dependent Claim 105 words
In an operative liquid crystal display device comprised of a pair of opposing carrier plates spaced from one another via a frame means so as to define a liquid crystal chamber therebetween, with the respective surfaces of each plate facing one another being provided with an electrically conductive coating and an orientation layer thereabove, and said chamber being filled with a liquid crystal layer, the improvement comprising wherein said orientation layer is generated from an organic tin compound of the type: R.sub.n SnX.sub.4-n wherein R is an organic radical, X is a reactive residual radical and n is an integer ranging from 1 to 3.
Claim 15
Dependent Claim 71 words
In an operative liquid crystal display device as defined in claim 12 wherein said electrically conductive coating is composed of an admixture of oxides obtained by heating an organic tin compound of the type: R.sub.n SnX.sub.4-n wherein R is an organic radical, X is a reactive residual radical and n is an integer ranging from 1 to 3, and an oxidizable additive whose oxide increases the electrical conductivity of tin oxide.

References Cited (Backward Citations)

DE2238429A1 Cited
US3786486A Cited
US3728008A Cited
US3854793A Cited
US3973057A Cited
JPS54112658A Cited
US4273420A Cited
US4261650A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-01-24 1986-07-26 1987-01-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-01-24 1990-07-26 1991-01-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-01-24 1994-07-26 1995-01-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag