Abstract

Abstract In forming a fluorescent screen of a black matrix type color picture tube, a light absorptive film is first formed on the inner surface of a face plate of the color picture tube. Formed on the light absorptive film is a light-hardenable photosensitive resin film which in turn is exposed to light through a shadow mask at portions corresponding to phosphor applying portions. The unexposed portion of the light-hardenable photosensitive film is then developed. Finally, the exposed portion of the light-hardenable photosensitive film and portion of the light absorptive film therebeneath are removed to partly perforate the light absorptive film so that in the light absorptive film, openings are formed into which the phosphor is applied.

Inventors

  • 👤 Yoshiyuki Odaka
  • 👤 Kiyoshi Miura

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 06:35
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/0005; G03F7/0007; H; H01; H01J; H01J9/00; H01J9/20; H01J9/22; H01J9/227; H01J9/2278

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 200 words
In a method of forming a fluorescent screen of a black matrix type color picture tube wherein a plurality of trios of phosphor are arranged, in a predetermined pattern, on the inner surface of a face plate of the color picture tube with a film of a light absorptive material applied on gaps between the patterned trios, said method comprising the steps of: forming a porous light absorptive film on the inner surface of the face plate; forming a light-hardenable photosensitive resin film on the light absorptive film with some absorption of the resin material into the underlying upper region of the light absorptive film; exposing to light the portion of the light-hardenable resin film corresponding to a phosphor applying portion through a shadow mask sufficient to harden the exposed portion and said underlying upper region to firmly couple said films at their interface; removing the unexposed portion of the light-hardenable photosensitive film by developing; and continuing the development to remove the exposed portion of the light-hardenable photosensitive film and portion of the light absorptive film therebeneath to partly perforate the light absorptive film so that in the light absorptive film, openings are formed into which the phosphor is applied.
Claim 2
Dependent Claim 200 words
In a method of forming a fluorescent screen of a black matrix type color picture tube wherein a plurality of trios of phosphor are arranged, in a predetermined pattern, on the inner surface of a face plate of the color picture tube with a film of a light absorptive material applied on gaps between the patterned trios, said method comprising the steps of: forming a porous light absorptive film on the inner surface of the face plate; forming a light-hardenable photosensitive resin film on the light absorptive film with some absorption of the resin material into the underlying upper region of the light absorptive film; exposing to light the portion of the light-hardenable resin film corresponding to a phosphor applying portion through a shadow mask sufficient to harden the exposed portion and said underlying upper region to firmly couple said films at their interface; removing the unexposed portion of the light-hardenable photosensitive film by developing; and continuing the development to remove the exposed portion of the light-hardenable photosensitive film and portion of the light absorptive film therebeneath to partly perforate the light absorptive film so that in the light absorptive film, openings are formed into which the phosphor is applied.

References Cited (Backward Citations)

US2533530A Cited
US2564414A Cited
US3146368A Cited
US3317319A Cited
US3615460A Cited
US3661580A Cited
US4234669A Cited
US4292393A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-01-17 1986-07-19 1987-01-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-01-17 1990-07-19 1991-01-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-01-17 1994-07-19 1995-01-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag