Preparation of amphoteric water-in-oil self-inverting polymer emulsion

Assignee: Diamond Shamrock Chemicals Co
•
Filing: 1981-09-04
•
Granted: 1982-12-14
•
Expires: 2001-09-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An amphoteric water-in-oil self-inverting polymer emulsion is prepared which contains a copolymer of (1) a nonionic vinyl monomer and (2) an amphoteric vinyl monomer or a terpolymer of (1) a nonionic vinyl monomer, (2) an anionic vinyl monomer and (3) a cationic vinyl monomer in the aqueous phase, a hydrocarbon oil for the oil phase, a water-in-oil emulsifying agent and an inverting surfactant. An example of a copolymer is a copolymer of (1) a nonionic vinyl monomer such as acrylamide or methacrylamide and (2) an amphoteric vinyl monomer such as a reaction product of dimethylaminoethyl methacrylate and monochloroacetic acid. An example of a terpolymer is a terpolymer of (1) a nonionic vinyl monomer such as acrylamide or methacrylamide, (2) an anionic vinyl monomer such as sodium acrylate and (3) a cationic vinyl monomer such as a triethyl ammonium ethyl methacrylate methosulfate salt. The emulsion is useful in papermaking, treatment of sewage and industrial wastes, drilling muds and secondary and tertiary recovery of petroleum by water flooding.

Inventors

  • 👤 Stanley A. Lipowski
  • 👤 John J. Miskel, Jr.

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 22:14
CPC Classifications
C; C08; C08J; C08J3/00; C08J3/02; C08J3/09; C02; C02F; C02F1/00; C02F1/52; C02F1/54; C08K; C08K5/00; C08K5/0008; C08K5/0075; C09; C09K; C09K8/00; C09K8/02; C09K8/03; C09K8/035; C09K8/58; C09K8/588; D; D21; D21H; D21H17/00; D21H17/20; D21H17/33; D21H17/34; D21H17/41; D21H17/42; D21H17/44; C08J2300/00; C08J2300/14

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 234 words
A method of preparing an amphoteric water-in-oil self-inverting polymer emulsion comprising (A) forming a water-in-oil emulsion of (1) from about 10 to about 50 parts by weight of a monomer mixture selected from the group consisting of (a) from about 30 to about 99 parts by weight of a water soluble nonionic vinyl monomer and from about 1 to about 70 parts by weight of a water soluble amphoteric vinyl monomer to form an amphoteric copolymer, and (b) from about 30 to 98 parts by weight of a water soluble nonionic vinyl monomer, from about 1 to about 35 parts by weight of a water soluble anionic vinyl monomer and from about 1 to about 35 parts by weight of a water soluble cationic vinyl monomer to form an amphoteric terpolymer, (2) from about 10 to about 50 parts by weight of water, (3) from about 5 to about 50 parts by weight of a hydrophobic liquid, (4) from about 2 to about 25 parts by weight of a water-in-oil emulsifying agent, and (5) an effective amount of a free radical yielding initiator to polymerize the monomer mixture, (B) polymerizing the monomer mixture under free radical polymerizing conditions to form a water-in-oil emulsion which contains finely dispersed particles of the amphoteric polymer, and (C) adding to the water in oil emulsion from about 1 to about 15 parts by weight of an inverting surfactant.
Claim 2
Independent Claim 234 words
A method of preparing an amphoteric water-in-oil self-inverting polymer emulsion comprising (A) forming a water-in-oil emulsion of (1) from about 10 to about 50 parts by weight of a monomer mixture selected from the group consisting of (a) from about 30 to about 99 parts by weight of a water soluble nonionic vinyl monomer and from about 1 to about 70 parts by weight of a water soluble amphoteric vinyl monomer to form an amphoteric copolymer, and (b) from about 30 to 98 parts by weight of a water soluble nonionic vinyl monomer, from about 1 to about 35 parts by weight of a water soluble anionic vinyl monomer and from about 1 to about 35 parts by weight of a water soluble cationic vinyl monomer to form an amphoteric terpolymer, (2) from about 10 to about 50 parts by weight of water, (3) from about 5 to about 50 parts by weight of a hydrophobic liquid, (4) from about 2 to about 25 parts by weight of a water-in-oil emulsifying agent, and (5) an effective amount of a free radical yielding initiator to polymerize the monomer mixture, (B) polymerizing the monomer mixture under free radical polymerizing conditions to form a water-in-oil emulsion which contains finely dispersed particles of the amphoteric polymer, and (C) adding to the water in oil emulsion from about 1 to about 15 parts by weight of an inverting surfactant.
Claim 3
Dependent Claim 34 words
The method of claim 1 wherein the water soluble nonionic vinyl monomer is selected from the group consisting of acrylamide, methacrylamide, allyl alcohol, 3-methylallyl alcohol, vinyl chloride, vinyl methyl ether and vinyl ethyl ether.
Claim 4
Dependent Claim 22 words
The method of claim 1 wherein the water soluble nonionic vinyl monomer is selected from the group consisting of acrylamide and methacrylamide.
Claim 5
Dependent Claim 33 words
The method of claim 1 wherein the water soluble cationic vinyl monomer is selected from the group consisting of N-substituted-(N'-dialkylaminoalkyl)acrylamide, aminoalkylacrylate, dialkylaminoalkylacrylate, vinylpyridine, diallylalkylamine and quaternary having at least one ethylenically unsaturated substituent.
Claim 6
Dependent Claim 22 words
The method of claim 1 wherein the water soluble cationic vinyl monomer is selected from the group consisting of N-substituted-(N'-dialkylaminoalkyl)acrylamide and aminoalkylacrylate.
Claim 7
Dependent Claim 52 words
The method of claim 1 wherein the water soluble anionic vinyl monomer is selected from the group consisting of acrylic acid, 1,2-dichloroacrylic acid, 2-methylacrylic acid, ethylene sulfonic acid, fumaric acid, chlorofumaric acid, methylfumaric acid, itaconic acid, maleic acid, dichloromaleic acid, methylmaleic acid, methacrylic acid, styrene sulfonic acid, crotonic acid and salt thereof.
Claim 8
Dependent Claim 62 words
The method of claim 1 wherein the amphoteric water soluble vinyl monomer is a reaction product of a cationic water soluble vinyl monomer slected from the group consisting of N-substituted-(N'-dialkylaminoalkyl)acrylamide, aminoalkylacrylate, dialkylaminoalkylacrylate, vinylpyridine, diallylalkylamine and a quaternary having at least one ethylenically unsaturated substituent with an anionic reactant selected from the group consisting of chloroacetic acid, chlorosulfonic acid and bromoethanol sulfonic acid.
Claim 9
Dependent Claim 24 words
The method of claim 1 wherein the monomer mixture is acrylamide and an amphoteric vinyl monomer reaction product of dimethylaminoethyl methacrylate and monochloroacetic acid.
Claim 10
Dependent Claim 26 words
The method of claim 1 wherein the monomer mixture is acrylamide, acrylic acid and a quaternization vinyl monomeric reaction product of dimethylaminoethyl methacrylate and dimethyl sulfate.

References Cited (Backward Citations)

US3284393A Cited
US4077930A Cited
US4022736A Cited
US4022731A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-12-13 1986-06-14 1986-12-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-12-13 1990-06-14 1990-12-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-12-13 1994-06-14 1994-12-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag