Abstract PCT No. PCT/JP80/00242 Sec. 371 Date Jun. 9, 1981 Sec. 102(e) Date May 20, 1981 PCT Filed Oct. 8, 1980 PCT Pub. No. WO81/00981 PCT Pub. Date Apr. 16, 1981.This invention provides a metal bonded diamond abrasive article of nickel-copper basis. The sintered metal bond, which consists essentially of 2 to 30% by weight of copper, 1 to 40% by weight of tin, 0.2 to 3% by weight of phosphorous, and at least 50% by weight of the remainder nickel, well disperses and retains diamond grits and minimizes the clogging and the variation in rate of stock removal.

Inventors

  • 👤 Eiji Isobe
  • 👤 Izumi Hayakawa
  • 👤 Akira Emura

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 08:50
CPC Classifications
C; C22; C22C; C22C26/00; B; B24; B24D; B24D3/00; B24D3/02; B24D3/04; B24D3/06; B24D3/08

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 75 words
A metal bonded diamond abrasive article composed of a diamond powder and of a sintered nickel base metal bond retaining the diamond powder, which is characterized in that the sintered metal bond consists essentially of 2 to 30% by weight of copper, 1 to 40% by weight of tin, 0.2 to 3% by weight of phosphorous, and the balance of nickel, the total amount of copper, tin, and phosphorous being less than 50% by weight.
Claim 2
Dependent Claim 75 words
A metal bonded diamond abrasive article composed of a diamond powder and of a sintered nickel base metal bond retaining the diamond powder, which is characterized in that the sintered metal bond consists essentially of 2 to 30% by weight of copper, 1 to 40% by weight of tin, 0.2 to 3% by weight of phosphorous, and the balance of nickel, the total amount of copper, tin, and phosphorous being less than 50% by weight.
Claim 3
Dependent Claim 49 words
A metal bonded diamond abrasive article of claim 1, wherein the sintered metal bond consists essentially of 3 to 20% by weight of copper, 2 to 30% by weight of tin, 0.3 to 2% by weight of phosphorous, and the balance of 70% by weight or more of nickel.

References Cited (Backward Citations)

US3036907A Cited
US3293012A Cited
US3389981A Cited
US3372010A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-12-06 1986-06-07 1986-12-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-12-06 1990-06-07 1990-12-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-12-06 1994-06-07 1994-12-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag