← Back to Patent Explorer
US4361679A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for producing heat-resistant and moisture-resistant polyborometallosiloxanes

Assignee: YAJIMA SEISHI TOHOKU DAIGAKUSHUKUSHA
•
Filing: 1981-06-30
•
Granted: 1982-11-30
•
Expires: 2001-06-30
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for producing a heat-resistant and moisture-resistant polyborometallosiloxane, which comprises adding a metal compound and a compound capable of easily forming a complex with the metal compound to an organoborosiloxane, the metal in said metal compound being at least one member of the group consisting of Ti, Zr, V, P, Al, Fe, Cr, Co, Ni, Ge, Sn, As, Mg, Pb and Sb; and heating the resulting mixture to a temperature of 550° C. or lower to bond the metal atom to the silicon atom and/or the boron atom through an oxygen atom.

Inventors

  • 👤 Seishi Yajima
  • 👤 Kiyohito Okamura
  • 👤 Toetsu Shishido

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 07:17
CPC Classifications
C; C08; C08G; C08G77/00; C08G77/60; C08G77/48; C08G77/56; C08G77/58

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 198 words
A process for producing a heat-resistant and moisture-resistant polyborometallosiloxane, which comprises adding (1) a phosphorus or metal compound which compound is selected from the group consisting of salts which are halides, oxyhalides, sulfates, oxysulfates, oxalates and oxyoxalates; alkali metal and ammonium salts of said salts; and acetylacetone complexes; and (2) a compound capable of easily forming a complex with the phosphorus or metal compound, said compound capable of easily forming a complex being selected from the group consisting of ethers, monohydric and polyhydric alcohols, ketones, phenols, heterocyclic compounds containing oxygen as a hetero atom, and chain and cyclic compounds having quinonic oxygen, an aldehyde group, or a carboxyl group in the side chain; to (3) an organoborosiloxane, being a monomer, oligomer or polymer whose main chain consists mainly of B, Si and O elements; the metal in said metal compound being at least one member selected from the group consisting of Ti, Zr, V, Al, Fe, Cr, Co, Ni, Ge, Sn, As, Mg, Pb and Sb; and heating the resulting mixture to a temperature of 550° C. or lower to bond the phosphorus or metal atom to the silicon atom and/or the boron atom through an oxygen atom.
Claim 2
Dependent Claim 198 words
A process for producing a heat-resistant and moisture-resistant polyborometallosiloxane, which comprises adding (1) a phosphorus or metal compound which compound is selected from the group consisting of salts which are halides, oxyhalides, sulfates, oxysulfates, oxalates and oxyoxalates; alkali metal and ammonium salts of said salts; and acetylacetone complexes; and (2) a compound capable of easily forming a complex with the phosphorus or metal compound, said compound capable of easily forming a complex being selected from the group consisting of ethers, monohydric and polyhydric alcohols, ketones, phenols, heterocyclic compounds containing oxygen as a hetero atom, and chain and cyclic compounds having quinonic oxygen, an aldehyde group, or a carboxyl group in the side chain; to (3) an organoborosiloxane, being a monomer, oligomer or polymer whose main chain consists mainly of B, Si and O elements; the metal in said metal compound being at least one member selected from the group consisting of Ti, Zr, V, Al, Fe, Cr, Co, Ni, Ge, Sn, As, Mg, Pb and Sb; and heating the resulting mixture to a temperature of 550° C. or lower to bond the phosphorus or metal atom to the silicon atom and/or the boron atom through an oxygen atom.
Claim 3
Dependent Claim 56 words
The process of claim 1 wherein the ratio of the amount of the organoborosiloxane to that of the phosphorus or metal compound is from 2:1 to 200:1 in terms of the atomic ratio of the Si atoms and B atoms combined of the organoborosiloxane to the phosphorous or metal atoms of the phosphorus or metal compound.
Claim 4
Dependent Claim 32 words
The process of claim 1 wherein the amount of the compound capable of forming a complex is the one at least required to form a complex with the phosphorus or metal compound.
Claim 5
Dependent Claim 16 words
The process of claim 1 wherein the heating temperature is from 200° C. to 500° C.

References Cited (Backward Citations)

US2463974A Cited
US2994711A Cited
US3086983A Cited
US3377312A Cited
US4070343A Cited
US4152509A Cited
US4242487A Cited
US4334051A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-11-29 1986-05-31 1986-11-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-11-29 1990-05-31 1990-11-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-11-29 1994-05-31 1994-11-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag