Abstract

Abstract A cable filler composition comprises a mixture of mineral oil, a styrene-ethylene butylene-stryene block copolymer, and about 2-6 percent by weight of a thermoplastic polymer comprising an isotactic, crystalline polypropylene copolymer containing 0.1-4% by weight of an olefinic comonomer, the copolymer having a molecular weight of between 20,000 and 40,000.

Inventors

  • 👤 Larry G. Bourland

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 12:31
CPC Classifications
H; H01; H01B; H01B7/00; H01B7/17; H01B7/28; H01B7/282; H01B7/285; C; C08; C08L; C08L53/00; C08L53/02; C08L53/025; Y; Y02; Y02A; Y02A30/00; Y02A30/14

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 69 words
In a cable filling composition for use in waterproofing electrical cables wherein a thermoplastic polymer is admixed with a styrene-ethylene butylene-styrene block copolymer and mineral oil in an amount of 87-91 percent by weight of said composition, the improvement wherein said thermoplastic polymer comprises an isotactic, crystalline polypropylene copolymer containing 0.1-4% by weight of an olefinic comonomer, said copolymer having an average molecular weight of between 20,000 and 40,000.
Claim 2
Dependent Claim 69 words
In a cable filling composition for use in waterproofing electrical cables wherein a thermoplastic polymer is admixed with a styrene-ethylene butylene-styrene block copolymer and mineral oil in an amount of 87-91 percent by weight of said composition, the improvement wherein said thermoplastic polymer comprises an isotactic, crystalline polypropylene copolymer containing 0.1-4% by weight of an olefinic comonomer, said copolymer having an average molecular weight of between 20,000 and 40,000.
Claim 3
Dependent Claim 37 words
In a cable filling composition for use in waterproofing electrical cables as defined in claim 1, the improvement wherein said styrene-ethylene butylene-styrene block copolymer is present in an amount of 5-7 percent by weight of said compositions.
Claim 4
Dependent Claim 37 words
In a cable filling composition for use in waterproofing electrical cables as defined in claim 1, the improvement wherein said isotactic, crystalline polypropylene copolymer is present in an amount of 2-6 percent by weight of said compositions.
Claim 5
Dependent Claim 64 words
In a cable filling composition for use in waterproofing electrical cables as defined in claim 1, the improvement wherein said comonomer is of the general formula: CH.sub.2 ═CRR' wherein R is a member selected from the group consisting of hydrogen and aromatic and aliphatic hydrogen groups containing 2-20 carbon atoms, and R' is a member selected from the group consisting of hydrogen and methyl.
Claim 6
Dependent Claim 24 words
In a cable filling composition for use in waterproofing electrical cables as defined in claim 1, the improvement wherein said olefinic comonomer is ethylene.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-11-29 1986-05-31 1986-11-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-11-29 1990-05-31 1990-11-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-11-29 1994-05-31 1994-11-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag