← Back to Patent Explorer
US4359526A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for forming a photosensitive silver halide element

Assignee: Polaroid Corp
•
Filing: 1981-09-02
•
Granted: 1982-11-16
•
Expires: 2001-09-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for forming a photosensitive element comprising a plurality of single effective silver halide grains in a predetermined spaced array which comprises coalescing a fine-grain silver halide emulsion in a plurality of predetermined spaced depressions in a surface, wherein said coalescence is carried out by contacting said fine-grain emulsion with a silver halide solvent in the vapor phase.

Inventors

  • 👤 Vivian K. Walworth

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 17:12
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/76; G03C1/765; G03C1/005; G03C1/74; Y; Y10; Y10S; Y10S430/00; Y10S430/136; Y10S430/149; Y10S430/162

Claims Analysis

Total Claims: 21
Claim 1
Independent Claim 53 words
A method for forming a photosensitive element comprising a plurality of single effective silver halide grains in a predetermined spaced array which comprises coalescing a fine-grain silver halide emulsion in a plurality of predetermined spaced depressions in a surface by contacting said fine-grain emulsion with a silver halide solvent in the vapor phase.
Claim 2
Independent Claim 53 words
A method for forming a photosensitive element comprising a plurality of single effective silver halide grains in a predetermined spaced array which comprises coalescing a fine-grain silver halide emulsion in a plurality of predetermined spaced depressions in a surface by contacting said fine-grain emulsion with a silver halide solvent in the vapor phase.
Claim 3
Dependent Claim 15 words
The method of claim 1 wherein said spaced depressions are in a substantially planar surface.
Claim 4
Dependent Claim 18 words
The method of claim 1 which includes the step of depositing said fine-grain emulsion in said spaced depressions.
Claim 5
Dependent Claim 21 words
The method of claim 3 wherein said fine-grain emulsion comprises silver halide grains about 0.01 to 0.50 μm in average diameter.
Claim 6
Dependent Claim 18 words
The method of claim 4 wherein said fine-grain emulsion comprises grains about 0.1 μm or less in diameter.
Claim 7
Dependent Claim 20 words
The method of claim 1 wherein said fine-grain emulsion has a binder to silver ratio of about 0.1 or less.
Claim 8
Dependent Claim 14 words
The method of claim 6 wherein said binder to silver ratio is about 0.075.
Claim 9
Dependent Claim 12 words
The method of claim 1 wherein said silver halide solvent is ammonia.
Claim 10
Independent Claim 87 words
A method for forming a photosensitive element comprising a plurality of single effective silver halide grains in a predetermined spaced array which comprises the following steps in sequence: (a) depositing a fine-grain silver halide emulsion in a plurality of predetermined spaced depressions in a surface; (b) contacting said fine-grain emulsion with a silver halide solvent in the vapor phase for a time sufficient to partially dissolve said grains in each depression; and (c) coalescing said grains to a single effective silver halide grain in substantially each depression.
Claim 11
Independent Claim 87 words
A method for forming a photosensitive element comprising a plurality of single effective silver halide grains in a predetermined spaced array which comprises the following steps in sequence: (a) depositing a fine-grain silver halide emulsion in a plurality of predetermined spaced depressions in a surface; (b) contacting said fine-grain emulsion with a silver halide solvent in the vapor phase for a time sufficient to partially dissolve said grains in each depression; and (c) coalescing said grains to a single effective silver halide grain in substantially each depression.
Claim 12
Dependent Claim 21 words
The method of claim 9 wherein said fine-grain emulsion comprises silver halide grains about 0.01 to 0.50 μm in average diameter.
Claim 13
Dependent Claim 18 words
The method of claim 10 wherein said fine-grain emulsion comprises grains about 0.1 μm or less in diameter.
Claim 14
Dependent Claim 20 words
The method of claim 9 wherein said fine-grain emulsion has a binder to silver ratio of about 0.1 or less.
Claim 15
Dependent Claim 14 words
The method of claim 12 wherein said binder to silver ratio is about 0.075.
Claim 16
Dependent Claim 11 words
The method of claim 9 wherein said silver solvent is ammonia.
Claim 17
Dependent Claim 15 words
The method of claim 9 which includes the step of washing said single effective grains.
Claim 18
Dependent Claim 16 words
The method of claim 9 which includes the step of chemically sensitizing said single effective grains.
Claim 19
Dependent Claim 18 words
The method of claim 9 which includes the step of spectrally sensitizing said single effective silver halide grains.
Claim 20
Dependent Claim 23 words
The method of claim 9 which includes applying a polymeric material over said fine-grain emulsion prior to contact with said silver halide solvent.
Claim 21
Dependent Claim 11 words
The method of claim 18 wherein said polymeric material is gelatin.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-11-15 1986-05-17 1986-11-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-11-15 1990-05-17 1990-11-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-11-15 1994-05-17 1994-11-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag