Abstract

Abstract Hydrocarbon resins having an increased softening point are obtained by a process featuring the sequential steps of: isomerizing the 2-methylbutene-1 component of a branched olefin modifier stream whereby its 2-methylbutene-2 content is enriched; polymerizing a feedstock consisting of the mixture of said enriched modifier stream and a piperylene rich feed stream; and, recovering said hydrocarbon resin with properties enhancing its utility for adhesive applications.

Inventors

  • 👤 Vincent L. Hughes

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 18:20
CPC Classifications
C; C08; C08F; C08F240/00; C08F236/00; C08F236/02; C08F236/04

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 77 words
A hydrocarbon resin comprising from 40 to 50 weight percent units derived from piperylene, 15 to 20 weight percent units derived from 2-methylbutenes and the balance derived from other olefinic compounds having from 5 to 6 carbons, said 2-methylbutenes consisting essentially as the 2-methylbutene-2 isomer and the 2-methylbutene-1 isomer in a weight ratio of the former isomer to the latter isomer being greater than 10 whereby said resin has a softening point of at least 90° C.
Claim 2
Dependent Claim 77 words
A hydrocarbon resin comprising from 40 to 50 weight percent units derived from piperylene, 15 to 20 weight percent units derived from 2-methylbutenes and the balance derived from other olefinic compounds having from 5 to 6 carbons, said 2-methylbutenes consisting essentially as the 2-methylbutene-2 isomer and the 2-methylbutene-1 isomer in a weight ratio of the former isomer to the latter isomer being greater than 10 whereby said resin has a softening point of at least 90° C.
Claim 3
Dependent Claim 35 words
The hydrocarbon resin according to claim 1 wherein said isomer weight ratio of 2-methylbutene-2 to 2-methylbutene-1 ranges from 15 to 100 whereby said resin has a softening point of from 90° C. to 100° C.
Claim 4
Dependent Claim 35 words
The hydrocarbon resin according to claim 1 wherein said isomer weight ratio of 2-methylbutene-2 to 2-methylbutene-1 ranges from 18 to 30 whereby said resin has a softening point of from 90° C. to 100° C.

References Cited (Backward Citations)

US2753382A Cited
US2753325A Cited
US3104269A Cited
US3151179A Cited
US3290404A Cited
US3268617A Cited
US3577398A Cited
US3920765A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-11-08 1986-05-10 1986-11-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-11-08 1990-05-10 1990-11-09 $3760.00 Window Closed / Lapsed