← Back to Patent Explorer
US4358554A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for repairing asphalt pavement

Assignee: Mobil Oil AS
•
Filing: 1981-02-10
•
Granted: 1982-11-09
•
Expires: 2001-02-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract This invention provides a process for repairing and surfacing broken asphalt pavements which involves applying to the distressed pavement a binder composition which has exceptional solvating power for asphaltic material, and which functions to solubilize and incorporate aged pavement asphalt into the binder composition as it penetrates and fills void spaces. Illustrative of a preferred binder composition which is applied to the distressed pavement is a homogeneous blend of (1) a FCC main column bottoms residuum boiling above about 650 DEG F., and (2) an asphalt-soluble elastomer which improves the elasticity and wear resistance of the binder composition.

Inventors

  • 👤 Tsoung Y. Yan
  • 👤 Costandi A. Audeh

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 17:09
CPC Classifications
E; E01; E01C; E01C7/00; E01C7/08; E01C7/35; E01C7/358; C; C08; C08L; C08L95/00; E01C7/18; E01C7/187; C08L2207/00; C08L2207/20; C08L2207/24; Y; Y10; Y10S; Y10S106/00; Y10S106/07

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 189 words
In a process for repairing and surfacing broken asphalt pavement which comprises heating and applying a fluid ductile asphaltic composition to a distressed pavement surface in a sufficient quantity to penetrate and fill void spaces, the improvement being said ductile asphaltic composition comprising a homogeneous blend of (1) between about 30-80 weight percent of an asphalt component selected from marginal asphalt materials having a viscosity penetration index lower than about 2.5×10 5 ; (2) between about 10-60 weight percent of a highly aromatic petroleum refinery residuum solvent component having a boiling range above about 650° F. and having a hydrogen content distribution in which the H Ar proton content is between about 30 and 50 percent, the H.sub.α proton content is at least 30 percent and the H.sub.α /H.sub.β proton ratio is above about 1.4; and (3) between about 1-20 weight percent of a polymeric component which is substantially asphalt-soluble; wherein the said asphaltic composition has a ring and ball softening point in the range between about 110°-185° F., a ductility of more than 100 centimeters at 77° F., and a penetration value in the range between about 70-300.
Claim 2
Dependent Claim 189 words
In a process for repairing and surfacing broken asphalt pavement which comprises heating and applying a fluid ductile asphaltic composition to a distressed pavement surface in a sufficient quantity to penetrate and fill void spaces, the improvement being said ductile asphaltic composition comprising a homogeneous blend of (1) between about 30-80 weight percent of an asphalt component selected from marginal asphalt materials having a viscosity penetration index lower than about 2.5×10 5 ; (2) between about 10-60 weight percent of a highly aromatic petroleum refinery residuum solvent component having a boiling range above about 650° F. and having a hydrogen content distribution in which the H Ar proton content is between about 30 and 50 percent, the H.sub.α proton content is at least 30 percent and the H.sub.α /H.sub.β proton ratio is above about 1.4; and (3) between about 1-20 weight percent of a polymeric component which is substantially asphalt-soluble; wherein the said asphaltic composition has a ring and ball softening point in the range between about 110°-185° F., a ductility of more than 100 centimeters at 77° F., and a penetration value in the range between about 70-300.
Claim 3
Dependent Claim 28 words
A process in accordance with claim 1 wherein the highly aromatic solvent component of the binder composition is selected from FCC main column bottoms and TCC syntower bottoms.
Claim 4
Dependent Claim 19 words
A process in accordance with claim 1 wherein the polymeric component of the binder composition is comminuted scrap rubber.
Claim 5
Dependent Claim 30 words
A process in accordance with claim 1 wherein the polymeric component of the binder composition is a copolymer of ethylene and vinyl acetate having a melt index between about 20-50.

References Cited (Backward Citations)

US3919148A Cited
US4105612A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-11-08 1986-05-10 1986-11-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-11-08 1990-05-10 1990-11-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-11-08 1994-05-10 1994-11-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag