Abstract
Abstract A method for manufacturing commutator for use in rotary electric machines, in which a shaping material prepared from electrically conductive metal powder material or a mixture of the metal powder material and additive powder material such as carbon, molybdenum disulfide, etc. is placed in a shaping mold and subjected to compression-molding into annular or cylindrical shaped electrically conductive body, then an electrically insulative synthetic resin material is coated around, or filled in, the hollow cavity of the annular or hollow cylindrical body, and thereafter this annular or cylindrical body is machined to be divided into a plurality of segments for constituting the commutator.
Inventors
- 👤 Makoto Yoshida
- 👤 Satoru Baba
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-31 11:57
CPC Classifications
H; H01; H01R; H01R43/00; H01R43/06; H01R43/08; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49009; Y10T29/49011
Claims Analysis
Total Claims: 11
Claim 1
Independent Claim
161 words
In a method for manufacturing a commutator, wherein a shaping material comprising an electrically conductive metal powder is placed in a shaping mold, compression-molded into an annular body, and sintered, re-compression being done on the sintered body, depending on necessity, to increase its mechanical strength and material hardness, the improvement comprising forming said annular body to have oppositely disposed spaced, generally radially extending, side surfaces with radially extending grooves in one of said side surfaces, and a peripheral surface; covering said grooved radial side, at least a portion of the peripheral surface and the center hollow portion and filling said grooves with an electrically insulative synthetic resin bearing material, the other side being exposed to a substantial degree; and cutting off the exposed surface side of said insulative material-coated annular body in parallel with the plane of said surface to a depth reaching said filled grooves in the opposite surface of said body thereby to define a plurality of commutator segments.
Claim 2
Dependent Claim
161 words
In a method for manufacturing a commutator, wherein a shaping material comprising an electrically conductive metal powder is placed in a shaping mold, compression-molded into an annular body, and sintered, re-compression being done on the sintered body, depending on necessity, to increase its mechanical strength and material hardness, the improvement comprising forming said annular body to have oppositely disposed spaced, generally radially extending, side surfaces with radially extending grooves in one of said side surfaces, and a peripheral surface; covering said grooved radial side, at least a portion of the peripheral surface and the center hollow portion and filling said grooves with an electrically insulative synthetic resin bearing material, the other side being exposed to a substantial degree; and cutting off the exposed surface side of said insulative material-coated annular body in parallel with the plane of said surface to a depth reaching said filled grooves in the opposite surface of said body thereby to define a plurality of commutator segments.
Claim 3
Dependent Claim
41 words
The method for manufacturing commutator as set forth in claim 1, in which said compression-molded electrically conductive annular body has an inclined outer peripheral surface toward one side surface where it is covered with said electrically insulative synthetic resin bearing material.
Claim 4
Dependent Claim
30 words
The method for manufacturing commutator as set forth in claim 1, in which said shaping material consists of from 85% to 95% of copper and 15% to 5% of carbon.
Claim 5
Dependent Claim
47 words
The method as set forth in claim 1, wherein said shaping material is a mixture of the electrically conductive metal powder and an additive material powder selected from the group consisting of carbon and molybdenum disulfide, which serve for enhancing electrical and mechanical characteristics of the commutator.
Claim 6
Dependent Claim
114 words
In a method for manufacturing commutator, wherein a shaping material comprising an electrically conductive metal powder is placed in a shaping mold, compression-molded into a hollow cylindrical body, and sintered, re-compression being done on the sintered body, depending on necessity, to increase its mechanical strength and material hardness, the improvement comprising introducing an electrically insulative synthetic resin material in the hollow cavity to integrally form a bearing member with said cylindrical body; and forming a plurality of grooves in said electrically conductive hollow cylindrical body from the outer peripheral surface thereof to a depth reaching said bearing material, and in parallel with the axial line, thereby defining a plurality of segments for the commutator.
Claim 7
Dependent Claim
114 words
In a method for manufacturing commutator, wherein a shaping material comprising an electrically conductive metal powder is placed in a shaping mold, compression-molded into a hollow cylindrical body, and sintered, re-compression being done on the sintered body, depending on necessity, to increase its mechanical strength and material hardness, the improvement comprising introducing an electrically insulative synthetic resin material in the hollow cavity to integrally form a bearing member with said cylindrical body; and forming a plurality of grooves in said electrically conductive hollow cylindrical body from the outer peripheral surface thereof to a depth reaching said bearing material, and in parallel with the axial line, thereby defining a plurality of segments for the commutator.
Claim 8
Dependent Claim
62 words
The method for manufacturing commutator as set forth in claim 5, in which said electrically conductive hollow cylindrical body as molded has a plurality of radial slits extending from the inner surface up to a half way in said cylindrical body, and said electrically insulative synthetic resin material also fills in said radial slits to increase rigid combination with said cylindrical body.
Claim 9
Dependent Claim
150 words
In a method for manufacturing a commutator, wherein a shaping material comprising an electrically conductive metal powder is placed in a shaping mold, compression-molded into a hollow cylindrical body, and sintered, re-compression being done on the sintered body, depending on necessity, to increase its mechanical strength and material hardness, the improvement comprising forming a radially outwardly, axially inwardly convergent tapered annular keying surface adjacent the two ends of said cylindrical body, filling an electrically insulative synthetic resin material in the said hollow cylindrical body, covering said tapered annular surface at both ends of said cylindrical body integrally, to form a bearing member; and, thereafter, forming a plurality of radial grooves in said hollow cylindrical body to a depth reaching said electrically insulative synthetic resin bearing material at substantially equal space intervals from the outer peripheral surface thereof, thereby dividing said cylindrical body into a plurality of segments for the commutator.
Claim 10
Dependent Claim
150 words
In a method for manufacturing a commutator, wherein a shaping material comprising an electrically conductive metal powder is placed in a shaping mold, compression-molded into a hollow cylindrical body, and sintered, re-compression being done on the sintered body, depending on necessity, to increase its mechanical strength and material hardness, the improvement comprising forming a radially outwardly, axially inwardly convergent tapered annular keying surface adjacent the two ends of said cylindrical body, filling an electrically insulative synthetic resin material in the said hollow cylindrical body, covering said tapered annular surface at both ends of said cylindrical body integrally, to form a bearing member; and, thereafter, forming a plurality of radial grooves in said hollow cylindrical body to a depth reaching said electrically insulative synthetic resin bearing material at substantially equal space intervals from the outer peripheral surface thereof, thereby dividing said cylindrical body into a plurality of segments for the commutator.
Claim 11
Dependent Claim
30 words
The method for manufacturing commutator as set forth in claim 7, in which said shaping material consists of from 85% to 95% of copper and 15% to 5% of carbon.
References Cited (Backward Citations)
DE63662C
Cited
US2053662A
Cited
DE1034262B
Cited
US3248215A
Cited
US3568309A
Cited
US3837819A
Cited
US3812576A
Cited
US4188713A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1985-11-08 | 1986-05-10 | 1986-11-09 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1989-11-08 | 1990-05-10 | 1990-11-09 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1993-11-08 | 1994-05-10 | 1994-11-09 | $7700.00 | Window Closed / Lapsed |