Chemiluminescence apparatus and method for determining the oxidative stability of polymers
Assignee: Individual
•
Filing: 1980-12-08
•
Granted: 1982-09-21
•
Expires: 2000-12-08
Abstract
Abstract A chemiluminescence apparatus and method for determining polymer stability by measuring the intensity of the light emitted during thermal oxidation. The apparatus described in the invention measures the light intensity vs. time from polymers in an oxidative atmosphere. On the basis of this information, important parameters such as induction time and oxidation rate can be obtained. The apparatus has the advantage of simultaneous multi-sample analysis and the mathematical approach enables data computerization.
Inventors
- 👤 Lawrence J. Broutman
- 👤 Boris Rozhansky
- 👤 Lev Zlatkevich
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-27 19:44
CPC Classifications
G; G01; G01N; G01N33/00; G01N33/44; G01N33/442; G01N17/00; G01N21/00; G01N21/75; G01N21/76
Claims Analysis
Total Claims: 21
Claim 1
Independent Claim
77 words
A method of determining chemical processes accompanied by chemiluminescence and oxidative stability of a polymer by measuring the chemiluminescence produced by auto-oxidation of the polymer comprising heating the polymer in a cell to elevated temperature, exposing the polymer to oxygen for thermal oxidation of the polymer, recording the light intensity versus time given off by the polymer during oxidation while at relatively constant temperature from which the chemiluminescence can be determined by auto oxidation of the polymer.
Claim 2
Independent Claim
77 words
A method of determining chemical processes accompanied by chemiluminescence and oxidative stability of a polymer by measuring the chemiluminescence produced by auto-oxidation of the polymer comprising heating the polymer in a cell to elevated temperature, exposing the polymer to oxygen for thermal oxidation of the polymer, recording the light intensity versus time given off by the polymer during oxidation while at relatively constant temperature from which the chemiluminescence can be determined by auto oxidation of the polymer.
Claim 3
Dependent Claim
29 words
The method as claimed in claim 1 in which the polymer in the cell is maintained under inert atmosphere until the inert atmosphere is replaced by an oxidative atmosphere.
Claim 4
Dependent Claim
24 words
The method as claimed in claim 1 in which the polymer is exposed to an oxidative atmosphere under flow of an oxygen containing gas.
Claim 5
Dependent Claim
88 words
Apparatus for determining polymer stability by measurement of the intensity of light emitted from the polymer during thermal oxidation comprising a dark chamber, a support for the polymer, means for moving the support into and out of the dark chamber, means for heating the polymer while in the dark chamber, means for exposing the polymer to an oxidative atmosphere containing gas while at elevated temperature within the chamber for thermal oxidation of the polymer and means for measuring the intensity of light emitted from the polymer during auto-oxidation.
Claim 6
Dependent Claim
88 words
Apparatus for determining polymer stability by measurement of the intensity of light emitted from the polymer during thermal oxidation comprising a dark chamber, a support for the polymer, means for moving the support into and out of the dark chamber, means for heating the polymer while in the dark chamber, means for exposing the polymer to an oxidative atmosphere containing gas while at elevated temperature within the chamber for thermal oxidation of the polymer and means for measuring the intensity of light emitted from the polymer during auto-oxidation.
Claim 7
Dependent Claim
18 words
Apparatus as claimed in claim 4 which includes means for maintaining an inert atmosphere within the dark chamber.
Claim 8
Dependent Claim
14 words
Apparatus as claimed in claim 4 in which the support comprises a metal plate.
Claim 9
Dependent Claim
29 words
Apparatus as claimed in claim 6 in which the means for heating the polymer while in the dark chamber comprises heaters adjacent the bottom side of the metal plate.
Claim 10
Dependent Claim
23 words
Apparatus as claimed in claim 4 which includes metal shavings for elevating the temperature of the oxygen containing gas before reaching the polymer.
Claim 11
Dependent Claim
25 words
Apparatus as claimed in claim 4 in which the support is in the form of a sliding stage which supports a plurality of test cells.
Claim 12
Dependent Claim
19 words
Apparatus as claimed in claim 9 which includes a glass cover for each test cell to prevent cross contamination.
Claim 13
Dependent Claim
25 words
Apparatus as claimed in claim 9 which includes enclosures for each test cell to restrict reaction volume and enhance replacement of one gas by another.
Claim 14
Dependent Claim
24 words
Apparatus as claimed in claim 9 which includes a means for enclosing the test polymer for exposure of the polymer to oxygen under pressure.
Claim 15
Dependent Claim
39 words
Apparatus as claimed in claim 9 which includes a partitioning plate which subdivides the dark chamber into an upper portion and a lower portion, said partitioning plate having openings which overlie the test cell when in position of use.
Claim 16
Dependent Claim
28 words
Apparatus as claimed in claim 13 which includes transparent windows to cover the openings in the partitioning plate for visual access to the test cells underlying the openings.
Claim 17
Dependent Claim
44 words
Apparatus as claimed in claim 9 which includes a photomultiplier and means for movement of the photomultiplier for sequential measurement of the light intensity being emitted from the test cells and a power source connected to the photomultiplier for supply of operative voltage thereto.
Claim 18
Dependent Claim
27 words
Apparatus as claimed in claim 15 which includes means for circulating cooling gas through the upper portion of the dark chamber to prevent overheating of the photomultiplier.
Claim 19
Dependent Claim
22 words
The method as claimed in claim 1 in which the polymer is exposed to oxygen for auto oxidation by oxygen under pressure.
Claim 20
Dependent Claim
23 words
The method as claimed in claim 1 in which the polymer is heated to a temperature 5°-30° C. below its melting point temperature.
Claim 21
Dependent Claim
28 words
The method as claimed in claim 18 in which the polymer is maintained at a temperature 5°-30° C. below its melting point during the auto oxidation period recorded.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1985-09-20 | 1986-03-22 | 1986-09-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1989-09-20 | 1990-03-22 | 1990-09-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1993-09-20 | 1994-03-22 | 1994-09-21 | $7700.00 | Window Closed / Lapsed |