US4349409A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method and apparatus for plasma etching
Assignee: Fujitsu Ltd
•
Filing: 1981-05-11
•
Granted: 1982-09-14
•
Expires: 2001-05-11
Abstract
Abstract A method and an apparatus for plasma etching semiconductor materials by providing an intermediate electrode between the electrodes in a parallel state type plasma etching apparatus, moving the intermediate electrode by a drive mechanism, and continuously changing from a condition of high input power and high self-bias voltage to a condition of low input power and low self-bias voltage while varying the distance between the intermediate electrode and the first electrode and the RF power, thereby to remove damage or deposits that may have been formed on the surface when the semiconductor material was being subjected to processing.
Inventors
- 👤 Hikou Shibayama
- 👤 Tetsuya Ogawa
- 👤 Makoto Kosugi
- 👤 Tokushige Hisatsugu
- 👤 Koichi Kobayashi
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 23:16
CPC Classifications
H; H01; H01J; H01J37/00; H01J37/32; H01J37/32431; H01J37/32623; H01J37/32532; H01J37/32568; H01J37/32587; H01J37/34; H01J37/3411; H01J37/3438; H10; H10P; H10P50/00; H10P50/20; H10P50/28; H10P50/282; H10P50/283
Claims Analysis
Total Claims: 20
Claim 1
Independent Claim
85 words
A method for effecting plasma etching of a semiconductor material comprising the steps of: providing a first and a second electrode and an electrically floating intermediate electrode, placing a semiconductor material on said first electrode and said electrically floated intermediate electrode, applying a high frequency power between said first and second electrode to produce a plasma between said first and second electrode, and etching the semiconductor material under the condition that the distance between said first and said intermediate electrode is changed during said etching.
Claim 2
Independent Claim
85 words
A method for effecting plasma etching of a semiconductor material comprising the steps of: providing a first and a second electrode and an electrically floating intermediate electrode, placing a semiconductor material on said first electrode and said electrically floated intermediate electrode, applying a high frequency power between said first and second electrode to produce a plasma between said first and second electrode, and etching the semiconductor material under the condition that the distance between said first and said intermediate electrode is changed during said etching.
Claim 3
Dependent Claim
72 words
A method as set forth in claim 1, wherein the semiconductor material is processed under the conditions of a high input power and a high self-bias voltage while maintaining a predetermined distance between the intermediate electrode and the first electrode, then said distance is reduced to be smaller than said predetermined distance, and the semiconductor material is further processed under the conditions of a low input power and a low self-bias voltage.
Claim 4
Dependent Claim
32 words
A method as set forth in claim 1 or 2, wherein the semiconductor material is subjected to the etching while continuously changing the distance between said intermediate electrode and said first electrode.
Claim 5
Dependent Claim
23 words
A method as set forth in claim 1 or 2, wherein a voltage from an external source is applied to said intermediate electrode.
Claim 6
Dependent Claim
104 words
A method as set forth in claim 1 or 2, wherein the distance between said intermediate electrode and said first electrode is set to a predetermined length, said high frequency power is set to a predetermined value, and wherein the semiconductor material is subjected to a first etching using a first reactive gas, the distance between said intermediate electrode and said first electrode is then reduced to be smaller than said predetermined length, the high frequency power is set to a value which is smaller than said predetermined value, and the semiconductor material is subjected to an additional etching using a second reactive gas.
Claim 7
Dependent Claim
73 words
A method as set forth in claim 5, wherein the semiconductor material comprises a substrate and a SiO 2 layer and wherein in the first etching the SiO 2 layer is removed using a first reactive gas selected from CHF 3 , C 2 F 6 , C 3 F 8 , and CF 4 +H 2 , and in the additional etching the second reactive gas is CF 4 +O 2 .
Claim 8
Dependent Claim
77 words
A method as set forth in claim 5, wherein the semiconductor material comprises a substrate and a Si 3 N 4 layer and wherein in the first etching the Si 3 N 4 layer is removed using a first reactive gas selected from CHF 3 , C 2 F 6 , C 3 F 8 , and CF 4 +H 2 , and in the additional etching the second reactive gas is CF 4 +O 2 .
Claim 9
Dependent Claim
31 words
The method of claim 6 or 7, wherein the pedetermined distance between the intermediate electrode and the first electrode in the initial etching is set at approximately 48 mm. or more.
Claim 10
Dependent Claim
19 words
The method of claim 6 or 7, wherein the thickness of the intermediate electrode is less than 2 mm.
Claim 11
Dependent Claim
17 words
The method of claim 8, wherein the thickness of the intermediate electrode is less than 2 mm.
Claim 12
Independent Claim
38 words
An apparatus for plasma etching comprising a first electrode, a second electrode, an electrically floated intermediate electrode positioned between said two electrodes, and a drive mechanism for varying the distance between said intermediate electrode and said first electrode.
Claim 13
Independent Claim
38 words
An apparatus for plasma etching comprising a first electrode, a second electrode, an electrically floated intermediate electrode positioned between said two electrodes, and a drive mechanism for varying the distance between said intermediate electrode and said first electrode.
Claim 14
Dependent Claim
23 words
An apparatus for plasma etching as set forth in claim 11, wherein the thickness of said intermediate electrode is smaller than 2 mm.
Claim 15
Dependent Claim
35 words
The apparatus of claim 11, wherein said intermediate electrode has spacers formed of an insulating material, facing the first electrode, and with a thickness for maintaining a predetermined distance between the first and intermediate electrodes.
Claim 16
Dependent Claim
39 words
The apparatus of claim 11 or 13, wherein said intermediate electrode has electrically conductive support rods facing the second electrode, wherein the second electrode becomes electrically conductive to the intermediate electrode when the support rods contact the second electrode.
Claim 17
Dependent Claim
23 words
The apparatus of claim 11, further comprising a housing for containing said first, second, and intermediate electrodes and introducing an etching plasma therein.
Claim 18
Dependent Claim
20 words
The apparatus of claim 15, further comprising means external of said housing for supplying a voltage to the intermediate electrode.
Claim 19
Dependent Claim
20 words
The apparatus of claim 15, further comprising means internal of said housing for supplying a voltage to the intermediate electrode.
Claim 20
Dependent Claim
30 words
The apparatus of claim 17, wherein said internal voltage supplying means comprises at least one resistor connected between the intermediate and first electrodes or between the intermediate and second electrodes.
References Cited (Backward Citations)
US4233109A
Cited
US4174251A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1985-09-13 | 1986-03-15 | 1986-09-14 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1989-09-13 | 1990-03-15 | 1990-09-14 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1993-09-13 | 1994-03-15 | 1994-09-14 | $7700.00 | Window Closed / Lapsed |