Abstract
Abstract A thermally processable imaging element and method are disclosed, wherein dimensional changes after thermal processing for about 5 seconds at a temperature of about 125° C., do not exceed ±0.03%. The imaging element features an amine-generating and an amine-responsive composition. The method features preheating the element prior to exposure to dimensionally stabilize it.
Inventors
- 👤 Raymond F. Limoges
- 👤 Anthony A. Scribani
- 👤 Robert J. Wilson
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 09:10
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/67; Y; Y10; Y10S; Y10S430/00; Y10S430/136; Y10S430/137; Y10S430/14
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
187 words
In a method of making an imaging element comprising, on a polymeric film support, at least one layer comprising an amine-generating composition that includes a reducible cobalt(III) complex containing releasable amine ligands, and an amine-responsive dye precursor; the method comprising the steps of (a) coating said composition and said precursor onto a support having dimensional changes that are no greater than ±0.1% in width and length when heated in an uncoated state for about 5 seconds at a temperature of about 125° C., to form at least one layer and; (b) drying said layer to form the element; the improvement wherein said method further includes, prior to exposure of the element to activating radiation, the additional steps of (c) dimensionally stabilizing said dried element by heating said dried element to a temperature of between about 100° C. and about 140° C. for a length of time sufficient to form in said element an overall thermal-reaction hysteresis that produces dimensional changes of no greater than ±0.03% in width or length when said element is processed by heating for about 5 seconds at a temperature of about 125° C.
Claim 2
Dependent Claim
187 words
In a method of making an imaging element comprising, on a polymeric film support, at least one layer comprising an amine-generating composition that includes a reducible cobalt(III) complex containing releasable amine ligands, and an amine-responsive dye precursor; the method comprising the steps of (a) coating said composition and said precursor onto a support having dimensional changes that are no greater than ±0.1% in width and length when heated in an uncoated state for about 5 seconds at a temperature of about 125° C., to form at least one layer and; (b) drying said layer to form the element; the improvement wherein said method further includes, prior to exposure of the element to activating radiation, the additional steps of (c) dimensionally stabilizing said dried element by heating said dried element to a temperature of between about 100° C. and about 140° C. for a length of time sufficient to form in said element an overall thermal-reaction hysteresis that produces dimensional changes of no greater than ±0.03% in width or length when said element is processed by heating for about 5 seconds at a temperature of about 125° C.
Claim 3
Dependent Claim
181 words
In a method of making an imaging element comprising, on a polymeric film support, at least one layer comprising an amine-generating composition that includes a reducible cobalt(III) complex containing releasable amine ligands, and an amine-responsive dye precursor; the method comprising the steps of (a) coating said composition and said precursor onto a support having dimensional changes that are no greater than ±0.1% in width and length when heated in an uncoated state for about 5 seconds at a temperature of about 125° C., to form at least one layer and; (b) drying said layer to form the element; the improvement wherein said method further includes, prior to exposure of the element to activating radiation, the additional step of (c) dimensionally stabilizing said element by heating said dried element to a temperature of between about 100° C. and about 140° C. for a time of between about 2 and about 20 seconds, whereby the overall thermal-reaction hysteresis of the element provides a dimensional change of no greater than ±0.03% in width or length when processed under the heating conditions of step (a).
Claim 4
Dependent Claim
181 words
In a method of making an imaging element comprising, on a polymeric film support, at least one layer comprising an amine-generating composition that includes a reducible cobalt(III) complex containing releasable amine ligands, and an amine-responsive dye precursor; the method comprising the steps of (a) coating said composition and said precursor onto a support having dimensional changes that are no greater than ±0.1% in width and length when heated in an uncoated state for about 5 seconds at a temperature of about 125° C., to form at least one layer and; (b) drying said layer to form the element; the improvement wherein said method further includes, prior to exposure of the element to activating radiation, the additional step of (c) dimensionally stabilizing said element by heating said dried element to a temperature of between about 100° C. and about 140° C. for a time of between about 2 and about 20 seconds, whereby the overall thermal-reaction hysteresis of the element provides a dimensional change of no greater than ±0.03% in width or length when processed under the heating conditions of step (a).
Claim 5
Dependent Claim
30 words
A method as defined in claim 1 or 2, wherein said element is heated prior to exposure for at least 5 seconds at a temperature of at least 120° C.
Claim 6
Independent Claim
159 words
A method of dimensionally stabilizing a dried imaging element comprising, on a polymeric film support, at least one layer comprising an amine-generating composition that includes a reducible cobalt(III) complex containing releasable amine ligands, and an amine-responsive dye precursor; said support having dimensional changes that are no greater than ±0.1% in width and length when heated in an uncoated state for about 5 seconds at a temperature of about 125° C.; the method comprising prior to exposure of the element to activating radiation, the step of dimensionally stabilizing said element by heating said element to a temperature of between about 100° C. and about 140° C. for a time of between about 2 and about 20 seconds, whereby the overall thermal-reaction hysteresis of the element provides a dimensional change of no greater than ±0.3% in width or length when processed under the heating conditions of step (a) by heating for about 5 seconds at a temperature of about 125° C.
Claim 7
Independent Claim
159 words
A method of dimensionally stabilizing a dried imaging element comprising, on a polymeric film support, at least one layer comprising an amine-generating composition that includes a reducible cobalt(III) complex containing releasable amine ligands, and an amine-responsive dye precursor; said support having dimensional changes that are no greater than ±0.1% in width and length when heated in an uncoated state for about 5 seconds at a temperature of about 125° C.; the method comprising prior to exposure of the element to activating radiation, the step of dimensionally stabilizing said element by heating said element to a temperature of between about 100° C. and about 140° C. for a time of between about 2 and about 20 seconds, whereby the overall thermal-reaction hysteresis of the element provides a dimensional change of no greater than ±0.3% in width or length when processed under the heating conditions of step (a) by heating for about 5 seconds at a temperature of about 125° C.
References Cited (Backward Citations)
US2627088A
Cited
US2779684A
Cited
GB1000361A
Cited
US3834928A
Cited
US3939000A
Cited
US4141735A
Cited
US4076532A
Cited
JPS52149117A
Cited
US4112280A
Cited
US4255481A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1985-08-30 | 1986-03-01 | 1986-08-31 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1989-08-30 | 1990-03-01 | 1990-08-31 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1993-08-30 | 1994-03-01 | 1994-08-31 | $7700.00 | Window Closed / Lapsed |