Abstract

Abstract An effective amount of a copolymer of maleic acid or anhydride and allyl sulfonic acid when added to the water to be treated provides increased inhibition of scale formation in evaporative desalination units.

Inventors

  • 👤 Arthur M. Schiller
  • 👤 James S. Balcerski

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 10:27
CPC Classifications
C; C02; C02F; C02F1/00; C02F1/02; C02F1/04; C02F1/042; C02F5/00; C02F5/08; C02F5/10; Y; Y02; Y02A; Y02A20/00; Y02A20/124

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 130 words
In a process for inhibiting scaling in evaporative desalination units comprising adding to the water to be treated an aliphatic copolymer derived from a monovinyl compound and a vinyl sulfonate, the improvement therein providing improved inhibition of magnesium hydroxide in desalination units operating at temperatures above 90° C. comprising selecting as the copolymer additive one derived from about 50 mole percent of maleic acid or anhydride and, correspondingly, from about 50 mole percent of allyl sulfonic acid, said copolymer having a molecular weight in the range of about 500 to about 10,000, adding the copolymer to the water to be treated in an amount effective to inhibit magnesium hydroxide scaling, heating the water in the desalination unit to temperatures above 90° C. and substantially inhibiting the magnesium hydroxide precipitation therein.
Claim 2
Dependent Claim 130 words
In a process for inhibiting scaling in evaporative desalination units comprising adding to the water to be treated an aliphatic copolymer derived from a monovinyl compound and a vinyl sulfonate, the improvement therein providing improved inhibition of magnesium hydroxide in desalination units operating at temperatures above 90° C. comprising selecting as the copolymer additive one derived from about 50 mole percent of maleic acid or anhydride and, correspondingly, from about 50 mole percent of allyl sulfonic acid, said copolymer having a molecular weight in the range of about 500 to about 10,000, adding the copolymer to the water to be treated in an amount effective to inhibit magnesium hydroxide scaling, heating the water in the desalination unit to temperatures above 90° C. and substantially inhibiting the magnesium hydroxide precipitation therein.
Claim 3
Dependent Claim 24 words
The process of claim 1 wherein the amount of copolymer added is from about 0.2 to 2,000 parts per million of the water treated.

References Cited (Backward Citations)

US3706717A Cited
US3879288A Cited
US4001134A Cited
US4166041A Cited
US4253968A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-08-02 1986-02-01 1986-08-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-08-02 1990-02-01 1990-08-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-08-02 1994-02-01 1994-08-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag