Abstract

Abstract An additive for deep-well cement slurries comprising a water-soluble anionic copolymer having a molecular weight from about 50,000 to 500,000 and comprising about 1 to 60 mole % of anionic structural units and about 99 to 40 mole % of nonanionic structural units. A preferred additive comprises a terpolymer of acrylamide, sodium acrylate and sodium vinylsulphonate. The additives retard the setting action of the slurry, stabilize the slurry, prevent the swelling of readily hydratable clays and are resistant to electrolytes which would accelerate setting and seepage of water from the slurry.

Inventors

  • 👤 Wolfgang Hubner
  • 👤 Otto Schroers
  • 👤 Hans J. Sladeck

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 19:36
CPC Classifications
C; C09; C09K; C09K8/00; C09K8/50; C09K8/504; C09K8/506; C09K8/508; C09K8/512; C04; C04B; C04B24/00; C04B24/16; C04B24/24; C04B24/26; C04B24/2652; C09K8/42; C09K8/46; C09K8/467; C09K8/487; C04B2103/00; C04B2103/46

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 72 words
In the cementing of a deep-well employing a deep-well cement slurry, the improvement which comprises including in such cement or cement slurry an additive comprising a water-soluble anionic copolymer having a molecular weight from 50,000 to 500,000 and comprising 1 to 60 mole% of anionic structural units and 99 to 40 mole% of non-ionic structural units, the copolymer having been obtained by radical polymerization of a substantially neutral solution of the monomers.
Claim 2
Dependent Claim 72 words
In the cementing of a deep-well employing a deep-well cement slurry, the improvement which comprises including in such cement or cement slurry an additive comprising a water-soluble anionic copolymer having a molecular weight from 50,000 to 500,000 and comprising 1 to 60 mole% of anionic structural units and 99 to 40 mole% of non-ionic structural units, the copolymer having been obtained by radical polymerization of a substantially neutral solution of the monomers.
Claim 3
Dependent Claim 18 words
A method according to claim 1, wherein the copolymer has a molecular weight from about 60,000 to 150,000.
Claim 4
Dependent Claim 18 words
A method according to claim 1, wherein the copolymer has a molecular weight from about 70,000 to 150,000.
Claim 5
Dependent Claim 31 words
A method according to claim 1, wherein the copolymer comprises about 10 to 50 mole % of anionic structural units and about 90 to 50 mole % of non-ionic structural units.
Claim 6
Dependent Claim 31 words
A method according to claim 1, wherein the copolymer comprises about 20 to 40 mole % of anionic structural units and about 80 to 60 mole % of non-ionic structural units.
Claim 7
Dependent Claim 22 words
A method according to claim 1, wherein the anionic structural units of the copolymer comprise salts of acrylic acid and/or methacrylic acid.
Claim 8
Dependent Claim 18 words
A method according to claim 1, wherein the non-ionic structural units of the copolymer comprise acrylamide and/or methacrylamide.
Claim 9
Dependent Claim 17 words
A method according to claim 1, wherein the copolymer comprises units of acrylamide and acrylic acid salts.
Claim 10
Dependent Claim 60 words
A method according to claim 1, wherein the copolymer further comprises up to about 10 mole % based on the sum of all monomeric structural units of at least one water-soluble monomer selected from the group consisting of vinylsulphonic acid, vinylpyrrolidone, esters of amino alcohols and acrylic acid, esters of amino alcohols and methacrylic acid and acrylic acid amidosulphonic acid.
Claim 11
Dependent Claim 46 words
A method according to claim 1, wherein the copolymer further comprises up to about 10 mole % based on the sum of all monomeric structural units of at least one water-insoluble monomer selected from the group consisting of acrylic acid esters, methacrylic acid esters and acrylonitrile.
Claim 12
Dependent Claim 16 words
A method according to claim 9, comprising a terpolymer of acrylamide, sodium acrylate and sodium vinylsulphonate.
Claim 13
Dependent Claim 19 words
A method according to claim 1, dissolved in water to a concentration of about 1 to 40% by weight.
Claim 14
Dependent Claim 42 words
A method according to claim 11, wherein in making the slurry the additive is added to the cement as an aqueous solution of about 1 to 40% concentration, the additive being present in about 0.1 to 2% by weight of the cement.

References Cited (Backward Citations)

US2775557A Cited
US2868753A Cited
US3937633A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-07-19 1986-01-18 1986-07-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-07-19 1990-01-18 1990-07-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-07-19 1994-01-18 1994-07-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag