A method of making bituminous concrete having a sulfur-extended asphalt binder comprising the steps of: heating liquid asphalt cement to a temperature of at least 300° F. but less than 305° F.; adding solid sulfur in substantially crushed form to the heated asphalt cement on substantially a 1:1 weight basis; pre-blending the solid sulfur and asphalt cement together while transferring from the asphalt cement to the sulfur a major portion of the heat required to melt the sulfur until the sulfur has been melted and dispersed throughout the asphalt cement, and adding heat during the pre-blending step or as required to maintain the temperature above the melting point of sulfur; heating aggregate in a drying apparatus to a maximum temperature of 305° F; and introducing the liquid blend of sulfur and asphalt cement into the heated aggregate to form bituminous concrete, the amount of asphalt being less than 3.1% by weight of the bituminous concrete.
Claim 2
Independent Claim
155 words
A method of making bituminous concrete having a sulfur-extended asphalt binder comprising the steps of: heating liquid asphalt cement to a temperature of at least 300° F. but less than 305° F.; adding solid sulfur in substantially crushed form to the heated asphalt cement on substantially a 1:1 weight basis; pre-blending the solid sulfur and asphalt cement together while transferring from the asphalt cement to the sulfur a major portion of the heat required to melt the sulfur until the sulfur has been melted and dispersed throughout the asphalt cement, and adding heat during the pre-blending step or as required to maintain the temperature above the melting point of sulfur; heating aggregate in a drying apparatus to a maximum temperature of 305° F; and introducing the liquid blend of sulfur and asphalt cement into the heated aggregate to form bituminous concrete, the amount of asphalt being less than 3.1% by weight of the bituminous concrete.
Claim 3
Dependent Claim
39 words
The method of claim 1, and selectively varying the binder content of the bituminous concrete to obtain desired paving lay down criteria so as to assure use of the 1:1 by weight addition of solid sulfur to asphalt cement.
Claim 4
Dependent Claim
21 words
The method of claim 1, and compacting the final mixture prior to cooling to form a layer of bituminous concrete pavement.
Claim 5
Dependent Claim
41 words
The method of claim 1, and heating the aggregate to a temperature of no more than 305° F., whereby when the solid sulfur is added to and blended with the heated asphalt cement, substantially no harmful sulfur-related gas emissions are produced.
Claim 6
Independent Claim
125 words
The method of making a sulfur-extended asphalt composition, comprising the steps of: heating asphalt cement to a temperature of at least 300° F. but less than 305° F.; adding solid sulfur in a substantially crushed form to the heated asphalt cement on substantially a 1:1 weight basis; utilizing the heat present in the heated asphalt cement to provide a major portion of the heat required to melt the solid sulfur; pre-blending the melted sulfur and asphalt cement together into a substantially homogeneous mixture while adding heat to maintain the temperature of the mixture above the melting point of sulfur; and mixing the blended mixture of sulfur and asphalt cement with heated aggregate, the asphalt being less than 3.1% by weight of the resulting bituminous concrete.
Claim 7
Independent Claim
125 words
The method of making a sulfur-extended asphalt composition, comprising the steps of: heating asphalt cement to a temperature of at least 300° F. but less than 305° F.; adding solid sulfur in a substantially crushed form to the heated asphalt cement on substantially a 1:1 weight basis; utilizing the heat present in the heated asphalt cement to provide a major portion of the heat required to melt the solid sulfur; pre-blending the melted sulfur and asphalt cement together into a substantially homogeneous mixture while adding heat to maintain the temperature of the mixture above the melting point of sulfur; and mixing the blended mixture of sulfur and asphalt cement with heated aggregate, the asphalt being less than 3.1% by weight of the resulting bituminous concrete.
Claim 8
Dependent Claim
37 words
The invention of claim 5, and selectively adjusting the binder content of the resulting asphalt composition to obtain desired lay down characteristics, thereby allowing use of the 1:1 by weight addition of solid sulfur to asphalt cement.
Claim 9
Dependent Claim
90 words
A bituminous concrete mix having a sulfur-extended asphalt binder, comprising in combination: solid sulfur being by weight between 2.0 and 2.75% of the total bituminous concrete mix; liquid asphalt having a temperature of less than 305° F. being by weight no more than 3.1% of the total bituminous concrete mix, the solid sulfur and liquid asphalt being present on substantially a 1:1 weight basis; and heated aggregate having a temperature of less than 305° F. including fillers being by weight between 93 and 95% of the total bituminous concrete mix.
Claim 10
Dependent Claim
90 words
A bituminous concrete mix having a sulfur-extended asphalt binder, comprising in combination: solid sulfur being by weight between 2.0 and 2.75% of the total bituminous concrete mix; liquid asphalt having a temperature of less than 305° F. being by weight no more than 3.1% of the total bituminous concrete mix, the solid sulfur and liquid asphalt being present on substantially a 1:1 weight basis; and heated aggregate having a temperature of less than 305° F. including fillers being by weight between 93 and 95% of the total bituminous concrete mix.