Abstract The invention provides a novel method for preventing bleeding of a plasticizer or other additive ingredients contained in a shaped article of a vinyl chloride-based resin composition on to the surface of the article by the treatment with low temperature plasma. Different from conventional procedures for the plasma treatment, much improved reliability and reproducibility as well as effectiveness are obtained by subjecting the article to intermittent exposure to the plasma atmosphere instead of continuous exposure. In the inventive method, the overall treatment time is an alternate sequence of exposure times, each being of the length of 0.001 second to 1000 seconds, and repose times, each being also of the length of 0.001 second to 1000 seconds. The gas for the plasma atmosphere is desirably an inorganic gas selected from the gases other than oxygenic gases, halogen containing gases and sulfur containing gases.
A method for modifying surface properties of a shaped article composed of a vinyl chloride-based resin composition and having a plasticizer therein which comprises subjecting the surface of the article to intermittent exposure to an atmosphere of low temperature plasma of an inorganic gas under a pressure in the range from 0.01 Torr to 1.0 Torr for a length of the treatment time which is an alternate sequence of at least five alternating exposure and repose times wherein the length of each of the exposure times is in the range from 0.001 second to 1000 seconds and the length of each of the repose times is in the range from 0.001 second to 1000 seconds.
Claim 2
Independent Claim
115 words
A method for modifying surface properties of a shaped article composed of a vinyl chloride-based resin composition and having a plasticizer therein which comprises subjecting the surface of the article to intermittent exposure to an atmosphere of low temperature plasma of an inorganic gas under a pressure in the range from 0.01 Torr to 1.0 Torr for a length of the treatment time which is an alternate sequence of at least five alternating exposure and repose times wherein the length of each of the exposure times is in the range from 0.001 second to 1000 seconds and the length of each of the repose times is in the range from 0.001 second to 1000 seconds.
Claim 3
Dependent Claim
25 words
The method as claimed in claim 1 wherein the inorganic gas is selected from the gases other than oxygenic gases, halogen compounds and sulfur compounds.
Claim 4
Dependent Claim
26 words
The method as claimed in claim 1 wherein the length of each of the exposure times is in the range from 0.01 second to 100 seconds.
Claim 5
Dependent Claim
26 words
The method as claimed in claim 1 wherein the length of each of the repose times is in the range from 0.01 second to 100 seconds.