Method for elevated-temperature bonding of material with different coefficients of thermal expansion
Assignee: Lockheed Martin Corp
•
Filing: 1980-12-09
•
Granted: 1982-02-09
•
Expires: 2000-12-09
Abstract
Abstract A method to eliminate stresses and consequent warping in elevated-temperature cured adhesive bonded parts with different coefficients of thermal expansion.
Inventors
- 👤 Robert C. Webber
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-30 21:38
CPC Classifications
B; B32; B32B; B32B37/00; B32B37/14; B32B37/144; B29; B29C; B29C66/00; B29C66/01; B29C66/05; B29C66/10; B29C66/11; B29C66/112; B29C66/1122; B32B37/10; C; C09; C09J; C09J5/00; C09J5/06; B29C65/00; B29C65/02; B29C65/48; B29C65/4805; B29C65/483; B29C65/4835; B29C65/56; B29C65/64; B29C66/40; B29C66/41; B29C66/45; B29C66/70; B29C66/73; B29C66/731; B29C66/7311; B29C66/73111; B29C66/73112; B29C66/74; B29C66/742; B32B2307/00; B32B2307/70; B32B2307/732; B32B2307/734
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
165 words
A method for reducing post-adhesive-cured warping or deformation of thermal cured adhesive bonded adherends having different coefficients of thermal expansion comprising the steps of: (a) stacking the adherends in a clamping means with a thermal curing adhesive in an uncured state between each adjacent pair of adherends; (b) compressing one pair of opposite side edges of the adherends by closure of the clamping means by an amount substantially equal to the amount of thermal expansion the clamping means will experience between the clamping means members compressing the adherends by the temperature differential between the clamping temperature and the adhesive cure temperature so that the dimension between the opposite side edges of the adherends at the adhesive cure temperature will be substantially the same dimension as at the clamping temperature; (c) elevating the temperature of the clamping means, the adherends and the adhesive to at least the cure temperature of the adhesive; and (d) after cure of the adhesive, removing the adherends from the clamping means.
Claim 2
Independent Claim
165 words
A method for reducing post-adhesive-cured warping or deformation of thermal cured adhesive bonded adherends having different coefficients of thermal expansion comprising the steps of: (a) stacking the adherends in a clamping means with a thermal curing adhesive in an uncured state between each adjacent pair of adherends; (b) compressing one pair of opposite side edges of the adherends by closure of the clamping means by an amount substantially equal to the amount of thermal expansion the clamping means will experience between the clamping means members compressing the adherends by the temperature differential between the clamping temperature and the adhesive cure temperature so that the dimension between the opposite side edges of the adherends at the adhesive cure temperature will be substantially the same dimension as at the clamping temperature; (c) elevating the temperature of the clamping means, the adherends and the adhesive to at least the cure temperature of the adhesive; and (d) after cure of the adhesive, removing the adherends from the clamping means.
Claim 3
Dependent Claim
40 words
A method as claimed in claim 1 wherein the step comprising providing planar retention of the adherends in the clamping means to eliminate bowing or arching of the adherends in their compressed state is utilized between steps (b) and (c).
Claim 4
Dependent Claim
23 words
A method as claimed in claim 2 wherein the planar retention step includes vacuum bag packaging of the clamping means, adherends and adhesive.
Claim 5
Dependent Claim
23 words
A method as claimed in claim 2 wherein the planar retention step includes placement of a weight means planarly on the adherend stack.
Claim 6
Dependent Claim
23 words
A method as claimed in claim 2 wherein the planar retention step includes planarly clamping of the adherend stack to the clamping means.
Claim 7
Dependent Claim
35 words
A method as claimed in claim 1 wherein the removal of adherends from the clamping means in step (d) occurs during cool down from the adhesive curing temperature and before attainment of ambient room temperature.
Claim 8
Dependent Claim
32 words
A method as claimed in claim 1 wherein the removal of adherends from the clamping means in step (d) occurs at ambient room temperature after cool down from the adhesive curing temperature.
Claim 9
Dependent Claim
30 words
A method as claimed in claim 1 wherein an additional step (b) is included on a second pair of opposite side edges of the adherends utilizing a second clamping means.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1985-02-08 | 1985-08-10 | 1986-02-09 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1989-02-08 | 1989-08-10 | 1990-02-09 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1993-02-08 | 1993-08-10 | 1994-02-09 | $7700.00 | Window Closed / Lapsed |