Abstract

Abstract A cam of a camshaft has its surface hardened by rotating the camshaft about its axis while maintaining a TIG torch at a fixed spacing from the surface, and while relatively axially reciprocating the torch and the camshaft so the torch heats the surface along an undulating path. The pitch or crest-to-crest spacing of this path is maintained constant for uniform hardening either by varying the angular rotation rate of the camshaft or by varying the axial reciprocation frequency between the camshaft and torch. The radial spacing of the portion of the surface being heated at a given instant from the axis is measured to control the rotation or reciprocation rate.

Inventors

  • 👤 Volker Riedl

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 21:10
CPC Classifications
C; C21; C21D; C21D9/00; C21D9/30; C21D1/00; C21D1/06; C21D1/09

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 120 words
A method of surface-hardening an object having an axis and an eccentric surface, said method comprising the steps of: rotating said object about said axis at an angular speed rate; juxtaposing a torch-type heat source with and directing same radially at said surface; displacing said heat source radially of said axis relative to said eccentric surface during rotation thereof to hold said heat source at a substantially fixed radial distance from said surface; relatively axially reciprocating said heat source and said object during rotation thereof at a reciprocation rate so that said heat source heats said surface along an undulating path; and varying one of said rates in such a manner that the pitch of said path remains substantially constant.
Claim 2
Independent Claim 120 words
A method of surface-hardening an object having an axis and an eccentric surface, said method comprising the steps of: rotating said object about said axis at an angular speed rate; juxtaposing a torch-type heat source with and directing same radially at said surface; displacing said heat source radially of said axis relative to said eccentric surface during rotation thereof to hold said heat source at a substantially fixed radial distance from said surface; relatively axially reciprocating said heat source and said object during rotation thereof at a reciprocation rate so that said heat source heats said surface along an undulating path; and varying one of said rates in such a manner that the pitch of said path remains substantially constant.
Claim 3
Dependent Claim 31 words
The method defined in claim 1 wherein said one rate is generally varied in dependence on the instantaneous radial distance between the location juxtaposed with said heat source and said axis.
Claim 4
Dependent Claim 115 words
The method defined in claim 2 wherein said one rate is the instantaneous angular speed ω i of the object about the axis and is varied in accordance with the formula: ω.sub.i =(r.sub.min /r.sub.i)ω.sub.min sinγ.sub.i wherein: r min is the radius of the surface at its region of smallest (minimum) radius; r i is the instantaneous radius from the location juxtaposed with the heat source; ω min is the angular speed of the object when the source is juxtaposed with the region of smallest radius; and γ i is the instantaneous angle between a plane tangent to the surface at the location juxtaposed with the source and a plane through the location and the axis.
Claim 5
Dependent Claim 120 words
The method defined in claim 2 wherein said one rate is the instantaneous axial reciprocation frequency f i between the object and the source and is varied in accordance with the formula: f.sub.i =(r.sub.i /r.sub.min)f.sub.min /sinγ.sub.i wherein: r min is the radius of the surface at its region of smallest (minimum) radius; r i is the instantaneous radius from the location juxtaposed with the heat source; f min is the axial reciprocation frequency of the object and the source when the source is juxtaposted with the region of smallest diameter; and γ i is the instantaneous angle between a plane tangent to the surface at the location juxtaposed with the source and a plane through the location and the axis.
Claim 6
Dependent Claim 23 words
The method defined in claim 1 wherein said object is a camshaft having a plurality of cams, each cam having one such surface.

References Cited (Backward Citations)

US3231434A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-01-25 1985-07-27 1986-01-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-01-25 1989-07-27 1990-01-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-01-25 1993-07-27 1994-01-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag