Abstract

Abstract A process for the production of storable 2-chloro-1,3-butadiene/sulphur copolymers by peptization using sulphur containing petizing agents, wherein a compound corresponding to the following general formula: R1-Sn-R1 wherein n represents an integer having a value of from 2 to 10, preferably from 3 to 8 and, more particularly, from 4 to 6; and R1 represents a C6-C14 aryl radical, a C6-C14 aryl-C1-C3 alkyl radical or a heterocycle containing from 1 to 3 hereto atoms, such as N, which may be the same or different and which may optionally be substituted; optionally in combination with a nucleophilic substance, is added to the latex and peptized at from 5 DEG to 100 DEG C. and at pH of from 14 to 3.

Inventors

  • 👤 Rudiger Musch
  • 👤 Rudiger Schubart
  • 👤 Wilhelm Gobel
  • 👤 Gottfried Pampus

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 21:23
CPC Classifications
C; C08; C08F; C08F36/00; C08F36/02; C08F36/04; C08F36/14; C08F36/16; C08F36/18; C08C; C08C19/00; C08C19/08

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 120 words
A process for producing storable 2-chloro-1,3-butadiene/sulfur copolymer latex by peptization of a highly viscous 2-chloro-1,3-butadiene/sulfur copolymer latex using a sulfur containing peptizing agent wherein as the peptizing agent a compound of the formula R 1 --S n --R 1 is added to the highly viscous latex of said copolymer after polymerization and the copolymer is peptized at from 5° to 100° C. at a pH of from 14 to 3, n being an integer of from 4 to 6 and R 1 being selected from the group consisting of aryl having 6 to 14 carbon atoms and aralkyl wherein the aryl moiety has from 6 to 14 carbon atoms and the alkyl moiety has from 1 to 3 carbon atoms.
Claim 2
Dependent Claim 120 words
A process for producing storable 2-chloro-1,3-butadiene/sulfur copolymer latex by peptization of a highly viscous 2-chloro-1,3-butadiene/sulfur copolymer latex using a sulfur containing peptizing agent wherein as the peptizing agent a compound of the formula R 1 --S n --R 1 is added to the highly viscous latex of said copolymer after polymerization and the copolymer is peptized at from 5° to 100° C. at a pH of from 14 to 3, n being an integer of from 4 to 6 and R 1 being selected from the group consisting of aryl having 6 to 14 carbon atoms and aralkyl wherein the aryl moiety has from 6 to 14 carbon atoms and the alkyl moiety has from 1 to 3 carbon atoms.
Claim 3
Dependent Claim 29 words
A process as claimed in claim 1 wherein the compound of said formula is added in an amount of from 0.1 to 10 millimoles per 100 g of copolymer.
Claim 4
Dependent Claim 29 words
A process as claimed in claim 1 wherein the compound of said formula is added in an amount of from 0.2 to 5 millimoles per 100 g of copolymer.
Claim 5
Dependent Claim 17 words
A process as claimed in claim 1 wherein a nucleophilic substance is added to said copolymer latex.

References Cited (Backward Citations)

US2234215A Cited
GB1040954A Cited
US3507825A Cited
US3808183A Cited
US3816323A Cited
US3795655A Cited
US3852250A Cited
US4051078A Cited
US4124754A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-11-30 1985-06-01 1985-12-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-11-30 1989-06-01 1989-12-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-11-30 1993-06-01 1993-12-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag