Patent US2283139A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4301104A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for self-crimping acrylic fiber from a melt of two non-compatible polymers

Assignee: Wyeth Holdings LLC
•
Filing: 1980-03-12
•
Granted: 1981-11-17
•
Expires: 2000-03-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A self-crimping, melt-spun acrylonitrile polymer fiber comprising as the continuous fiber matrix a first polymer comprising from about 80 to about 99 weight percent acrylonitrile and from about 1 to about 20 weight percent of one or more monomers copolymerizable with acrylonitrile and heterogeneously dispersed within said fiber matrix a second polymer incompatible with said first polymer.

Inventors

  • 👤 William E. Streetman
  • 👤 Shashikumar H. Daftary

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 03:34
CPC Classifications
D; D01; D01D; D01D5/00; D01D5/22; Y; Y10; Y10S; Y10S525/00; Y10S525/931

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 173 words
A process for producing a self-crimping acrylonitrile polymer fiber which comprises preparing a fusion melt of water and (1) a first polymer comporising from about 80 to about 99 weight percent acrylonitrile and about 1 to about 20 weight percent of one or more monomers copolymerizable with acrylonitrile and (2) a second polymer incompatible with said first polymer and having thermal and/or hydrophilic properties which differ from those of said first polymer by an amount sufficient to provide self-crimping properties in said fiber, said first polymer constituting the major weight proportion of polymer and said fusion melt being free of any separate phase of water and/or unmelted polymer, dispersing the second polymer melt heterogeneously within the first polymer melt, extruding the resultant dispersion through a spinneret directly into a steam-pressurized solidification zone maintained under conditions which control the rate of release of water from the nascent extrudate, enable the extrude to solidify and maintain the solidified extrudate in plastic state and subjecting the plastic extrudate to stretching to provide desirable textile properties therein.
Claim 2
Dependent Claim 173 words
A process for producing a self-crimping acrylonitrile polymer fiber which comprises preparing a fusion melt of water and (1) a first polymer comporising from about 80 to about 99 weight percent acrylonitrile and about 1 to about 20 weight percent of one or more monomers copolymerizable with acrylonitrile and (2) a second polymer incompatible with said first polymer and having thermal and/or hydrophilic properties which differ from those of said first polymer by an amount sufficient to provide self-crimping properties in said fiber, said first polymer constituting the major weight proportion of polymer and said fusion melt being free of any separate phase of water and/or unmelted polymer, dispersing the second polymer melt heterogeneously within the first polymer melt, extruding the resultant dispersion through a spinneret directly into a steam-pressurized solidification zone maintained under conditions which control the rate of release of water from the nascent extrudate, enable the extrude to solidify and maintain the solidified extrudate in plastic state and subjecting the plastic extrudate to stretching to provide desirable textile properties therein.
Claim 3
Dependent Claim 28 words
The process of claim 1 including the additional step of drying the stretched extrudate at a dry-bulb temperature of 120°-180° C. and a wet-bulb temperature of 60°-100° C.
Claim 4
Dependent Claim 18 words
The process of claim 1 including the additional step of relaxing the stretched extrudate in steam under pressure.
Claim 5
Dependent Claim 37 words
The process of claim 1 including the additional steps of drying the stretched extrudate at a dry-bulb temperature of 120°-180° C. and a wet-bulb temperature of 60°-100° C. and relaxing the dried extrudate in steam under pressure.

References Cited (Backward Citations)

DE1469105A1 Cited
US3033813A Cited
US4166091A Cited
US4205039A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-11-16 1985-05-18 1985-11-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-11-16 1989-05-18 1989-11-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-11-16 1993-05-18 1993-11-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag