Abstract

Abstract A magnetic alloy which contains not less than 0.03 weight % but not more than 5.0 weight % of P not less than 3.0 weight % but not more than 26.0 weight % of Al and Si totally (where Al is not less than 0.01 weight % but not more than 13.0 weight % and Si is not less than 0.01 weight % but not more than 13.0 weight %), the remaining part of the alloy consists mainly of Fe and the alloy is characterized in that P is presented on the grain boundary thereof with the amount more than 0.5 weight % of the atoms which form said grain boundary.

Inventors

  • 👤 Hiroshi Kimira
  • 👤 Kenji Abiko
  • 👤 Takashi Sato
  • 👤 Isamu Yoshii
  • 👤 Sadao Watanabe
  • 👤 Yutaka Takei

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 12:56
CPC Classifications
C; C22; C22C; C22C38/00; C22C38/02; C22C38/06; G; G11; G11B; G11B5/00; G11B5/127; G11B5/147; H; H01; H01F; H01F1/00; H01F1/01; H01F1/03; H01F1/12; H01F1/14; H01F1/147; H01F1/14766; H01F1/14791

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 106 words
A magnetic alloy containing not less than 0.03 weight % but not more than 5.0 weight % of P, not less than 3.0 weight % but not more than 26.0 weight % of Al and Si totally (where Al is not less than 0.01 weight % but not more than 13.0 weight % and Si is not less than 0.01 weight % but not more 13.0 weight %), the remaining part consisting mainly of Fe, said alloy being characterized in that P is present on the grain boundaries thereof in an amount of more than 0.5 weight % of the atoms which form said grain boundaries.
Claim 2
Dependent Claim 106 words
A magnetic alloy containing not less than 0.03 weight % but not more than 5.0 weight % of P, not less than 3.0 weight % but not more than 26.0 weight % of Al and Si totally (where Al is not less than 0.01 weight % but not more than 13.0 weight % and Si is not less than 0.01 weight % but not more 13.0 weight %), the remaining part consisting mainly of Fe, said alloy being characterized in that P is present on the grain boundaries thereof in an amount of more than 0.5 weight % of the atoms which form said grain boundaries.
Claim 3
Dependent Claim 253 words
A magnetic alloy containing not less than 0.03 weight % but not more than 5.0 weight % of P and not less than 3.0 weight % but not more than 26.0 weight % of Al and Si totally (where Al is not less than 0.01 weight % but not more than 13.0 weight % and Si is not less than 0.01 weight % but not more than 13.0 weight %), and containing 0.01-10% by weight in total of at least one element selected from the group consisting of ______________________________________ Ti not more than 5.0 weight % V " Cr not more than 7.0 weight % Mn not more than 5.0 weight % Co " Ni not more than 7.0 weight % Cu not more than 6.0 weight % Ge not more than 5.0 weight % Y " Zr " Nb not more than 6.0 weight % Mo not more than 5.0 weight % Hf " Ta " W " Rare earth not more than 3.0 weight % elements B not more than 0.5 weight % Ca " C not more than 0.8 weight % N not more than 0.1 weight % Sn not more than 3.0 weight % Sb " Pb not more than 0.5 weight % Be not more than 3.0 weight % ______________________________________ the remaining part consisting mainly of Fe, said alloy being characterized in that P is present on the grain boundaries thereof in an amount of more than 0.5 weight % of the atoms which form said grain boundaries.
Claim 4
Dependent Claim 253 words
A magnetic alloy containing not less than 0.03 weight % but not more than 5.0 weight % of P and not less than 3.0 weight % but not more than 26.0 weight % of Al and Si totally (where Al is not less than 0.01 weight % but not more than 13.0 weight % and Si is not less than 0.01 weight % but not more than 13.0 weight %), and containing 0.01-10% by weight in total of at least one element selected from the group consisting of ______________________________________ Ti not more than 5.0 weight % V " Cr not more than 7.0 weight % Mn not more than 5.0 weight % Co " Ni not more than 7.0 weight % Cu not more than 6.0 weight % Ge not more than 5.0 weight % Y " Zr " Nb not more than 6.0 weight % Mo not more than 5.0 weight % Hf " Ta " W " Rare earth not more than 3.0 weight % elements B not more than 0.5 weight % Ca " C not more than 0.8 weight % N not more than 0.1 weight % Sn not more than 3.0 weight % Sb " Pb not more than 0.5 weight % Be not more than 3.0 weight % ______________________________________ the remaining part consisting mainly of Fe, said alloy being characterized in that P is present on the grain boundaries thereof in an amount of more than 0.5 weight % of the atoms which form said grain boundaries.

References Cited (Backward Citations)

US2899346A Cited
US2193768A Cited
US2186659A Cited
US2843478A Cited
US3392013A Cited
US3698964A Cited
US3971678A Cited
US4065330A Cited
US4168187A Cited
US4131456A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-11-09 1985-05-11 1985-11-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-11-09 1989-05-11 1989-11-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-11-09 1993-05-11 1993-11-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag