US4299608A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Joint doping of porous glasses to produce materials with high modifier concentrations
Assignee: Individual
•
Filing: 1979-09-14
•
Granted: 1981-11-10
•
Expires: 1999-09-14
Abstract
Abstract A glass composition having at least 85 mole percent of SiO 2 , where the improvement comprises at least 7 wt percent of at least one member selected from the group consisting of PbO and Bi 2 O 3 and at least 1.5 mole percent of at least one member selected from the group consisting of K 2 O, Rb 2 O and Cs 2 O.
Inventors
- 👤 Pedro B. Macedo
- 👤 Mrinmay Samanta
- 👤 Joseph H. Simmons
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-02 00:27
CPC Classifications
C; C03; C03C; C03C23/00; C03C23/0095; C03C11/00; C03C13/00; C03C13/001; C03C3/00; C03C3/04; C03C3/06; C03C3/076; C03C3/102; C03C3/108; C03C2201/00; C03C2201/06; C03C2201/08; C03C2201/10; C03C2201/30; C03C2201/50; G; G02; G02B; G02B6/00; G02B6/02; G02B6/028; G02B6/0281
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
163 words
In a method of producing a glass article comprising adding a dopant to a porous glass matrix with interconnective pores by immersing the porous glass matrix in a solution of a dopant to impregnate the porous glass matrix with the solution, precipitating the dopant from the solution within the porous glass matrix, removing solvent and where necessary decomposition products from the porous glass matrix and collapsing the porous glass matrix to a solid form, the improvement which comprises immersing the porous glass matrix in a dopant impregnating solution containing a mixture of dopants to impregnate the porous glass matrix with the solution and form an impregnated porous glass matrix with the following composition: (I) 7 to 25 weight percent of the oxide equivalent of at least one member selected from the group consisting of Pb and Bi, and (II) 1.5 to 9 mole percent of the oxide equivalent of at least one member selected from the group consisting of Cs, Rb, and K.
Claim 2
Dependent Claim
163 words
In a method of producing a glass article comprising adding a dopant to a porous glass matrix with interconnective pores by immersing the porous glass matrix in a solution of a dopant to impregnate the porous glass matrix with the solution, precipitating the dopant from the solution within the porous glass matrix, removing solvent and where necessary decomposition products from the porous glass matrix and collapsing the porous glass matrix to a solid form, the improvement which comprises immersing the porous glass matrix in a dopant impregnating solution containing a mixture of dopants to impregnate the porous glass matrix with the solution and form an impregnated porous glass matrix with the following composition: (I) 7 to 25 weight percent of the oxide equivalent of at least one member selected from the group consisting of Pb and Bi, and (II) 1.5 to 9 mole percent of the oxide equivalent of at least one member selected from the group consisting of Cs, Rb, and K.
Claim 3
Dependent Claim
28 words
The method according to claim 1 wherein the amount of group (I) is 7 to 20 weight percent and of group (II) is 1.5 to 7 mole percent.
Claim 4
Dependent Claim
80 words
The method according to claim 1 in which the dopant impregnating solution is an aqueous solution whose composition is 45 to 200 g of at least one member selected from the group (I) consisting of Pb(NO 3 ) 2 and Bi(NO 3 ) 3 per 100 cm 3 of solution and 40 to 200 g of at least one member selected from the group (II) consisting of CsNO 3 , RbNO 3 and KNO 3 per 100 cm 3 .
Claim 5
Dependent Claim
35 words
The method according to claim 3 in which the aqueous solution has 50 to 150 g of group I/100 cm 3 of solution and 50 to 150 g of group II/100 cm 3 of solution.
Claim 6
Dependent Claim
47 words
The method according to claim 3 in which the dopant impregnating solution is an aqueous solution whose composition is 50 to 150 g/100 cm 3 of solution of Pb(NO 3 ) 2 and 50 to 150 g/100 cm 3 of Cs in the form of a nitrate.
References Cited (Backward Citations)
US3938974A
Cited
US3859073A
Cited
US4110093A
Cited
US4110096A
Cited
US4183620A
Cited
US4188198A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-11-09 | 1985-05-11 | 1985-11-10 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-11-09 | 1989-05-11 | 1989-11-10 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-11-09 | 1993-05-11 | 1993-11-10 | $7700.00 | Window Closed / Lapsed |