Selective flocculation, magnetic separation, and flotation of ores

Assignee: University of Minnesota System
•
Filing: 1979-09-26
•
Granted: 1981-11-03
•
Expires: 1999-09-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Low-grade, finely disseminated, ores that are not readily amenable to conventional flotation can be upgraded by a selective flocculation-magnetic separation-flotation process. Non-magnetic particles in such an ore can be selectively flocculated either by iron particles in the ore that contain residual magnetite or by the addition of a finely ground magnetic concentrate to the ore. The selectively flocculated pulp is then passed through a magnetic separator for the rejection of siliceous gangue. Depending on the grade of the magnetic concentrates, either cationic or anionic silica flotation may be applied for further upgrading.

Inventors

  • 👤 Iwao Iwasaki

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 04:41
CPC Classifications
B; B03; B03B; B03B1/00; B03B1/04; B03C; B03C1/00; B03C1/005; B03C1/01; B03D; B03D1/00; B03D1/02; B03D3/00; B03D3/06

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 94 words
A method of concentrating low-grade ores containing residual magnetite, which method comprises: (A) mixing said ore with water and grinding to a fineness sufficient to substantially liberate the desired mineral values in said ore, (B) mixing said finely divided ore, containing magnetite, with a flocculating material selected from the class consisting of carbohydrate and synthetic polymerized flocculating agents to induce selective flocculation of the desired mineral on nuclei of ore particles containing residual magnetite, (C) subjecting said flocculated mineral to magnetic separation, (D) recovering the flocs of mineral, and (E) discarding the non-magnetic gangue.
Claim 2
Independent Claim 94 words
A method of concentrating low-grade ores containing residual magnetite, which method comprises: (A) mixing said ore with water and grinding to a fineness sufficient to substantially liberate the desired mineral values in said ore, (B) mixing said finely divided ore, containing magnetite, with a flocculating material selected from the class consisting of carbohydrate and synthetic polymerized flocculating agents to induce selective flocculation of the desired mineral on nuclei of ore particles containing residual magnetite, (C) subjecting said flocculated mineral to magnetic separation, (D) recovering the flocs of mineral, and (E) discarding the non-magnetic gangue.
Claim 3
Dependent Claim 19 words
A method according to claim 1 wherein the resulting magnetically separated concentrate is further concentrated by flotation of silica.
Claim 4
Dependent Claim 28 words
A method according to claim 1 wherein the ore initially contains little or no residual magnetite and finely ground magnetite concentrate is added to the ore before flocculation.
Claim 5
Dependent Claim 16 words
A method according to claim 1 wherein a dispersant is added to the ore before grinding.
Claim 6
Dependent Claim 34 words
A method according to claim 4 wherein said ore is oxidized or partially oxidized iron ore and said dispersant is selected from the group consisting of caustic soda and sodium silicate and mixtures thereof.
Claim 7
Dependent Claim 22 words
A method according to claim 1 wherein said ore is oxidized or partially oxidized iron ore and said flocculating material is starch.
Claim 8
Dependent Claim 13 words
A method according to claim 6 wherein said starch is causticized corn starch.
Claim 9
Dependent Claim 49 words
A method according to claim 1 wherein: (A) said desired mineral is recovered by flowing a stream of dispersed flocculated ore over a magnetic surface, (B) the gangue is washed from the surface, and (C) the retained flocs of desired mineral are concentrated by removal from the magnetic surface.
Claim 10
Dependent Claim 20 words
A method according to claim 8 wherein said magnetic surface is inclined to facilitate washing of gangue from the surface.
Claim 11
Independent Claim 121 words
A method of concentrating low-grade oxidized and partially oxidized iron ores containing residual magnetite, which method comprises: (A) mixing said ore with a dispersant selected from the group consisting of caustic soda and sodium silicate and mixtures thereof, and water, and grinding to a fineness sufficient to substantially liberate the iron values in said ore, (B) mixing said finely divided ore containing magnetite with a causticized starch flocculating material to induce selective flocculation of iron oxides on nuclei of ore particles containing residual magnetite, (C) flowing a stream of selectively flocculated ore over an inclined magnetic surface, (D) washing the siliceous gangue from the magnetic surface, and (E) recovering the retained flocs of iron oxide by removal from the magnetic surface.
Claim 12
Independent Claim 121 words
A method of concentrating low-grade oxidized and partially oxidized iron ores containing residual magnetite, which method comprises: (A) mixing said ore with a dispersant selected from the group consisting of caustic soda and sodium silicate and mixtures thereof, and water, and grinding to a fineness sufficient to substantially liberate the iron values in said ore, (B) mixing said finely divided ore containing magnetite with a causticized starch flocculating material to induce selective flocculation of iron oxides on nuclei of ore particles containing residual magnetite, (C) flowing a stream of selectively flocculated ore over an inclined magnetic surface, (D) washing the siliceous gangue from the magnetic surface, and (E) recovering the retained flocs of iron oxide by removal from the magnetic surface.
Claim 13
Dependent Claim 19 words
A method according to claim 10 wherein the resulting magnetically separated iron oxide concentrate is further concentrated by flotation.
Claim 14
Dependent Claim 28 words
A method according to claim 10 wherein the ore initially contains little or no residual magnetite and finely ground magnetite concentrate is added to the ore before flocculation.
Claim 15
Independent Claim 177 words
A method of concentrating low-grade oxidized and partially oxidized iron ores containing residual magnetite, which method comprises: (A) mixing said ore with about 1 to 4 pounds of an alkaline dispersant per ton of ore and water to provide a slurry containing about 50 to 80 percent solids and having a pH of from about 9.5 to about 11.0, (B) grinding said slurry to a fineness sufficient to substantially liberate the iron values in said ore, (C) diluting the finely divided ground material to between about 5 and 40 percent solids, (D) mixing said diluted slurry of finely divided ore containing magnetite with about 0.25 to 1.0 pound per ton of ore of a flocculating material to induce selective flocculation of iron oxides on nuclei of ore particles containing residual magnetite, (E) flowing a stream of selectively flocculated ore over an inclined magnetic surface to trap the ore particles containing residual magnetite thereon, (F) washing the siliceous gangue from the magnetic surface, and (G) recovering the retained flocs of iron oxide by removal from the magnetic surface.
Claim 16
Independent Claim 177 words
A method of concentrating low-grade oxidized and partially oxidized iron ores containing residual magnetite, which method comprises: (A) mixing said ore with about 1 to 4 pounds of an alkaline dispersant per ton of ore and water to provide a slurry containing about 50 to 80 percent solids and having a pH of from about 9.5 to about 11.0, (B) grinding said slurry to a fineness sufficient to substantially liberate the iron values in said ore, (C) diluting the finely divided ground material to between about 5 and 40 percent solids, (D) mixing said diluted slurry of finely divided ore containing magnetite with about 0.25 to 1.0 pound per ton of ore of a flocculating material to induce selective flocculation of iron oxides on nuclei of ore particles containing residual magnetite, (E) flowing a stream of selectively flocculated ore over an inclined magnetic surface to trap the ore particles containing residual magnetite thereon, (F) washing the siliceous gangue from the magnetic surface, and (G) recovering the retained flocs of iron oxide by removal from the magnetic surface.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-11-02 1985-05-04 1985-11-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-11-02 1989-05-04 1989-11-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-11-02 1993-05-04 1993-11-03 $7700.00 Window Closed / Lapsed