Abstract
Abstract A process for recovering gold from a raw material containing gold by treating the raw material with either aqua regia or hydrochloric acid to form chloroauric acid, extracting the chloroauric acid with an organic solvent and reducing the acid to precipitate gold for separation and recovery.
Inventors
- 👤 Keita Yamada
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-07 08:59
CPC Classifications
C; C22; C22B; C22B11/00; C22B11/04; C01; C01G; C01G7/00; C01G7/003; C22B3/00; C22B3/20; C22B3/26; C22B3/306; Y; Y02; Y02P; Y02P10/00; Y02P10/20
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
143 words
A process for recovering gold from a raw material containing gold comprising the steps of treating the raw material with either aqua regia or 6.0 to 6.5 normal hydrochloric acid to form chloroauric acid; extracting the chloroauric acid with an organic solvent selected from the group consisting of ethyl ether, methyl isobutyl ketone and a mixture of methyl isobutyl ketone and isoamyl acetate; separating and washing the organic solvent; stripping the gold contained in the organic solvent into an aqueous phase as gold hydroxide by adding a 30 to 50% solution of NaOH or NH 4 OH to the organic solvent and agitating the resulting mixture; separating the aqueous layer; reacting the gold hydroxide in the aqueous layer with 3 to 5 normal hydrochloric acid to form chloroauric acid; reducing the chloroauric acid to precipitate the gold; and separating and recovering the gold.
Claim 2
Dependent Claim
143 words
A process for recovering gold from a raw material containing gold comprising the steps of treating the raw material with either aqua regia or 6.0 to 6.5 normal hydrochloric acid to form chloroauric acid; extracting the chloroauric acid with an organic solvent selected from the group consisting of ethyl ether, methyl isobutyl ketone and a mixture of methyl isobutyl ketone and isoamyl acetate; separating and washing the organic solvent; stripping the gold contained in the organic solvent into an aqueous phase as gold hydroxide by adding a 30 to 50% solution of NaOH or NH 4 OH to the organic solvent and agitating the resulting mixture; separating the aqueous layer; reacting the gold hydroxide in the aqueous layer with 3 to 5 normal hydrochloric acid to form chloroauric acid; reducing the chloroauric acid to precipitate the gold; and separating and recovering the gold.
Claim 3
Dependent Claim
17 words
The process of claim 1, wherein the reducing step is accomplished by the addition of sodium sulfite.
Claim 4
Dependent Claim
263 words
A process for recovering gold from materials containing gold comprising the steps of: (a) adding sufficient quantities of reagent selected from the group consisting of HCl and aqua regia, to a gold-containing material and heating the resulting mixture to between about 100° to 130° C., whereby a major portion of the gold is converted to chloroauric acid; (b) cooling the mixture containing chloroauric acid to about ambient conditions and adding thereto an organic solvent selected from the group consisting of methyl isobutyl ketone, ethyl ether and mixtures of methyl isobutyl ketone and isoamyl acetate, whereby there are formed a first aqueous phase and a first organic phase; (c) intimately mixing the first aqueous phase and the first organic phase; (d) separating the first organic phase from the first aqueous phase, the first organic phase containing substantially all of the chloroauric acid; (e) washing the first organic phase with 5 to 8 N hydrochloric acid; (f) mixing the first organic phase with an aqueous solution containing 30 to 50% of a reagent selected from the group consisting of sodium hydroxide and ammonia hydroxide, wherein a second aqueous phase is formed containing gold hydroxide, the chloroauric acid having been converted to gold hydroxide; (g) separating the second aqueous phase containing gold hydroxide; (h) reacting the second aqueous phase containing gold hydroxide with sufficient quantities of between about 3 to 5 N HCl to convert the gold in the second aqueous phase to chloroauric acid; (i) reacting the aqueous phase with a reducing agent whereby elemental gold is precipitated from solution; and (j) recovering elemental gold.
Claim 5
Dependent Claim
263 words
A process for recovering gold from materials containing gold comprising the steps of: (a) adding sufficient quantities of reagent selected from the group consisting of HCl and aqua regia, to a gold-containing material and heating the resulting mixture to between about 100° to 130° C., whereby a major portion of the gold is converted to chloroauric acid; (b) cooling the mixture containing chloroauric acid to about ambient conditions and adding thereto an organic solvent selected from the group consisting of methyl isobutyl ketone, ethyl ether and mixtures of methyl isobutyl ketone and isoamyl acetate, whereby there are formed a first aqueous phase and a first organic phase; (c) intimately mixing the first aqueous phase and the first organic phase; (d) separating the first organic phase from the first aqueous phase, the first organic phase containing substantially all of the chloroauric acid; (e) washing the first organic phase with 5 to 8 N hydrochloric acid; (f) mixing the first organic phase with an aqueous solution containing 30 to 50% of a reagent selected from the group consisting of sodium hydroxide and ammonia hydroxide, wherein a second aqueous phase is formed containing gold hydroxide, the chloroauric acid having been converted to gold hydroxide; (g) separating the second aqueous phase containing gold hydroxide; (h) reacting the second aqueous phase containing gold hydroxide with sufficient quantities of between about 3 to 5 N HCl to convert the gold in the second aqueous phase to chloroauric acid; (i) reacting the aqueous phase with a reducing agent whereby elemental gold is precipitated from solution; and (j) recovering elemental gold.
References Cited (Backward Citations)
US440143A
Cited
US3397040A
Cited
US3576620A
Cited
US3843379A
Cited
US3771996A
Cited
US3885955A
Cited
US3935006A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-10-26 | 1985-04-27 | 1985-10-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-10-26 | 1989-04-27 | 1989-10-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-10-26 | 1993-04-27 | 1993-10-27 | $7700.00 | Window Closed / Lapsed |