📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for emplacing a seal on a closure for a container which comprises despositing a foamed adhesive in liquid form on an interior surface of the closure and allowing that foamed adhesive to solidify and adhere as a solid cellular foam to the interior surface of the closure.

Inventors

  • 👤 Robert R. Terry
  • 👤 Jacob J. Boone

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 21:58
CPC Classifications
B; B05; B05B; B05B7/00; B05B7/24; B05B7/26; B05B7/262; B05C; B05C5/00; B05C5/02; B05C5/0208; B05C5/0212; B05C5/0216; B05C5/0225; B21; B21D; B21D51/00; B21D51/16; B21D51/38; B21D51/44; B21D51/46; B29; B29C; B29C31/00; B29C31/04; B29C31/042; B29C31/047; B29C70/00; B29C70/68; B29C70/78; B29C70/80; B29C43/00; B29C43/32; B29C43/34; B29C2043/3433; B29C43/02; B29C43/18; B29L; B29L2031/00; B29L2031/56; B29L2031/565; B29L2031/709; B29L2031/7096; Y; Y10; Y10T; Y10T156/00; Y10T156/17; Y10T156/1798; Y10T428/00; Y10T428/21; Y10T428/215; Y10T428/24; Y10T428/24479; Y10T428/24488; Y10T428/24496; Y10T428/24504; Y10T428/24802; Y10T428/249921; Y10T428/249953; Y10T428/249982; Y10T428/249984

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 149 words
The method of obtaining a seal upon the interior surface of a closure for a container, which method comprises heating a thermoplastic adhesive material which is solid at room temperature so as to convert said adhesive material to the molten state, creating a mixture of gas and molten thermoplastic adhesive, pressurizing said mixture of gas and molten thermoplastic adhesive so as to force said gas into solution with said molten thermoplastic adhesive, dispensing the pressurized mixture of gas and molten adhesive at atmospheric pressure onto the interior surface of a container closure, whereby said gas comes out of solution with said molten thermoplastic adhesive and forms a foamed molten adhesive bead upon said interior surface, and cooling said foamed molten adhesive bead while maintained as a foam on said interior surface of said closure so as to form a cellular seal adhered to said interior surface of said closure.
Claim 2
Independent Claim 149 words
The method of obtaining a seal upon the interior surface of a closure for a container, which method comprises heating a thermoplastic adhesive material which is solid at room temperature so as to convert said adhesive material to the molten state, creating a mixture of gas and molten thermoplastic adhesive, pressurizing said mixture of gas and molten thermoplastic adhesive so as to force said gas into solution with said molten thermoplastic adhesive, dispensing the pressurized mixture of gas and molten adhesive at atmospheric pressure onto the interior surface of a container closure, whereby said gas comes out of solution with said molten thermoplastic adhesive and forms a foamed molten adhesive bead upon said interior surface, and cooling said foamed molten adhesive bead while maintained as a foam on said interior surface of said closure so as to form a cellular seal adhered to said interior surface of said closure.
Claim 3
Dependent Claim 151 words
Apparatus for creating a seal upon the interior surface of a closure for a container, which apparatus comprises means for heating a thermoplastic adhesive material which is solid at room temperature so as to convert it to the molten state, means for creating a mixture of gas and said molten thermoplastic adhesive, means for pressurizing said mixture of gas and molten thermoplastic adhesive so as to force said gas into solution with said molten thermoplastic adhesive, means for dispensing the pressurized mixture of gas and molten adhesive at atmospheric pressure whereby said gas is released from solution to form a foamed adhesive in an annular pattern on the interior surface of the container closure, and means for maintaining said foamed molten adhesive in said annular pattern on said interior surface while said foam is cooled so as to form a solid cellular seal adhered to said interior surface of said closure.
Claim 4
Dependent Claim 151 words
Apparatus for creating a seal upon the interior surface of a closure for a container, which apparatus comprises means for heating a thermoplastic adhesive material which is solid at room temperature so as to convert it to the molten state, means for creating a mixture of gas and said molten thermoplastic adhesive, means for pressurizing said mixture of gas and molten thermoplastic adhesive so as to force said gas into solution with said molten thermoplastic adhesive, means for dispensing the pressurized mixture of gas and molten adhesive at atmospheric pressure whereby said gas is released from solution to form a foamed adhesive in an annular pattern on the interior surface of the container closure, and means for maintaining said foamed molten adhesive in said annular pattern on said interior surface while said foam is cooled so as to form a solid cellular seal adhered to said interior surface of said closure.

References Cited (Backward Citations)

US3053221A Cited
US3261895A Cited
US3570725A Cited
US3859113A Cited
US3788561A Cited
US4059714A Cited
US4156754A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-10-19 1985-04-20 1985-10-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-10-19 1989-04-20 1989-10-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-10-19 1993-04-20 1993-10-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag