Process for rapid annealing of refractory fiber bodies and laminated body produced by process

Assignee: Morgan Advanced Materials PLC
•
Filing: 1979-09-07
•
Granted: 1981-10-13
•
Expires: 1999-09-07
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for the rapid annealing of refractory fiber is disclosed. Air at a temperature of 750° F. (400° C.) to 1400° F. (760° C.) is passed through a refractory fiber body for a period of 5 to 200 seconds while the body is held securely in place for dimensional integrity. Apparatus for performing the process of this invention comprises an annealing unit containing opposed foraminous platens and means for passing hot air through the platens and through the fiber body retained between the platens or opposed foraminous belts and adjacent conduits and means for passing the hot annealing air through the conduits and belts and through the fiber body retained between the belts. The process and apparatus may be used to produce fiber bodies of a single material or laminated bodies of a plurality of interlocked layers, which may be of different fiber materials. The resultant products have excellent dimensional integrity, especially of the critical thickness dimension, and the process operates much more economically and thermally more efficiently than prior art tunnel oven processes.

Inventors

  • 👤 Richard N. Cunningham
  • 👤 Romain E. Loeffler, deceased

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 08:36
CPC Classifications
C; C04; C04B; C04B30/00; C04B30/02; C03; C03B; C03B37/00; C03B37/10; C03B37/14; C03B37/15; Y; Y10; Y10S; Y10S428/00; Y10S428/92; Y10T; Y10T428/00; Y10T428/24; Y10T428/24942

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 57 words
A process for annealing of a body of refractory fiber which comprises passing air at a temperature in the range of from about 750° F. to about 1400° F. through said body for a period of from about 5 to about 200 seconds while maintaining said body with a predetermined dimension in the direction of air flow.
Claim 2
Dependent Claim 57 words
A process for annealing of a body of refractory fiber which comprises passing air at a temperature in the range of from about 750° F. to about 1400° F. through said body for a period of from about 5 to about 200 seconds while maintaining said body with a predetermined dimension in the direction of air flow.
Claim 3
Dependent Claim 22 words
A process as in claim 1 wherein said temperature is in the range of from about 800° F. to about 1200° F.
Claim 4
Dependent Claim 22 words
A process as in claim 2 wherein said temperature is in the range of from about 900° F. to about 1100° F.
Claim 5
Dependent Claim 55 words
A process as in claims 1, 2 or 3 and further comprising, providing said fiber body in the form of a substantially continuous strip, passing segments of said fiber body seriatim into an annealing zone, retaining each segment in said annealing zone for said period while said air is passed therethrough to anneal said segment.
Claim 6
Dependent Claim 39 words
A process as in claim 4 and further comprising, moving said fiber body in the form of said continuous strip continuously into an inlet accumulation zone and passing segments of said strip intermittently and seriatim to said annealing zone.
Claim 7
Dependent Claim 37 words
A process as in claim 4 and further comprising, discharging said segments seriatim from said annealing zone and moving said segments intermittently into an outlet accumulation zone and discharging said segments continuously from said outlet accumulation zone.
Claim 8
Dependent Claim 31 words
A process as in claim 6 and further comprising, cooling each of said segments following said discharge from said annealing zone and prior to said receipt by said outlet accumulation zone.
Claim 9
Dependent Claim 20 words
A process as in claim 7 wherein said cooling is effected by passing ambient air through each of said segments.
Claim 10
Dependent Claim 33 words
A process as in claims 1, 2 or 3 and further comprising, maintaining the lateral or transverse dimensions of said body as well as the dimension in the direction of said air flow.
Claim 11
Dependent Claim 16 words
A process as in claim 4 wherein said strip comprises a plurality of layers of fibers.
Claim 12
Dependent Claim 33 words
A process as in claim 10 wherein the fibers in at least one of said layers differ in their temperature resistance properties from the fibers in at least one other of said layers.
Claim 13
Dependent Claim 17 words
A body of refractory fiber annealed according to a process as in claims 1, 2 or 3.
Claim 14
Dependent Claim 14 words
A body of refractory fiber annealed according to a process as in claim 4.
Claim 15
Dependent Claim 14 words
A laminated body of refractory fiber annealed according to the process of claim 10.
Claim 16
Dependent Claim 14 words
A laminated body of refractory fiber annealed according to the process of claim 11.

References Cited (Backward Citations)

US3723593A Cited
US3887524A Cited
US4151235A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-10-12 1985-04-13 1985-10-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-10-12 1989-04-13 1989-10-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-10-12 1993-04-13 1993-10-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag