← Back to Patent Explorer
US4293986A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of making a quartz crystal oscillator

Assignee: MATSUSHIMA KOGO KK
•
Filing: 1978-12-05
•
Granted: 1981-10-13
•
Expires: 1998-12-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A quartz crystal oscillator package comprising a quartz crystal vibrator leaf enclosed in an evacuated housing. The vibrator leaf frame is sandwiched and sealed between a pair of housing elements formed by etching at one time the periphery of each housing element and at another time etching a concave portion in each housing element. Opposed concave portions provide the internal volume wherein the vibrator leaf is sealed under vacuum. Using heat and vacuum, a metal film deposited on the sealing surfaces of the housing elements fuses with a binder material to form a eutectic alloy seal. A flat package having small size, high structural strength, an excellent hermetic seal, and high internal vacuum is produced by this method.

Inventors

  • 👤 Masatoshi Kobayashi
  • 👤 George Shimakawa
  • 👤 Yukio Hara
  • 👤 Hiroyuki Fujii
  • 👤 Kabushiki Kaisha Seikosha

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 22:45
CPC Classifications
H; H03; H03H; H03H9/00; H03H9/02; H03H9/05; H03H9/10; H03H9/1007; H03H9/1014; H03H9/1021; G; G04; G04F; G04F5/00; G04F5/04; G04F5/06; G04F5/063; H03H3/00; H03H3/007; H03H3/02; H03H9/0595; Y; Y10; Y10T; Y10T29/00; Y10T29/42

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 218 words
A method for manufacturing a quartz crystal oscillator package having a high internal vacuum, said package comprising a quartz crystal vibrator with a frame, a pair of housing elements having peripheral surfaces, said peripheral surfaces being shaped to register one to the other, a hermetic seal at the periphery of said oscillator package, comprising the steps of: (a) coating said peripheral surfaces with a metal film; (b) coating at least one of said metal films with a gas free material capable of forming an alloy with said metal film, said alloy forming coating being produced on said at least one said metal film at an ambient pressure less than 10 -2 torr, whereby gas is eliminated from said alloy forming coating during step (b); (c) positioning said coated housing elements in an opposed position, said coatings being opposed one to the other, said crystal vibrator with a frame being enclosed within said opposed housing elements; (d) drawing a high vacuum over the elements of said quartz crystal oscillator package and within said housing elements; (e) applying heat under said high vacuum to fuse said alloy forming coating with said metal film to form an alloy whereby said housing elements are rigidly and hermetically joined together and said package has said high internal vacuum within said joined housing elements.
Claim 2
Independent Claim 218 words
A method for manufacturing a quartz crystal oscillator package having a high internal vacuum, said package comprising a quartz crystal vibrator with a frame, a pair of housing elements having peripheral surfaces, said peripheral surfaces being shaped to register one to the other, a hermetic seal at the periphery of said oscillator package, comprising the steps of: (a) coating said peripheral surfaces with a metal film; (b) coating at least one of said metal films with a gas free material capable of forming an alloy with said metal film, said alloy forming coating being produced on said at least one said metal film at an ambient pressure less than 10 -2 torr, whereby gas is eliminated from said alloy forming coating during step (b); (c) positioning said coated housing elements in an opposed position, said coatings being opposed one to the other, said crystal vibrator with a frame being enclosed within said opposed housing elements; (d) drawing a high vacuum over the elements of said quartz crystal oscillator package and within said housing elements; (e) applying heat under said high vacuum to fuse said alloy forming coating with said metal film to form an alloy whereby said housing elements are rigidly and hermetically joined together and said package has said high internal vacuum within said joined housing elements.
Claim 3
Dependent Claim 12 words
The method of claim 1, wherein said alloy is a eutectic alloy.
Claim 4
Dependent Claim 44 words
The method of claim 1, wherein said frame is coated with a metal film, said frame being sandwiched between said peripheral surfaces of said opposed housing elements, and said alloy forming coating element is interposed between said frame and said associated opposed housing elements.

References Cited (Backward Citations)

US3857161A Cited
US4135108A Cited
US4077558A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-10-12 1985-04-13 1985-10-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-10-12 1989-04-13 1989-10-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-10-12 1993-04-13 1993-10-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag