Underwater wax formulation and method

Assignee: United States Department of the Navy
•
Filing: 1980-02-28
•
Granted: 1981-10-06
•
Expires: 2000-02-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A wax coating composition capable of underwater application to submerged surfaces comprises a mixture of from about 2% to about 18% of a polymer having the recurring unit-C2F3Cl -; from about 20% to about 40% of a microcrystalline wax; from about 40% to about 70% of a chlorinated paraffinic hydrocarbon and up to about 5% of a surfactant. An appropriate biocide may be interspersed into the wax to prevent marine growth. Another wax coating composition comprises a mixture of from about 16% to about 27% of a paraffin wax; from about 22% to about 33% of a microcrystalline wax; and from about 36% to about 58% of a chlorinated paraffinic hydrocarbon. A biocide such as the organotins or cuprous oxide antifoulants may comprise from about 2% to about 10% of the wax mixture.

Inventors

  • 👤 Robert F. Supcoe
  • 👤 Thomas Radakovich

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 02:06
CPC Classifications
C; C09; C09D; C09D5/00; C09D5/16; C09D5/1656; C09D191/00; C09D191/06; C09D191/08

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 106 words
A wax coating material for application to submerged surfaces consisting essentially of a mixture, by weight percent, of from about 2% to about 18% of a fluorinatedchlorinated aliphatic polymer having a recurring unit of --C 2 F 3 Cl-- and an average molecular weight range of between about 500 to about 1200; from about 20% to about 40% of a microcrystalline wax; from about 40% to about 70% of a chlorinated paraffinic hydrocarbon having a chlorine content, by weight percent, of from about 40% to about 70% and up to about 5% of a surfactant for improving the displacement of the water molecules from the surface.
Claim 2
Dependent Claim 106 words
A wax coating material for application to submerged surfaces consisting essentially of a mixture, by weight percent, of from about 2% to about 18% of a fluorinatedchlorinated aliphatic polymer having a recurring unit of --C 2 F 3 Cl-- and an average molecular weight range of between about 500 to about 1200; from about 20% to about 40% of a microcrystalline wax; from about 40% to about 70% of a chlorinated paraffinic hydrocarbon having a chlorine content, by weight percent, of from about 40% to about 70% and up to about 5% of a surfactant for improving the displacement of the water molecules from the surface.
Claim 3
Dependent Claim 29 words
The wax material according to claim 1, further comprising a biocide for preventing marine growth comprising, by weight percent, from about 1% to about 10% of the wax mixture.
Claim 4
Dependent Claim 45 words
The wax material of claim 1, wherein said mixture has a viscosity of 100° C. of 6.7 to 7.4 cps; a melting point of about 41° C. to about 52° C. and a density of about 0.734 g/cm 3 to about 0.885 g/cm 3 .
Claim 5
Independent Claim 116 words
A method of coating submerged surfaces for preventing marine growth comprises applying a wax mixture directly to the submerged surfaces, said wax mixture having a formulation substantially as follows: from about 2% to about 18% of a fluorinated-chlorinated aliphatic polymer having a recurring structural unit --C 2 F 3 Cl-- and an average molecular weight range of between about 500 to about 1200; from about 20% to about 40% of a microcrystalline wax; from about 40% to about 70% of a chlorinated paraffinic hydrocarbon having a chlorine content, by weight percent, of from about 40% to about 70%; and up to about 5% of a surfactant for improving the displacement of the molecules from the surface.
Claim 6
Independent Claim 116 words
A method of coating submerged surfaces for preventing marine growth comprises applying a wax mixture directly to the submerged surfaces, said wax mixture having a formulation substantially as follows: from about 2% to about 18% of a fluorinated-chlorinated aliphatic polymer having a recurring structural unit --C 2 F 3 Cl-- and an average molecular weight range of between about 500 to about 1200; from about 20% to about 40% of a microcrystalline wax; from about 40% to about 70% of a chlorinated paraffinic hydrocarbon having a chlorine content, by weight percent, of from about 40% to about 70%; and up to about 5% of a surfactant for improving the displacement of the molecules from the surface.

References Cited (Backward Citations)

US2838419A Cited
US3806352A Cited
US3959530A Cited
US4019922A Cited
US4020200A Cited
US4183757A Cited
US4098925A Cited
US4115130A Cited
US4154818A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-10-05 1985-04-06 1985-10-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-10-05 1989-04-06 1989-10-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-10-05 1993-04-06 1993-10-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag