Abstract

Abstract A potting process for a magnetic speed pickup including elements subject to substantial thermal expansion and contraction, wherein each step of the potting process is performed at an elevated temperature corresponding to the highest expected temperature for a given application. As a result, adequate spacing is provided between the various pickup elements to accommodate for thermal expansion and contraction of the elements when the pickup is used in a thermally variant environment.

Inventors

  • 👤 Glen E. Tranbarger

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 04:35
CPC Classifications
H; H01; H01F; H01F1/00; H01F1/01; H01F1/03; H01F1/032; H01F1/10; H01F1/11; H01F1/113; B; B29; B29C; B29C37/00; B29C37/005; B29C39/00; B29C39/02; B29C39/10; B29C70/00; B29C70/68; B29C70/70; G; G01; G01P; G01P3/00; G01P3/42; G01P3/44; G01P3/48; G01P3/481; G01P3/488; B29K; B29K2105/00; B29K2105/06; B29K2105/20; B29K2105/203

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 123 words
A method of potting a magnetic pickup assembly that comprises a housing containing a permanent magnet of a type that thermally expands with increasing temperature comprising the steps of: heating the pickup assembly to a temperature that causes thermal expansion of the permanent magnet; introducing a resinous material into said housing; evacuating the pickup assembly so that said resinous material impregnates the spaces surrounding said permanent magnet; curing said resinous material by maintaining the temperature of the material at a predetermined value for a period of time sufficient to solidify said material; and cooling said assembly to permit said permanent magnet to contract, whereby adequate spacing is provided within said pickup assembly to accommodate for thermal expansion and contraction of said permanent magnet.
Claim 2
Independent Claim 123 words
A method of potting a magnetic pickup assembly that comprises a housing containing a permanent magnet of a type that thermally expands with increasing temperature comprising the steps of: heating the pickup assembly to a temperature that causes thermal expansion of the permanent magnet; introducing a resinous material into said housing; evacuating the pickup assembly so that said resinous material impregnates the spaces surrounding said permanent magnet; curing said resinous material by maintaining the temperature of the material at a predetermined value for a period of time sufficient to solidify said material; and cooling said assembly to permit said permanent magnet to contract, whereby adequate spacing is provided within said pickup assembly to accommodate for thermal expansion and contraction of said permanent magnet.
Claim 3
Independent Claim 118 words
A method of potting a magnetic pickup assembly that comprises a housing containing a plastic magnet comprising the steps of: heating the pickup assembly to a temperature that equals or exceeds the use temperature for the intended pickup application; introducing a resinous material into said housing; evacuating the pickup assembly so that said resinous material impregnates the spaces surrounding said magnet; curing said resinous material by maintaining the temperature of the assembly at or higher than said use temperature for a period of time sufficient to solidify said material; and cooling said assembly to permit said magnet to contract, whereby adequate spacing is provided within said pickup assembly to accommodate for thermal expansion and contraction of said magnet.
Claim 4
Independent Claim 118 words
A method of potting a magnetic pickup assembly that comprises a housing containing a plastic magnet comprising the steps of: heating the pickup assembly to a temperature that equals or exceeds the use temperature for the intended pickup application; introducing a resinous material into said housing; evacuating the pickup assembly so that said resinous material impregnates the spaces surrounding said magnet; curing said resinous material by maintaining the temperature of the assembly at or higher than said use temperature for a period of time sufficient to solidify said material; and cooling said assembly to permit said magnet to contract, whereby adequate spacing is provided within said pickup assembly to accommodate for thermal expansion and contraction of said magnet.
Claim 5
Independent Claim 127 words
A method of potting a magnetic pickup assembly that comprises a housing containing a polymer bonded barium-ferrite magnet comprising the steps of: heating the pickup assembly to a temperature that equals or exceeds the use temperature for the intended pickup application; introducing a heated resinous material comprising epoxy resin and hardener into said housing; evacuating the pickup assembly so that said resinous material impregnates the spaces surrounding said magnet; curing said resinous material by maintaining the temperature of the pickup assembly at or higher than said use temperature for a period of time sufficient to solidify said material; and cooling said assembly to permit said magnet to contract, whereby adequate spacing is provided within said pickup assembly to accommodate for thermal expansion and contraction of said magnet.
Claim 6
Independent Claim 127 words
A method of potting a magnetic pickup assembly that comprises a housing containing a polymer bonded barium-ferrite magnet comprising the steps of: heating the pickup assembly to a temperature that equals or exceeds the use temperature for the intended pickup application; introducing a heated resinous material comprising epoxy resin and hardener into said housing; evacuating the pickup assembly so that said resinous material impregnates the spaces surrounding said magnet; curing said resinous material by maintaining the temperature of the pickup assembly at or higher than said use temperature for a period of time sufficient to solidify said material; and cooling said assembly to permit said magnet to contract, whereby adequate spacing is provided within said pickup assembly to accommodate for thermal expansion and contraction of said magnet.

References Cited (Backward Citations)

US3693252A Cited
US3710437A Cited
US4045738A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-09-14 1985-03-16 1985-09-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-09-14 1989-03-16 1989-09-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-09-14 1993-03-16 1993-09-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag